| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage, Flow | 0.013 - 0.0165 cm/cm | 0.013 - 0.0165 in/in | |
|
LATI Latamid 66 E21 PA 66, Impact Modified
Polyamide 66 (PA66). Toughened. Good impact resistance.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p...
|
|||
| Linear Mold Shrinkage, Flow | 0.0135 - 0.0165 cm/cm | 0.0135 - 0.0165 in/in | |
|
LATI Latene® 7 TR-V2 PP Homopolymer, Mineral Reinforced, Flame Retardant
Polypropylene homopolymer (PPh) based compound. Mineral filler. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free. Good surface appearance.Availability: Africa & Middle East; Asia..
|
|||
| Linear Mold Shrinkage, Flow | 0.0135 - 0.0165 cm/cm | 0.0135 - 0.0165 in/in | |
|
LATI Latene® EP 7-V2HF PP Copolymer, Flame Retardant
Polypropylene copolymer (PPc) based compound. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; N..
|
|||
| Linear Mold Shrinkage, Flow | 0.013 - 0.0165 cm/cm | 0.013 - 0.0165 in/in | |
|
LATI Latistat 67-08 PA66, Impact Modified
Dissipative product based on Polyamide 66 (PA66), impact modified. Unfilled.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industr..
|
|||
| Linear Mold Shrinkage, Flow | 0.013 - 0.0165 cm/cm | 0.013 - 0.0165 in/in | |
|
LATI Latiohm 66-10 H2 CNT CE/10 PA66, 10% Mineral Fiber Reinforced, Heat Stabilized
Semiconductive/dissipative product based on Polyamide 66 (PA66). Heat stabilized. Carbon nanotubes. Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ame..
|
|||