Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage, Flow = 0.019 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.015 - 0.019 cm/cm

@Thickness 2.00 mm,
Temperature 23.0 °C
0.015 - 0.019 in/in

@Thickness 0.0787 in,
Temperature 73.4 °F
Internal Method
PolyOne OnFlex™ HT 70A-3S2103 Thermoplastic Elastomer (TPE)
OnFlex™ HT thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds is specially formulated to deliver very good compression set performance at..
Linear Mold Shrinkage, Flow 0.015 - 0.019 cm/cm

@Thickness 3.17 mm
0.015 - 0.019 in/in

@Thickness 0.125 in
ASTM D955
Ravago Manufacturing Americas Enviramid™ N1300HL BK/UV2 Post Consumer Recycle Nylon 66
Heat Stabilized, Lubricated, UV Stabilized, Black and made from EnViramid Post Consumer Recycled NylonInformation provided by Ravago.
Linear Mold Shrinkage, Flow 0.015 - 0.019 cm/cm

@Thickness 3.17 mm
0.015 - 0.019 in/in

@Thickness 0.125 in
ASTM D955
Ravago Manufacturing Americas Enviramid™ N2300HL BK Post Consumer Recycle Nylon 6
Heat Stabilized, Lubricated, Black, and made from EnViramid™ Post Consumer Recycled NylonInformation provided by Ravago.
Linear Mold Shrinkage, Flow 0.015 - 0.019 cm/cm

@Thickness 3.17 mm
0.015 - 0.019 in/in

@Thickness 0.125 in
ASTM D955
Ravago Manufacturing Americas Enviramid™ N2300HL BK/UV2 Post Consumer Recycle Nylon 6
Heat Stabilized, Lubricated, UV Stabilized, Black, and made from EnViramid™ Post Consumer Recycled NylonInformation provided by Ravago.
Linear Mold Shrinkage, Flow 0.015 - 0.019 cm/cm

@Thickness 3.17 mm
0.015 - 0.019 in/in

@Thickness 0.125 in
ASTM D955
Ravago Manufacturing Americas Enviramid™ N2300THL BK/HF Post Consumer Recycle Nylon 6
Impact Modified, High Flow, Heat Stabilized, Lubricated, Black and Made from EnViramid Post Consumer Recycled NylonInformation provided by Ravago.
Linear Mold Shrinkage, Flow 0.014 - 0.019 cm/cm

@Thickness 3.17 mm
0.014 - 0.019 in/in

@Thickness 0.125 in
ASTM D955
Ravago Manufacturing Americas Hylon® N1000HL Nylon 6/6
Available in North America Additive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and Lubricated RoHS Compliant Auto Specifications: FORD WSK-M4D648-A Color: Black Form: Pellets Processi..
Linear Mold Shrinkage, Flow 0.013 - 0.019 cm/cm
0.013 - 0.019 in/in
ASTM D955
PolyOne Dynaflex™ G2712-1000-02 Thermoplastic Elastomer (TPE)
Dynaflex™ G2712-1000-02 is an easy processing TPE designed for injection molding and extrusion aplications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - High..
Linear Mold Shrinkage, Flow 0.013 - 0.019 cm/cm
0.013 - 0.019 in/in
ASTM D955
PolyOne Dynaflex™ G7950-1 NSFG Thermoplastic Elastomer (TPE)
Dynaflex™ G7950-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,..
Linear Mold Shrinkage, Flow 0.013 - 0.019 cm/cm
0.013 - 0.019 in/in
ASTM D955
PolyOne Dynaflex™ G7950-1001-00 Thermoplastic Elastomer (TPE)
Dynaflex™ G7950-1001-00 is an easy processing, general purpose material designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypro..
Linear Mold Shrinkage, Flow 0.013 - 0.019 cm/cm
0.013 - 0.019 in/in
ASTM D955
PolyOne Dynaflex™ G7950-9 NSFG Thermoplastic Elastomer (TPE)
Dynaflex™ G7950-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,..
Linear Mold Shrinkage, Flow 0.015 - 0.019 cm/cm
0.015 - 0.019 in/in
ASTM D955
PolyOne Geon™ Vinyl Flexible A8000 Polyvinyl Chloride, Flexible (PVC, Flexible)
Recommended for interior applications.Information provided by PolyOne
Linear Mold Shrinkage, Flow 0.011 - 0.019 cm/cm
0.011 - 0.019 in/in
ASTM D955
PolyOne Dynaflex™ G7650-9 (Black) Thermoplastic Elastomer (TPE)
Dynaflex™ G7650-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl..
Linear Mold Shrinkage, Flow 0.015 - 0.019 cm/cm

@Thickness 3.17 mm
0.015 - 0.019 in/in

@Thickness 0.125 in
ASTM D955
Ravago Manufacturing Americas Enviramid™ N1300HL Nylon 66
Heat Stabilized, Lubricated, Black and made from EnViramid™ Post Consumer Recycled NylonInformation provided by Ravago.
Linear Mold Shrinkage, Flow 0.015 - 0.019 cm/cm

