| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 0.977 g/cc | 0.977 g/cc | ISO 1183 |
|
Nanocyl PLASTICYL™ HDPE1501 High Density Polyethylene - Carbon Nanotube Masterbatch