| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage, Flow | 0.017 - 0.021 cm/cm | 0.017 - 0.021 in/in | ASTM D955 |
|
PolyOne Versaflex™ OM 6160-1 Thermoplastic Elastomer (TPE)
Versaflex™ OM 6160-1 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Excell..
|
|||
| Linear Mold Shrinkage, Flow | 0.017 - 0.021 cm/cm | 0.017 - 0.021 in/in | ASTM D955 |
|
PolyOne Versaflex™ OM 6160-9 Thermoplastic Elastomer (TPE)
Versaflex™ OM 6160-9 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Excell..
|
|||
| Linear Mold Shrinkage, Flow |
0.017
-
0.021
cm/cm @Thickness 3.17 mm |
0.017
-
0.021
in/in @Thickness 0.125 in |
ASTM D955 |
|
Ravago Manufacturing Americas Hylon® N1200THL BK Nylon 6/6
Available in North America Additive: Heat Stabilizer, Impact Modifier and Lubricant Features: Lubricated, Impact Modified and Heat StabilizedRoHS CompliantForm: Pellets Color: BlackInformation prov..
|
|||
| Linear Mold Shrinkage, Flow | 0.013 - 0.021 cm/cm | 0.013 - 0.021 in/in | ASTM D955 |
|
PolyOne Dynaflex™ G7630-1 (Natural) Thermoplastic Elastomer (TPE)
Dynaflex™ G7630-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhe..
|
|||
| Linear Mold Shrinkage, Flow | 0.013 - 0.021 cm/cm | 0.013 - 0.021 in/in | ASTM D955 |
|
PolyOne Dynaflex™ G7630-9 (Black) Thermoplastic Elastomer (TPE)
Dynaflex™ G7630-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. *Made with Kraton® Polymer - Non..
|
|||
| Linear Mold Shrinkage, Flow | 0.013 - 0.021 cm/cm | 0.013 - 0.021 in/in | ASTM D955 |
|
PolyOne Dynaflex™ G7930-1001-00 Thermoplastic Elastomer (TPE)
Dynaflex™ G7930-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhesion..
|
|||
| Linear Mold Shrinkage, Flow | 0.013 - 0.021 cm/cm | 0.013 - 0.021 in/in | ASTM D955 |
|
PolyOne Dynaflex™ G7930-9001-02 Thermoplastic Elastomer (TPE)
Dynaflex™ G7930-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhesion..
|
|||
| Linear Mold Shrinkage, Flow | 0.013 - 0.021 cm/cm | 0.013 - 0.021 in/in | ASTM D955 |
|
PolyOne Dynaflex™ G7940-9 NSFG Thermoplastic Elastomer (TPE)
Dynaflex™ G7940-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,..
|
|||
| Linear Mold Shrinkage, Flow | 0.013 - 0.021 cm/cm | 0.013 - 0.021 in/in | ASTM D955 |
|
PolyOne Dynaflex™ G7640-1 (Natural) Thermoplastic Elastomer (TPE)
Dynaflex™ G7640-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhe..
|
|||
| Linear Mold Shrinkage, Flow | 0.017 - 0.021 cm/cm | 0.017 - 0.021 in/in | ASTM D955 |
|
PolyOne Geon™ Vinyl Flexible C8000 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
|
|||
| Linear Mold Shrinkage, Flow | 0.017 - 0.021 cm/cm | 0.017 - 0.021 in/in | ASTM D955 and ISO 294-4 |
|
Ravago Manufacturing Americas Hylon® N1000STHL HF Nylon 6/6
(discontinued **)
Available in North America Additive: Heat Stabilizer and LubricantFeatures: Lubricated, Heat Stabilized, High Flow and Ultra High ToughnessRoHS CompliantAuto Specifications: DELPHI DCM 4849 Color: B..
|
|||
| Linear Mold Shrinkage, Flow |
0.017
-
0.021
cm/cm @Thickness 3.17 mm |
0.017
-
0.021
in/in @Thickness 0.125 in |
ASTM D955 |
|
Ravago Manufacturing Americas Hylon® N1000STHL UV2 Nylon 6/6
(discontinued **)
Available in North America Additive: Heat Stabilizer, Lubricant and UV StabilizerFeatures: Good Toughness, Lubricated, Heat StabilizedRoHS CompliantAuto Specifications: GM GMP.PA66.074 Color: BlackF..
|
|||
| Linear Mold Shrinkage, Flow |
0.017
-
0.021
cm/cm @Thickness 3.20 mm |
0.017
-
0.021
in/in @Thickness 0.126 in |
ASTM D955 |
|
LG Chemical LUCEL FW715CS Modified POM, Friction Resistance, Abrasion Resistance
Feature: Injection Molding, Modified POM, Friction Resistance, Abrasion ResistanceApplication: Gears, Printer Roller Pumps, Gear Worm WheelsCAS No. 66455-31-0 and 471-34-1Information provided by LG ..
