| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 0.960 - 0.980 g/cc | 0.960 - 0.980 g/cc | |
|
Michelman® FiberMax® 5000 Water based medium treatment to replace paraffin wax
Description: Water based medium treatment to replace paraffin waxUsage: FibreMax® 5000 is a new alternative to paraffin wax for treating medium. It is a repulpable, machine ready fiber treatment ..
|
|||
| Specific Gravity | 0.960 - 0.980 g/cc | 0.960 - 0.980 g/cc | |
|
Michelman® Michem® Emulsion 09730 Cationic polyethylene emulsion
Description: Cationic polyethylene emulsionUsage: Michem® Emulsion 09730 is an additive to improve mar and scratch resistance. This product is used successfully for improving slip and reducing ma..
|
|||
| Specific Gravity | 0.960 - 0.980 g/cc | 0.960 - 0.980 g/cc | |
|
Michelman® Michem® Emulsion 48040M2 Nonionic microcrystalline wax emulsion
Description: Nonionic microcrystalline wax emulsionUsage: Michem® Emulsion 47950 is a wax emulsion which is effective as an anti-graffiti and sacrificial coating and can also contribute water res..
|
|||
| Specific Gravity | 0.960 - 0.980 g/cc | 0.960 - 0.980 g/cc | |
|
Michelman® Michem® Emulsion 80939M Nonionic paraffin wax emulsion
Description: Nonionic paraffin wax emulsionUsage: Michem® Emulsion 80939M provides excellent water resistance when used as an additive for Industrial coatings.We serve many markets through Michem..
|
|||
| Specific Gravity | 0.960 - 0.980 g/cc | 0.960 - 0.980 g/cc | |
|
Michelman® Michem® Emulsion 91735 Nonionic polypropylene emulsion
Description: Nonionic polypropylene emulsionUsage: Michem® Emulsion 91735 is a sizing polymer for fiberglass and other fibers used to reinforce polypropylene.We serve many markets through MichemÂ..
|
|||
| Specific Gravity | 0.950 - 0.980 g/cc | 0.950 - 0.980 g/cc | |
|
Michelman® Michem® Guard 1351 Nonionic based product of polyethylene wax
Description: Nonionic based product of polyethylene waxUsage: Michem® Guard 1351 is a water based dispersion which improves rub and abrasion resistance in pigmented coatings and semi-gloss coatin..
|
|||
| Specific Gravity | 0.960 - 0.980 g/cc | 0.960 - 0.980 g/cc | |
|
Michelman® Michem® Lube 124 Anionic microcrystalline wax emulsion
Description: Anionic microcrystalline wax emulsionUsage: Michem® Lube 124 as an additive provides release and acts as a detackifier for synthetic and natural rubber. Michem® Lube 124 is used s..
|
|||
| Specific Gravity | 0.960 - 0.980 g/cc | 0.960 - 0.980 g/cc | |
|
Michelman® Michem® Lube 270R Anionic paraffin/polyethylene wax emulsion
Description: Anionic paraffin/polyethylene wax emulsionUsage: Michem® Lube 270R is an additive which provides excellent water resistance in paint and coating formulations. This product is useful ..
|
|||
| Specific Gravity | 0.960 - 0.980 g/cc | 0.960 - 0.980 g/cc | |
|
Michelman® Resisto Coat™ 39AF Abrasion resistance coating
Description: Abrasion resistance coatingUsage: Resisto Coatâ„¢ 39AF provides excellent, economical abrasion protection. It is used throughout the appliance industry as a protective finish on corn..
|
|||
| Specific Gravity | 0.960 - 0.980 g/cc | 0.960 - 0.980 g/cc | |
|
Michelman® Michem® Emulsion 71731MOD Anionic paraffin emulsion
Description: Anionic paraffin emulsionUsage: Michem® Emulsion 71731MOD is an additive designed to provide excellent water resistance especially at higher temperatures. Michem® Emulsion 71731MO..
|
|||
| Specific Gravity | 0.960 - 0.980 g/cc | 0.960 - 0.980 g/cc | |
|
Michelman® Michem® Guard 349 Nonionic, polyethylene dispersion
Description: Nonionic, polyethylene dispersionUsage: Michem® Guard 349 is designed to impart rub resistance, block resistance and matting properties to aqueous paints, coatings and inks.Typical u..
|
|||
| Specific Gravity |
0.970
-
0.980
g/cc <br>@Temperature 25.0 °C
|
0.970
-
0.980
g/cc <br>@Temperature 77.0 °F
|
|
|
Dow Corning 3-4222 DIELECTRIC FIRM GEL KIT
Two-part, translucent green, firm, fast RT or heat cure, and primerless chemical adhesion.Information provided by Dow Corning
|
|||
| Specific Gravity |
0.970
-
0.980
g/cc <br>@Temperature 25.0 °C
|
0.970
-
0.980
g/cc <br>@Temperature 77.0 °F
|
|
|
Dow Corning 3-4241 DIELECTRIC TOUGH GEL KIT
Two-part, translucent green, RT or heat cure, UV indicator, long working time, tough primerless chemical adhesion, UL 94 V-1 flammability classification.Information provided by Dow Corning
|
|||