Polymer Property : Specific Gravity = 0.850 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Specific Gravity 0.850 - 0.910 g/cc
0.850 - 0.910 g/cc
ASTM D792
S&E Specialty Polymers TufFlex™ GTPO8290 Natural TPO Compound
Application: An olefin based insulation & jacketing , 105°C rated compound formulated with excellent deformation characteristics. (SEW, SJEW)Information provided by S&E Specialty Polymers
Specific Gravity 0.850 - 0.950 g/cc
0.850 - 0.950 g/cc
COR12V Cork/Neoprene Rubber Sheet
Description: Harvested every 9-12 years from the cork oak tree, cork is able to rebound from compression with extrusion. Applications include: stoppers, soundproofing, flooring, gaskets, and many ot..
Specific Gravity 0.850 - 0.870 g/cc
0.850 - 0.870 g/cc
Michelman® Michem® Dispersion 275P Solvent dispersion of petroleum derived hydrocarbon
Description: Solvent dispersion of petroleum derived hydrocarbonUsage: Michem® Dispersion 275P is designed to be used as a slip aid and scratch resistant additive in coil coatings.Information pro..
Specific Gravity 0.850 - 0.950 g/cc
0.850 - 0.950 g/cc
ASTM D792
Loxim 800 00 HB Polypropylene Compound, Flame Retardant
Information provided by Loxim Industries
Specific Gravity 0.850 g/cc
0.850 g/cc
Momentive Performance Materials SS4004P Silicone Primer for use with RTV Silicone Adhesive Sealants, Pink
SS4004P, SS4044P, SS4120, SS4155, and SS4179 primers are formulated for use with GE Silicones RTV silicone rubber adhesive sealants.  GE Silicones one-component products offer primerless adhesion..
Specific Gravity 0.850 g/cc
0.850 g/cc
Momentive Performance Materials SS4044P Silicone Primer for use with RTV Silicone Adhesive Sealants, Light Yellow
SS4004P, SS4044P, SS4120, SS4155, and SS4179 primers are formulated for use with GE Silicones RTV silicone rubber adhesive sealants.  GE Silicones one-component products offer primerless adhesion..
Specific Gravity 0.850 g/cc
0.850 g/cc
d<sup>20</sup><sub>4</sub>; Anton Paar density meter
Mitsui LUCANTâ„¢ HC-2000 Synthetic Oil
LUCANT®, a hydrocarbon-based synthetic oil having no polar groups, is a co-oligomer of ethylene and -olefin. It possesses surpassing resistance to heat and cold and lower dependence of viscosity..
Specific Gravity 0.850 g/cc
0.850 g/cc
ASTM D792
Spartech SparAlloy Rigid Foamed ABS Specialty Sheet
Description: Specialty SheetInformation provided by Spartech.
Specific Gravity 0.850 g/cc
0.850 g/cc
15°C; ASTM D1298
ExxonMobil Gargoyle Arctic 230 SHC 200 Series
Gargoyle Arctic SHC 200 Series are fully synthetic, supreme performance lubricants, specifically designed for use in refrigeration compressors and heat pumps. They are formulated from wax-free, synt..
Specific Gravity 0.850 g/cc
0.850 g/cc
15°C; ASTM D1298
ExxonMobil Gargoyle Arctic 234 SHC 200 Series
Gargoyle Arctic SHC 200 Series are fully synthetic, supreme performance lubricants, specifically designed for use in refrigeration compressors and heat pumps. They are formulated from wax-free, synt..
Specific Gravity 0.850 g/cc
0.850 g/cc
Chesterton 438 PTFE Coating
Description: Chesterton® 438 PTFE Coating represents the best combination of clean, dry, PTFE – based powder lubricant with a tough, protective coating that resists water and chemicals. It does mu..
Specific Gravity 0.850 g/cc
<br>@Temperature 25.0 °C
0.850 g/cc
<br>@Temperature 77.0 °F
Dow Corning MOLYKOTE® G 68
Semi-synthetic greaseInformation provided by Dow Corning
Specific Gravity 0.850 g/cc
<br>@Temperature 25.0 °C
0.850 g/cc
<br>@Temperature 77.0 °F
Dow Corning OS-30
Information provided by Dow Corning
Specific Gravity 0.850 g/cc
<br>@Temperature 25.0 °C
0.850 g/cc
<br>@Temperature 77.0 °F
Dow Corning SYL-OFF® 294 COATING
Syl-Off® 294 Coating is one of several alternative base polymers for use in Syl-Off solvent-based, tin-catalyzed release coatings. It is a 40 percent solids dispersion of a blend of reactive silox..
