| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 0.930 g/cc | 0.930 g/cc | 23/23°C; ASTM D792 |
|
RheTech Products FT1100-689UV Thermoplastic Polyolefin, UV Stabilized, Light Natural Beige
Applications: Pillar plugsAirbag doorsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Specific Gravity | 0.930 g/cc | 0.930 g/cc | 23/23°C; ASTM D792 |
|
RheTech Products FT3080-727UV Thermoplastic Polyolefin, UV Stabilized, G01 Black
Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Specific Gravity | 0.930 g/cc | 0.930 g/cc | 23/23°C; ASTM D792 |
|
RheTech Products FT4600-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Scuff platesInterior trimI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Specific Gravity | 0.930 g/cc | 0.930 g/cc | ASTM D792 |
|
Quadrant EPP TIVAR® 1000 UV Stabilized UHMW-PE, Natural & Colored Except Black (ASTM Product Data Sheet) |
|||
| Specific Gravity | 0.930 g/cc | 0.930 g/cc | ASTM D792 |
|
Quadrant EPP Tivar® Premium UHMW-PE Tivar Premium UHMW-PE |
|||
| Specific Gravity | 0.930 g/cc | 0.930 g/cc | 23°C; ASTM D792 |
|
ExxonMobil Santoprene® 8291-70PA Thermoplastic Elastomer
(discontinued **)
A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PA-6 and blends thereof for applications where hard/s..
|
|||
| Specific Gravity | 0.930 - 0.940 g/cc | 0.930 - 0.940 g/cc | |
|
Inhance Fluoro-Seal INHANCE® UH-1045 Ultra High Molecular Weight Polyethylene
Product Description: INHANCE UH-1000 series particles are surface-activated Ultra High Molecular Weight Polyethylene (UHMWPE) in powder form. Surface activation makes the particles easy to disperse..
|
|||
| Specific Gravity | 0.930 - 0.940 g/cc | 0.930 - 0.940 g/cc | |
|
Inhance Fluoro-Seal INHANCE® UH-1500 Ultra High Molecular Weight Polyethylene
Product Description: INHANCE UH-1000 series particles are surface-activated Ultra High Molecular Weight Polyethylene (UHMWPE) in powder form. Surface activation makes the particles easy to disperse..
|
|||
| Specific Gravity | 0.930 - 0.940 g/cc | 0.930 - 0.940 g/cc | |
|
Inhance Fluoro-Seal INHANCE® UH-1700 Ultra High Molecular Weight Polyethylene
Product Description: INHANCE UH-1000 series particles are surface-activated Ultra High Molecular Weight Polyethylene (UHMWPE) in powder form. Surface activation makes the particles easy to disperse..
|
|||
| Specific Gravity | 0.930 g/cc | 0.930 g/cc | ASTM D792 |
|
SABIC Innovative Plastics NORYL WCP700 PPE-TPE
Flexible PPE-TPE injection grade suitable for over-molding applications such as plugs, strain relief's, and connectors. Good processability. 70 Shore A hardness.
|
|||
| Specific Gravity | 0.930 g/cc | 0.930 g/cc | |
|
Struktol TR 131 Slip Agent, Lubricant, Mold Release Agent
Unsaturated primary amide derived from erucic acid.STRUKTOL® TR 131 is mainly used as a slip agent in polyolefin films, reducing the coefficient of friction. It is the agent of choice at higher e..
|
|||
| Specific Gravity | 0.930 g/cc | 0.930 g/cc | |
|
Teknor Apex Elexar® EL-8431 Thermoplastic Elastomer
Notes: Sunlight Resistant; Temperature Rating: 105°C Processing Method: Extrusion; Injection MoldingInformation Provided by Teknor Apex
|
|||
| Specific Gravity | 0.930 g/cc | 0.930 g/cc | ASTM D792 |
|
Teknor Apex Monprene® MP-2602G Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Specific Gravity | 0.930 g/cc | 0.930 g/cc | |
|
Teknor Apex Tekbond® TB 1339A Thermoplastic Elastomer
Notes: Tekbond® TPEs are a functional series of elastomer compounds designed to not only bond to the most difficult neat and reinforced engineering substrates with no primer or surface treatment, b..
