Polymer Property : Specific Gravity = 0.800 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Specific Gravity 0.800 g/cc
0.800 g/cc
NextGen Adhesives G907-28 Potting Adhesive
Description: NGAC G907-28 is a medium viscosity adhesive system formulated with a spherical glass filler to provide light weight and low shrinkage performance.Advantages and Applications: The NGAC G..
Specific Gravity 0.800 g/cc
0.800 g/cc
Parker Chomerics CHO-BOND 1076, Part A Silicone
Information provided by Chomerics
Specific Gravity 0.800 - 0.880 g/cc
0.800 - 0.880 g/cc
712BNF Cork/Nitrile Rubber Sheet
Description: Harvested every 9-12 years from the cork oak tree, cork is able to rebound from compression with extrusion. Applications include: stoppers, soundproofing, flooring, gaskets, and many ot..
Specific Gravity 0.800 - 0.820 g/cc
0.800 - 0.820 g/cc
Michelman® Wax Dispersion 40 Solvent dispersion
Description: Solvent dispersion of paraffin waxUsage: Wax Dispersion 40 is most effective as a water repellent aid and also has some slip and release properties in solvent applications. Wax Dispersi..
Specific Gravity 0.800 g/cc
0.800 g/cc
20/20°C
LyondellBasell TEBOL® 99 High Purity TBA, Tertiary butyl alcohol
Information provided by Lyondell.
Specific Gravity 0.800 g/cc
0.800 g/cc
Mixed
Tra-Con Tra-Cast 3110 Low Density Epoxy Casting System
TRA-CAST 3110 is a unicellular, low density, syntactic-foam epoxy resin casting system of medium viscosity that easily handles, mixes and cures at room temperature. Developed for industrial encapsul..
Specific Gravity 0.800 g/cc
0.800 g/cc
Mixed
Tra-Con Tra-Bond 2125 Rigid Syntactic Repair Adhesive
TRA-BOND 2125 is a medium viscosity, low density syntactic foam epoxy formulation developed for industrial, electronic and aerospace honeycomb, fillet, edge-fill, contour repair, bonding and casting..
Specific Gravity 0.800 g/cc
0.800 g/cc
ASTM D792
Cheng Yu Plastic PE221 Flame Retardant LDPE
Specific Gravity 0.800 g/cc
0.800 g/cc
Chesterton 395 Tapping Lubricant
Description: Chesterton® 395 Tapping Lubricant is a high quality petroleum based machining lubricant specifically designed for aluminum and other soft metals. It is a high performance cutting fluid..
Specific Gravity 0.800 g/cc
0.800 g/cc
Chesterton 730 Spragrip®
Description: Chesterton® 730 Spragrip® is a premium quality, high performance belt dressing that will add up to 50% more pulling power and end belt slippage for all V, flat and round belts. 730 Sp..
Specific Gravity 0.800 g/cc
0.800 g/cc
Chesterton 775 Moisture Shield
Description: Chesterton® 775 Moisture Shield is a moisture displacing, clear protective coating that protects parts and equipment from corrosion for months. Sprayed on bare metal, it leaves a lubri..
Specific Gravity 0.800 g/cc
0.800 g/cc
Elisto THERMOSTAR® MD 80 Pattern material
Block materialInformation provided by elisto
Specific Gravity 0.800 g/cc
<br>@Temperature 25.0 °C
0.800 g/cc
<br>@Temperature 77.0 °F
Dow Corning 2-5088 Wax
Silicone wax (siloxane backbone with pendant C30 alkyl groups attached). In home and auto care applications, it combines the shine and durability associated with hard waxes, with features closer to ..