| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 0.970 g/cc | 0.970 g/cc | Part B |
|
Resinlab® EP324E Clear Two Part Epoxy Casting Resin
Resinlab™ EP 324E Clear is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wettin..
|
|||
| Specific Gravity | 0.970 - 0.990 g/cc | 0.970 - 0.990 g/cc | |
|
Michelman® Michem® Emulsion 62330 Anionic paraffin/polyethylene emulsion
Description: Anionic paraffin/polyethylene emulsionUsage: Michem® Emulsion 62330 is a fine particle sized emulsion that provides excellent water repellency when added to varnishes and other coati..
|
|||
| Specific Gravity | 0.970 - 0.990 g/cc | 0.970 - 0.990 g/cc | |
|
Michelman® Michem® Prime 4983-40R Ethylene acrylic acid dispersion
Description: Ethylene acrylic acid dispersionUsage: Michem® Prime 498340R is a high solids, more economical version of Michem® Prime 4983R. Like Michem® Prime 4983R, this product provides o..
|
|||
| Specific Gravity | 0.970 - 0.990 g/cc | 0.970 - 0.990 g/cc | |
|
Michelman® Michem® Prime 4983R Ethylene acrylic acid dispersion
Description: Ethylene acrylic acid dispersionUsage: Michem® Prime 4983R provides outstanding adhesion to both metallic and cellulosic substrates, and enhances the water, grease, oil and solvent r..
|
|||
| Specific Gravity | 0.970 g/cc | 0.970 g/cc | ASTM D792 |
|
Fiberfil® J-60/10/E8 Polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
|
|||
| Specific Gravity | 0.970 g/cc | 0.970 g/cc | |
|
Struktol TR 060 Blending Aid, Processing Additive
A mixture of light-colored aliphatic resins with a molecular weight below 2,000.At process temperatures, STRUKTOL® TR 060 melt has a natural tackiness and this "adhesive" nature enables it to act..
|
|||
| Specific Gravity | 0.970 g/cc | 0.970 g/cc | ASTM D792 |
|
Teknor Apex Telcar® OBC 2419B Thermoplastic Elastomer
Notes: Telcar OBC has superior mechanical strength and higher elongation which will provide a tougher more durable finished product. Telcar OBC can be used in less demanding sealing applications. T..
|
|||
| Specific Gravity | 0.970 g/cc | 0.970 g/cc | ASTM D792 |
|
Teknor Apex UNIPRENE® 7010-64 Thermoplastic Elastomer
Information provided by Teknor Apex Company
|
|||
| Specific Gravity | 0.970 g/cc | 0.970 g/cc | ASTM D792 |
|
A. Schulman POLYBATCH™ Red LL50283/3 Concentrate Based In LLDPE
DescriptionPOLYBATCH® LL50283/3 is a red color concentrate based in LLDPE. This concentrate was designed to provide opacity and color in blow molding applications. POLYBATCH® LL50283/3 is heavy ..
|
|||
| Specific Gravity | 0.970 g/cc | 0.970 g/cc | ASTM D792 |
|
A. Schulman POLYBATCH™ Red LL50283/3 Concentrate Based In LLDPE
DescriptionPOLYBATCH® LL50283/3 is a red color concentrate based in LLDPE. This concentrate was designed to provide opacity and color in blow molding applications. POLYBATCH® LL50283/3 is heavy ..
|
|||
| Specific Gravity | 0.970 g/cc | 0.970 g/cc | ASTM D792 |
|
A. Schulman POLYFORT™ FPP 1602 Glass Reinforced, Chemically Coupled Homopolymer
DescriptionPolyfort® FPP 1602 is a 10% glass reinforced chemically coupled homopolymer.Information provided by A. Schulman.
|
|||
| Specific Gravity | 0.970 g/cc | 0.970 g/cc | ASTM D792 |
|
A. Schulman POLYFORT™ FPP 1609 Mica Fortified Copolymer Polypropylene
DescriptionPolyfort® FPP 1609 is a 10% mica fortified copolymer polypropylene product. Information provided by A. Schulman.
