Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.022 cm/cm | 0.022 in/in | 60x60x2; 260°C / MT 80°C; 600 bar; ISO 294-4 |
Lanxess Pocan® B 5220 XF 000000 PBT, 20% Glass Spheres PBT, 20% glass spheres, injection molding, improved flowability, improved impact strength, low tendency to warpInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm @Thickness 3.17 mm |
0.022 in/in @Thickness 0.125 in |
1/8" Section |
Lucent Polymers POM-100 Acetal Copolymer, General Purpose, Injection Grade Add "U" for UV StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm @Thickness 3.17 mm |
0.022 in/in @Thickness 0.125 in |
1/8" Section |
Lucent Polymers POM-270 Acetal Copolymer, Easy Flow, Injection Grade Add "U" for UV StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm | 0.022 in/in | |
Solvay TECHNYL® B 230 PA66/6, DRY Description: Unreinforced and modified copolyamide 66/6, with high flexibility and improved impact resistance, for injection molding.Available in: Asia Pacific and EuropeProduct Applications: TECHN.. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm | 0.022 in/in | SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP YP003 Polyester Elastomer (Europe-Africa-Middle East) LNP* LUBRICOMP* YP003 is a compound based on Polyester Elastomer containing PTFE, Silicone. Added features include; Internally Lubricated. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm @Thickness 3.17 mm |
0.022 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® HDPE TM5 5% Talc Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 5% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm | 0.022 in/in | SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP KB008 Acetal Copolymer LNP THERMOCOMP* KB008 is a compound based on Acetal Copolymer resin containing 40% Glass Bead. |
|||
Linear Mold Shrinkage, Flow | 0.022 - 0.032 cm/cm | 0.022 - 0.032 in/in | ASTM D955 |
Elastocon TPE Technologies Elastocon® 2810 Thermoplastic Elastomer Elastocon® 2810 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® 2810 is FDA compliant and well suit.. |
|||
Linear Mold Shrinkage, Flow | 0.022 - 0.032 cm/cm | 0.022 - 0.032 in/in | ASTM D955 |
Elastocon TPE Technologies Elastocon® 2825 Thermoplastic Elastomer Elastocon® 2825 thermoplastic elastomer compound has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® 2825 is FDA compliant and .. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm | 0.022 in/in | ISO 294-4 |
DSM Stanyl® TS272A1 PA46-RF Aramid fiber reinforced, Wear and Friction Modified |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm | 0.022 in/in | annealed; ISO 294-4 |
DuPont Performance Polymers Crastin® S650FR NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)< Unreinforced Flame Retardant Polybutylene Terephthalate Crastin S650FR is an unreinforced flame retardant polybutylene terephthalate for injection molding.Information provided by DuPont Performance .. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm @Thickness 2.00 mm |
0.022 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
DuPont Performance Polymers Zytel® ST801AW BK195 Nylon 66
(Unverified Data**) Zytel® ST801AW BK195 is a Super Tough, weatherable, easy flow and processing friendly, black polyamide 66 resin for injection molding. It offers the best resistance to outdoor exposure.Information.. |
|||
Linear Mold Shrinkage, Flow | 0.022 - 0.024 cm/cm @Thickness 4.00 mm |
0.022 - 0.024 in/in @Thickness 0.157 in |
E2P method |
Eurostar Star L POM D51 POM, Injection Molded Star L POM D51 is a PTFE Lubricated, POM Copolymer Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.022 - 0.024 cm/cm @Thickness 4.00 mm |
0.022 - 0.024 in/in @Thickness 0.157 in |
E2P method |
Eurostar Starpylen HW 30K ECR-BK PP, Injection Molded Starpylen HW 30K ECR-BK is a reinforced Polypropylene with a low carbon footprint spherical filler, Injection Molding Resin (also known as HW30KECR)Information provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Clariant CA9000NAT` Acetal Copolymer Data provided by Clariant Masterbatches |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm | 0.022 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® 100 BK602 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and .. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm | 0.022 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® 100PE NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 100PE NC010 (formerly DE20573) is a high viscosity acetal homopolymer an enhanced version of Delrin 100P with very low VOC emissions... |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Ashley Polymers Ashlene® R190B Acetal General purpose reprocessed copolymer, excellent toughness, strength, stiffness and lubricity. Black. Available in UV stabilized grades: R190-B2 (good weatherability); R190-H2B (maximum weatherab.. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Ashley Polymers Ashlene® RH190H2-B Acetal General purpose, reprocessed homopolymer, excellent toughness, strength, stiffness and lubricity. UV stabilized with carbon black for outstanding weatherability.Data provided by the manufacturer |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm @Diameter 2.00 mm |
0.022 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, Conditioned Availability:Asia PacificEuropeNorth AmericaAdditive: Lubricant Features:Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood Tou.. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm @Diameter 2.00 mm |
0.022 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, DAM Availability:Asia PacificEuropeNorth AmericaAdditive: Lubricant Features:Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood Tou.. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm @Diameter 2.00 mm |
0.022 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 67R Nylon 66, Heat Stabilized, Conditioned Vydyne® 67R is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 67R resin offers high strength, .. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Ashley Polymers Ashlene® R190H Acetal General purpose, reprocessed copolymer, excellent toughness, strength, stiffness and lubricity. UV stabilized for good weatherability. Available in Natural and Black. Natural: Designated R190H-N3.. |