|
|||
| Linear Mold Shrinkage, Flow |
0.018
-
0.021
cm/cm @Thickness 3.20 mm |
0.018
-
0.021
in/in @Thickness 0.126 in |
ASTM D955 |
|
LG Chemical LUCEL N109LD POM, Chemical Resistance
Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical
|
|||
| Linear Mold Shrinkage, Flow |
0.018
-
0.021
cm/cm @Thickness 3.20 mm |
0.018
-
0.021
in/in @Thickness 0.126 in |
ASTM D955 |
|
LG Chemical LUCEL N109LDS POM, Chemical Resistance
Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical
|
|||
| Linear Mold Shrinkage, Flow |
0.018
-
0.021
cm/cm @Thickness 3.20 mm |
0.018
-
0.021
in/in @Thickness 0.126 in |
ASTM D955 |
|
LG Chemical LUCEL N145LD POM, Chemical Resistance
Feature: Injection Molding, POM, Chemical ResistanceApplication: Electric/Electronic Gears, Automobile speaker HousingCAS No. 66455-31-0Information provided by LG Chemical
|
|||
| Linear Mold Shrinkage, Flow |
0.020
-
0.021
cm/cm @Thickness 3.20 mm |
0.020
-
0.021
in/in @Thickness 0.126 in |
ASTM D955 |
|
LG Chemical Lupox® DP1000DU PBT
Description: Injection Molding, PBT, General PurposeCAS No. 30965-26-5Information provided by LG Chemical
|
|||
| Linear Mold Shrinkage, Flow |
0.018
-
0.021
cm/cm @Thickness 3.20 mm |
0.018
-
0.021
in/in @Thickness 0.126 in |
ASTM D955 |
|
LG Chemical Lupox® SV1120M PBT
Description: Injection Molding, PBT, General Purpose, High ViscosityApplication: Films & Sheets, Optical Loose TubeCAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical
|
|||
| Linear Mold Shrinkage, Flow | 0.018 - 0.021 cm/cm | 0.018 - 0.021 in/in | |
|
LATI Latilub 75/4-20T PBT, PTFE Filled
Self-lubricating product based on Polybutylene Terephthalate (PBT). PTFE.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria ..
|
|||
| Linear Mold Shrinkage, Flow |
0.019
-
0.021
cm/cm @Thickness 3.20 mm |
0.019
-
0.021
in/in @Thickness 0.126 in |
SABIC Method |
|
SABIC Innovative Plastics Valox® 308 PBT
PBT, For compounding only. Not intended for Injection Molding. Melt viscosity: 250C at 21.6 kgf is 3500-4500.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Linear Mold Shrinkage, Flow |
0.012
-
0.021
cm/cm @Thickness 3.20 mm |
0.012
-
0.021
in/in @Thickness 0.126 in |
ASTM D955 |
|
Samsung Cheil Industries Infino® GP-5000 PBT, Unreinforced
General PBT material that can be used for connectorsInformation provided by Samsung Cheil Industries.
|
|||
| Linear Mold Shrinkage, Flow | 0.017 - 0.021 cm/cm | 0.017 - 0.021 in/in | ISO DIS 294-4 |
|
Wellman Wellamid® 22LHI3 XE-NBK1 Impact Modified Engineering Nylon 66
Description: Impact Modified Engineering Nylon 66Information provided by Wellman.
|
|||
| Linear Mold Shrinkage, Flow | 0.011 - 0.021 cm/cm | 0.011 - 0.021 in/in | ASTM D955 |
|
Elastocon TPE Technologies Elastocon® 8068B Thermoplastic Elastomer
Elastocon® 8068B is a black thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8068B is well suited for consumer goods an..
|
|||
| Linear Mold Shrinkage, Flow | 0.0010 - 0.021 cm/cm | 0.0010 - 0.021 in/in | ASTM D955 |
|
Elastocon TPE Technologies Elastocon® 8068BL Thermoplastic Elastomer
Elastocon® 8068BL is a black lubricated thermoplastic elastomer formulated for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 8068BL is well sui..
|
|||
| Linear Mold Shrinkage, Flow | 0.011 - 0.021 cm/cm | 0.011 - 0.021 in/in | ASTM D955 |
|
Elastocon TPE Technologies Elastocon® 8068N Thermoplastic Elastomer
Elastocon® 8068N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8068N is FDA compliant and well suited..
|
|||
| Linear Mold Shrinkage, Flow | 0.019 - 0.021 cm/cm | 0.019 - 0.021 in/in | on Tensile Bar; ISO 294 |
|
Eurostar Staramide AST44 PA66, Impact Modified, Injection Molded
AST44 is a Low Temperature Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
|
|||
| Linear Mold Shrinkage, Flow |
0.019
-
0.021
cm/cm @Thickness 4.00 mm |
0.019
-
0.021
in/in @Thickness 0.157 in |
E2P method |
|
Eurostar Staramide PX06093 PA6, Impact Modified, Injection Molded
Staramide PX06093 is an UV Stabilized, Impact Modified Polyamide 6 Injection Molding Resin (also known as P1000HI020UVL)Information provided by Eurostar.
|
|||
| Linear Mold Shrinkage, Flow | 0.011 - 0.021 cm/cm | 0.011 - 0.021 in/in | ASTM D955 |
|
Elastocon TPE Technologies Elastocon® 8150B Thermoplastic Elastomer
Elastocon® 8150B is a black thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8150B is well suited for consumer goods a..
|
|||
| Linear Mold Shrinkage, Flow |
0.019
-
0.021
cm/cm @Time 86400 sec |
0.019
-
0.021
in/in @Time 24.0 hour |
ISO 294 |
|
SABIC Innovative Plastics LNP Thermotuf P1000EI3 PA 6 (Asia Pacific)
High Impact Nylon 6 compound containing Impact Modifier.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Linear Mold Shrinkage, Flow | 0.018 - 0.021 cm/cm | 0.018 - 0.021 in/in | |
|
LATI Later 4E61 PBT
Polybutylene Terephthalate (PBT). Toughened. Good impact resistance even at low temperature.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided..
|
|||