|
|||
| Specific Gravity | 0.970 g/cc | 0.970 g/cc | ASTM D792 |
|
A. Schulman POLYFORT™ 1602 UV-3120 UV Stabilized, Glass Reinforced Copolymer Polypropylene
DescriptionPolyfort® FPP 1602 UV-3120 is a black UV stabilized 10% chemically coupled glass reinforced copolymer polypropylene.Information provided by A. Schulman.
|
|||
| Specific Gravity | 0.970 g/cc | 0.970 g/cc | 15°C; ASTM D1298 |
|
ExxonMobil 46 Mobil EAL Arctic Series
Mobil EAL Arctic Series are high performance Environmental Awareness Lubricants (EAL) that are fully synthetic products designed specifically for the lubrication of refrigeration compressors and sys..
|
|||
| Specific Gravity | 0.970 g/cc | 0.970 g/cc | |
|
Dow Corning SYL-OFF® SL 700 COATING
Solvent-free, fast curing, provides extremely stable release, excellent bath stability, premium release at low peel speeds, requires catalyst additionInformation provided by Dow Corning
|
|||
| Specific Gravity | 0.970 g/cc | 0.970 g/cc | 23°C; ASTM D792 |
|
ExxonMobil Santoprene® 241-73W236 Thermoplastic Elastomer
A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and contains..
|
|||
| Specific Gravity |
0.970
g/cc <br>@Temperature 25.0 °C
|
0.970
g/cc <br>@Temperature 77.0 °F
|
|
|
Dow Corning XIAMETER® PMCPPMX-200 350CS Food Grade Silicone Fluid
Is chemically equivalent to DOW CORNING® 200 FLUID 350CS FOOD GRADE. 100% active, 350 cSt, Food grade, polydimethylsiloxane polymer.Information provided by Dow Corning
|
|||
| Specific Gravity |
0.970
g/cc <br>@Temperature 25.0 °C
|
0.970
g/cc <br>@Temperature 77.0 °F
|
|
|
Dow Corning 3-6512 A&B ELASTOMER
Two-part, transparent, 1:1, moderate heat cure, long pot life, cures to soft elastomer.Information provided by Dow Corning
|
|||
| Specific Gravity | 0.970 g/cc | 0.970 g/cc | "B" component |
|
ACC QGel 315 QSI Quantum Silicones General Purpose Silicone Gel
QGel 315 is a clear, very soft, tough moderately cross-linked silicone polymer. Silicone gels are used to provide protection from vibration and thermal or mechanical shock. Silicone gels also provid..
|
|||
| Specific Gravity | 0.970 g/cc | 0.970 g/cc | |
|
ATG s.r.l. NBR Nitrile-Butadiene Rubber |
|||
| Specific Gravity | 0.970 g/cc | 0.970 g/cc | ASTM D792 |
|
Asahi Kasei Thermylene® P-10TC-1777 10% Talc Filled, UV Stabilized Polypropylene
Information provided by Asahi Thermofil
|
|||
| Specific Gravity | 0.970 g/cc | 0.970 g/cc | ASTM D792 |
|
Asahi Kasei Thermylene® P6-10FG-0100 10% Glass Fiber Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
|
|||
| Specific Gravity |
0.970
g/cc <br>@Temperature 25.0 °C
|
0.970
g/cc <br>@Temperature 77.0 °F
|
|
|
Multibase Dow Corning® MB50-314 Siloxane Additive
DOW CORNING MB50-314 Masterbatch is a pelletized formulation containing 50% of an ultra-high molecular weight siloxane polymer dispersed in HDPE polymer. It is designed to be used as an additive in ..
|
|||
| Specific Gravity | 0.970 g/cc | 0.970 g/cc | 23°C; ASTM D792 |
|
ExxonMobil Santoprene® 181-64MED Thermoplastic Elastomer
(discontinued **)
A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of our medical grades. ..
|
|||
| Specific Gravity | 0.970 - 1.01 g/cc | 0.970 - 1.01 g/cc | ASTM D792 |
|
Buckeye Polymers BP RPP 1509 GK BLK Polypropylene, 15% Glass Filled
Product Information: 15% glass reinforced polypropyleneProduct Features:Offers improved flex modulus while maintaining a low specific gravity propertyChemically coupled for improvved physical proper..
|
|||