Specific Gravity 0.850 g/cc
<br>@Temperature 25.0 °C
0.850 g/cc
<br>@Temperature 77.0 °F
Dow Corning XIAMETER® PMCPPMX-1184 Silicone Fluid
Is chemically equivalent to DOW CORNING® 2-1184 FLUID. A mixture of volatile linear polydimethylsiloxane for use in skincare, suncare, color cosmetic, haircare, and antiperspirant / deodorant appli..
Specific Gravity 0.850 g/cc
0.850 g/cc
15°C; ASTM D4052
ExxonMobil 624 Mobil SHC 600 Series
Mobil SHC 600 Series lubricants are good performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are for..
Specific Gravity 0.850 g/cc
0.850 g/cc
15°C; ASTM D4052
ExxonMobil 625 Mobil SHC 600 Series
Mobil SHC 600 Series lubricants are supreme performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are ..
Specific Gravity 0.850 g/cc
0.850 g/cc
15°C; ASTM D1298
ExxonMobil Gargoyle Arctic 230 SHC 200 Series
Gargoyle Arctic SHC 200 Series are fully synthetic, supreme performance lubricants, specifically designed for use in refrigeration compressors and heat pumps. They are formulated from wax-free, synt..
Specific Gravity 0.850 g/cc
<br>@Temperature 25.0 °C
0.850 g/cc
<br>@Temperature 77.0 °F
Dow Corning 200® 1.5 CST FLUID
A polydimethylsiloxane polymer for use in skincare, suncare, woundcare, hair care, and color cosmetic applications.Information provided by Dow Corning
Specific Gravity 0.850 g/cc
0.850 g/cc
60°F; ASTM D-1298
ConocoPhillips ANDEROL® FGC 150 Compressor Fluid, Synthetic Food Grade ISO 150
Description: ANDEROL FGC 150 Compressor Fluid is a synthetic hydrocarbon (PAO) based lubricant formulated with special additive packages that provide good thermal and oxidative stability to keep val..
Specific Gravity 0.850 g/cc
<br>@Temperature 25.0 °C
0.850 g/cc
<br>@Temperature 77.0 °F
Dow Corning XIAMETER® PMCPPMX-200 1.5CS Silicone Fluid
Is chemically equivalent to DOW CORNING® 200 FLUID 1.5CS. A polydimethylsiloxane polymer for use in skincare, suncare, woundcare, hair care, and color cosmetic applications. INCI Name: DimethiconeI..
Specific Gravity 0.850 g/cc
<br>@Temperature 25.0 °C
0.850 g/cc
<br>@Temperature 77.0 °F
Dow Corning 2503 Cosmetic Wax
An alkylmethylsiloxane wax which melts on contact with skin and provides moisturizing benefits for hand lotions, body creams, facial treatments, suncare creams / lotions, woundcare, scar therapy tre..
Specific Gravity 0.850 g/cc
0.850 g/cc
60°F; ASTM D-1298
ConocoPhillips ANDEROL® 6100 Synthetic Food Grade Gear Fluid
Description: ANDEROL 6000 Series Food Grade Gear Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the ..
Specific Gravity 0.850 g/cc
0.850 g/cc
ASTM D3574
Azdel SuperLite® SL550700-100 PP Resin Matrix / 55% Glass Fiber (1 mm Molded Thickness)
AZDEL SuperLite® SL550700-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Specific Gravity 0.850 g/cc
0.850 g/cc
Aremco Aremco-Bond™ 568 High Performance Epoxide
Aluminum-Filled, 1:1, Good Bond Strength and High Thermal Conductivity.
Specific Gravity 0.850 g/cc
0.850 g/cc
15°C; ASTM D1298
ExxonMobil Gargoyle Arctic 234 SHC 200 Series
Gargoyle Arctic SHC 200 Series are fully synthetic, supreme performance lubricants, specifically designed for use in refrigeration compressors and heat pumps. They are formulated from wax-free, synt..
Specific Gravity 0.850 g/cc
0.850 g/cc
15°C; ASTM D4052
ExxonMobil 625 Mobil SHC 600 Series
Mobil SHC 600 Series lubricants are supreme performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are ..
Specific Gravity 0.850 g/cc
0.850 g/cc
QSil 12C
ACC QSil 12 QSI Quantum Silicones Clear Low Viscosity for Potting Material
QSil 12 is a clear, transparent, low viscosity, two-component, liquid silicone material which cures at room temperature and is primarily intended for potting applications. This material is typically..
Specific Gravity 0.850 g/cc
0.850 g/cc
15°C; ASTM D4052
ExxonMobil 624 Mobil SHC 600 Series
Mobil SHC 600 Series lubricants are good performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are for..
Copyright © lookpolymers.com All Rights Reserved