@Thickness 3.17 mm
0.015 - 0.019 in/in

@Thickness 0.125 in
ASTM D955
Ravago Manufacturing Americas Enviramid™ N1300THL BK Post Consumer Recycle Nylon 66
Impact Modified, Heat Stabilized, Lubricated, Black and Made from EnViramid Post Consumer Recycled NylonInformation provided by Ravago.
Linear Mold Shrinkage, Flow 0.015 - 0.019 cm/cm

@Thickness 3.17 mm
0.015 - 0.019 in/in

@Thickness 0.125 in
ASTM D955
Ravago Manufacturing Americas Enviramid™ N2300THL BK Post Consumer Recycle Nylon 6
Impact Modified, Heat Stabilized, Lubricated, Black and Made from EnViramid Post Consumer Recycled NylonInformation provided by Ravago.
Linear Mold Shrinkage, Flow 0.015 - 0.019 cm/cm

@Thickness 3.20 mm
0.015 - 0.019 in/in

@Thickness 0.126 in
ASTM D955
LG Chemical KEYFLEX BT 1072D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Linear Mold Shrinkage, Flow 0.015 - 0.019 cm/cm

@Thickness 3.20 mm
0.015 - 0.019 in/in

@Thickness 0.126 in
ASTM D955
LG Chemical KEYFLEX BT 1172D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical
Linear Mold Shrinkage, Flow 0.016 - 0.019 cm/cm
0.016 - 0.019 in/in
LATI Latigray 75/4-01 CX/45 PBT
Radiopaque compound based on Polybutylene Terephthalate (PBT). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by L..
Linear Mold Shrinkage, Flow 0.0155 - 0.019 cm/cm
0.0155 - 0.019 in/in
LATI Latilub 73/13-10T Y/15 POM, 15% Aramid Fiber Reinforced, PTFE Filled
Self-lubricating product based on Polyoxymethylene (POM). PTFE. Aramid fibersAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indust..
Linear Mold Shrinkage, Flow 0.017 - 0.019 cm/cm
0.017 - 0.019 in/in
on Tensile Bar; SABIC Method
SABIC Innovative Plastics LNP LUBRICOMP RL002 PA 66 (Europe-Africa-Middle East)
LNP* Verton* RL002 is a compound based on Nylon 66 resin containing PTFE.
Linear Mold Shrinkage, Flow 0.012 - 0.019 cm/cm

@Thickness 3.20 mm
0.012 - 0.019 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Valox® 7062 PBT+PET (Europe-Africa-Middle East)
Valox 7062 is Mineral filled PBT injection molding grade.
Linear Mold Shrinkage, Flow 0.012 - 0.019 cm/cm

@Thickness 3.20 mm
0.012 - 0.019 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Valox® 7062HP PBT
ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin.
Linear Mold Shrinkage, Flow 0.0060 - 0.019 cm/cm
0.0060 - 0.019 in/in
ASTM D955
Shinkong Synthetic Fibers Shinite® D202 PBT, Fire Retardant
Information from Shinkong Synthetic Fibers Corp.
Linear Mold Shrinkage, Flow 0.015 - 0.019 cm/cm
0.015 - 0.019 in/in
on Tensile Bar; SABIC Method
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA
NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability.
Linear Mold Shrinkage, Flow 0.0060 - 0.019 cm/cm
0.0060 - 0.019 in/in
ASTM D955
Shinkong Synthetic Fibers Shinite® D202 PBT, Fire Retardant
Information from Shinkong Synthetic Fibers Corp.
Linear Mold Shrinkage, Flow 0.015 - 0.019 cm/cm
0.015 - 0.019 in/in
DIS 294-4
Wellman Wellamid® FR1841-BK1 Nylon 66, Unfilled, Flame Retardant
All information provided by Wellman Engineered Resins.
Linear Mold Shrinkage, Flow 0.015 - 0.019 cm/cm
0.015 - 0.019 in/in
DIS 294-4
Wellman Wellamid® FR1841-N1 Nylon 66, Unfilled, Flame Retardant
All information provided by Wellman Engineered Resins.
Linear Mold Shrinkage, Flow 0.017 - 0.019 cm/cm
0.017 - 0.019 in/in
ISO DIS 294-4
Wellman Wellamid® NY1733-GY1 Lubricated, Nucleated, Unfilled Nylon 6
Description: Lubricated, Nucleated, Unfilled Nylon 6Information provided by Wellman.
Linear Mold Shrinkage, Flow 0.015 - 0.019 cm/cm
0.015 - 0.019 in/in
ISO DIS 294-4
Wellman Wellamid® XT1486-BK Medium Impact Nylon 66
Description: Medium Impact Nylon 66Information provided by Wellman.
Linear Mold Shrinkage, Flow 0.017 - 0.019 cm/cm
0.017 - 0.019 in/in
ASTM D955
Solvay Specialty Polymers Amodel® AT-1001L Polyphthalamide (PPA)  (Unverified Data**)
Amodel AT-1001L is an unreinforced, impact modified polyphthalamide (PPA) resin that exhibits exceptional impact strength at temperatures ranging from room temperature to as low as -40°F (-40°C), ..