|
|||
| Specific Gravity | 0.930 - 0.960 g/cc | 0.930 - 0.960 g/cc | |
|
Westlake Epolene® E-10 Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer
Epolene® E-Type Polymers are easily emulsifiable, available in PE and PP based materials, and approved by the FDA for food contact. They have a wide ring & ball softening point range, oil and water..
|
|||
| Specific Gravity | 0.930 - 0.960 g/cc | 0.930 - 0.960 g/cc | |
|
Westlake Epolene® EE-2 Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer
Product Description: EE-2 is a medium density, low molecular-weight oxidized polyethylene with exceptional hardness. It is an excellent asphalt modifier which mixes readily with all asphalts. It h..
|
|||
| Specific Gravity | 0.930 g/cc | 0.930 g/cc | ASTM D792 |
|
A. Schulman POLYBATCH™ ABPP-05 Antiblock Concentrate
DescriptionPOLYBATCH® ABPP-05 Antiblock is an antiblock concentrate containing 5% synthetic silica based in homopolymer polypropylene. This masterbatch is designed to provide high clarity, low haz..
|
|||
| Specific Gravity | 0.930 g/cc | 0.930 g/cc | ASTM D792 |
|
Teknor Apex Uniprene® UN-2420A Thermoplastic Vulcanizate
Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex..
|
|||
| Specific Gravity |
0.930
g/cc @Temperature 25.0 °C |
0.930
g/cc @Temperature 77.0 °F |
|
|
Dow Corning Z-6264 SILANE
Dow Corning® Z-6264 Silane is an alkylalkoxysilane. It has an n-propyl organic group and a trimethoxysilyl inorganic group.Information provided by Dow Corning
|
|||
| Specific Gravity | 0.930 g/cc | 0.930 g/cc | |
|
ExxonMobil Exxon™ 2222 Regular Cure Rate Grade
Exxon Bromobutyl is a brominated copolymer of isobutylene and isoprene. The product for is white to light amber bales.Information provided by ExxonMobil Chemical
|
|||
| Specific Gravity | 0.930 g/cc | 0.930 g/cc | 23°C; ASTM D792 |
|
ExxonMobil Santoprene® 8211-65 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif..
|
|||
| Specific Gravity | 0.930 g/cc | 0.930 g/cc | ASTM D792 and ISO 1183 |
|
ExxonMobil Santoprene® 8221-55M300 Thermoplastic Vulcanizate - UV Resistant
Product Description: A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for automotive interior applications requ..
|
|||
| Specific Gravity | 0.930 g/cc | 0.930 g/cc | DIN 53 479 |
|
Hippe PE 1000 Polyethylene
Tough, flexible and stiff, depending on the crystalline structure (density). Resinous surface. Excellent dielectric properties, Good resistance against solvents, acids and alkalis. Physiologicall..
|
|||
| Specific Gravity | 0.930 g/cc | 0.930 g/cc | ASTM D792/ISO 1183 |
|
Braskem UTEC® 5040 Ultra High Molecular Weight Polyethylene
Applications which require high wear resistance - technical parts, RAM extruded and compression molded sheets, rods and profiles.Information provided by Braskem.
|
|||
| Specific Gravity | 0.930 g/cc | 0.930 g/cc | ASTM D792/ISO 1183 |
|
Braskem UTEC® 6540 Ultra High Molecular Weight Polyethylene
Applications which require highest wear resistance - technical parts, RAM extruded and/or compression molded sheets, rods and profiles.Information provided by Braskem.
|
|||
| Specific Gravity | 0.930 g/cc | 0.930 g/cc | ASTM D792 |
|
Teknor Apex Monprene® MP-2691A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||