Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Gravity = 0.780 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Specific Gravity 0.780 g/cc
0.780 g/cc
ASTM D297
Parker Chomerics ParPHorm® S1945-25 Non-Conductive Form-in-Place Gasket
Description: A range of conductive particle technologies combined with thermoset and RTV silicone systems provide a material selection for most opportunities. Multiple filler grades balance material..
Specific Gravity 0.780 - 0.790 g/cc
0.780 - 0.790 g/cc
Michelman® Topaz Indicator Solution
Description: Indicator solution for Topaz primed sheet substratesUsage: Topaz Indicator is designed to measure the uniformity of the coated substrate.Application data: 1. Soak a cotton pad with Topa..
Specific Gravity 0.780 g/cc
0.780 g/cc
Chesterton 274 Industrial Degreaser
Description: Chesterton® 274 Industrial Degreaser is an industrial strength, hard surface degreaser which will dissolve grease, oil, tar and other similar water insoluble soils generally encountere..
Specific Gravity 0.780 g/cc
<br>@Temperature 25.0 °C
0.780 g/cc
<br>@Temperature 77.0 °F
Dow Corning OS-2 SILICONE CLEANER & SURFACE PREP
Non Ozone depleting, VOC exempt, Silicone cleaner to clean Plastic and Metals, excellent for removing oils, silicone-based car wax and protectants.Information provided by Dow Corning
Specific Gravity 0.780 g/cc
0.780 g/cc
BCC Products BC 7020 Epoxy Backfill System
BC 7020 is a lightweight two component epoxy backfill system. Unlike BC 7010, the filler portion is pre-blended into the resin and hardener components for easier handling, thus simplifying the mixin..
Specific Gravity 0.780 g/cc
0.780 g/cc
ASTM-D-792-66
BCC Products DP-11-88 Urethane Adhesive
DP-11-88 is a medium viscosity quick setting easy to use urethane adhesive. This system was specifically designed to bond together the MB2001/MB3000 Model/Tooling Board to create desired dimensions ..
Specific Gravity 0.780 g/cc
0.780 g/cc
Parker Chomerics CHO-SHIELD® 1091 Adhesion Promoter for Conductive Polyurethane Coatings
Information provided by Chomerics
Specific Gravity 0.780 g/cc
0.780 g/cc
Shin-Etsu Silicones Primer 4 Elastomer
Primer 4 is a primer designed for bonding platinum or peroxide cure type silicone products to metals including aluminum and various plastics.Information Provided by Shin-Etsu Silicones of America, I..
Copyright © lookpolymers.com All Rights Reserved