Polymer Property : Specific Gravity = 0.884 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Specific Gravity 0.884 g/cc
0.884 g/cc
15.6°C; ASTM D1298
ExxonMobil 100 Mobil DTE PM Series
Mobil DTE PM Series products are high-quality, high-performance lubricants specifically designed for demanding industrial paper machine circulating systems. They are engineered to provide exceptiona..
Specific Gravity 0.884 g/cc
0.884 g/cc
15.6°C; ASTM D1298
ExxonMobil 100 Mobil DTE PM Series
Mobil DTE PM Series products are high-quality, high-performance lubricants specifically designed for demanding industrial paper machine circulating systems. They are engineered to provide exceptiona..
Specific Gravity 0.884 g/cc
0.884 g/cc
60°F
ConocoPhillips Conoco® El Mar® 2000 Oil SAE Grade 30
Conoco® El Mar 2000 is a high-quality, very low-ash, dispersant detergent gas engine oil designed for use in naturally aspirated and moderately turbocharged, low- to medium-speed 2-stroke cycle and..
Specific Gravity 0.884 g/cc
0.884 g/cc
60°F
ConocoPhillips El Mar® 3000 Oil SAE Grade 30
Description: Conoco El Mar® 3000 Oil is a quality, low ash gas engine oil recommended for naturally aspirated and moderately turbocharged, four cycle, low-, medium- and high-speed gas engines, such..
Specific Gravity 0.884 g/cc
0.884 g/cc
60°F
ConocoPhillips El Mar® 3000 Oil SAE Grade 40
Description: Conoco El Mar® 3000 Oil is a quality, low ash gas engine oil recommended for naturally aspirated and moderately turbocharged, four cycle, low-, medium- and high-speed gas engines, such..
Specific Gravity 0.884 g/cc
0.884 g/cc
60°F
ConocoPhillips 220 Bearing Oil
Description: Conoco Bearing Oil is formulated for the circulating systems that lubricate roll-neck bearings in steel and nonferrous rolling mills. It is suited for systems in which water and corrosi..