| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 0.990 g/cc | 0.990 g/cc | 23/23°C; ASTM D792 |
|
RheTech Products G13P100-332UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, (GM 9772) Light Neutral
Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Specific Gravity | 0.990 g/cc | 0.990 g/cc | 23/23°C; ASTM D792 |
|
RheTech Products G13P100-553UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, (GM 501F) Dark Smoke Gray
Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Specific Gravity | 0.990 g/cc | 0.990 g/cc | 23/23°C; ASTM D792 |
|
RheTech Products G13P100-589UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, (YR169L) Mild Beige
Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Specific Gravity | 0.990 g/cc | 0.990 g/cc | 23/23°C; ASTM D792 |
|
RheTech Products G13P100-598UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, (NH-293L) Seagull Gray
Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Specific Gravity | 0.990 g/cc | 0.990 g/cc | 23/23°C; ASTM D792 |
|
RheTech Products G13P100-724UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, NH220L Clear Gray
Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Specific Gravity | 0.990 g/cc | 0.990 g/cc | ASTM D792 |
|
Ovation Polymers SOFTAPLAS™ S 56A Thermoplastic Elastomer
Thermoplastic Elastomer – Excellent hydrolytic Stability and balance of properties. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are p..
|
|||
| Specific Gravity | 0.990 g/cc | 0.990 g/cc | 23/23°C; ASTM D792 |
|
RheTech Products M12P256-01 12% Mica Reinforced Polypropylene Copolymer, Black
Applications: Air damsAir ducts - distributionClose out panelsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Specific Gravity | 0.990 g/cc | 0.990 g/cc | ISO 1183 |
|
Solvay Engineered Polymers SEQUEL® 1514 Engineered Polyolefin
(discontinued **)
Description: SEQUEL® 1514 engineered polyolefin material is designed to provide significantly greater mar resistance than conventional TPOs. SEQUEL® 1514 polyolefin is designed for automotive app..
|
|||
| Specific Gravity | 0.990 - 1.00 g/cc | 0.990 - 1.00 g/cc | |
|
Michelman® Licomer® W 315 FP Anionic / Nonionic polyethylene emulsion
Description: Anionic / Nonionic polyethylene emulsionUsage: Licomer® W 315 FP is a high anti-slip emulsion suitable for floors, finishes on shoes, leather, etc.Information provided by MichelmanÂ..
|
|||
| Specific Gravity | 0.990 - 1.01 g/cc | 0.990 - 1.01 g/cc | |
|
Michelman® Michem® Emulsion 13025 Slip and anti-block additive
Description: Slip and anti-block additiveUsage: Michem® Emulsion 13025 provides slip and block resistance in a wide variety of coatings and formulas. It has a very broad global food contact compl..
|
|||
| Specific Gravity | 0.990 - 1.01 g/cc | 0.990 - 1.01 g/cc | |
|
Michelman® Michem® Emulsion 37135 Nonionic polyethylene emulsion
Description: Nonionic polyethylene emulsionUsage: Michem® Emulsion 37135 provides mar and scratch resistance as well as some slip resistance when used as an additive in polishes and coatings.We s..
|
|||
| Specific Gravity | 0.990 - 1.01 g/cc | 0.990 - 1.01 g/cc | |
|
Michelman® Michem® Emulsion 91240 Nonionic polyethylene emulsion
Description: Nonionic polyethylene emulsionUsage: Michem® Emulsion 91240 is an additive which provides excellent anti-blocking, slip properties and mar resistance. This product is also used as an..
|
|||
| Specific Gravity | 0.990 - 1.01 g/cc | 0.990 - 1.01 g/cc | |
|
Michelman® Michem® In-Line Primer 30 Primer
Description: Primer for Digital PrintingUsage: Michem® In-Line Primer 030 imparts a print-receptive surface to paper substrates to improve the ink transfer and adhesion of HP Indigo Electroinks. ..
|
|||
| Specific Gravity | 0.990 g/cc | 0.990 g/cc | ASTM D792 |
|
LG Chemical LUPOL HM-5204B High Modulus Polypropylene, 20% Polymer Alloy, High Strength, High Flow, High Modulus
LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner..
|
|||
| Specific Gravity | 0.990 g/cc | 0.990 g/cc | |
|
LG Chemical NBR 6280 High Acrylonitrile Polymer
Description: NBR 6280 is a copolymer of butadiene and acrylonitrile manufactured by advanced emulsion polymerization technology of Goodyear and LG Chem. NBR 6280 is a non staining, high mooney, and ..
|
|||
| Specific Gravity | 0.990 g/cc | 0.990 g/cc | |
|
Shin-Etsu Silicones KE-1052A/B Silicone, Gel RTV
Information Provided by Shin-Etsu Silicones of America, Inc.
|
|||
| Specific Gravity | 0.990 g/cc | 0.990 g/cc | ASTM D792 |
|
SABIC Innovative Plastics NORYL PPX PPX7115 PPE+PP (Asia Pacific)
High modulus/impact/heat PPE+PP.
|
|||
| Specific Gravity | 0.990 g/cc | 0.990 g/cc | ASTM D792 |
|
Teknor Apex Telcar® TL-1221A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
|
|||
| Specific Gravity | 0.990 - 0.996 g/cc | 0.990 - 0.996 g/cc | ASTM D792 |
|
A. Schulman POLYFORT™ FPP 2181HU High Flow, Fortified, Impact Resistant Polypropylene
DescriptionPolyfort® FPP 2181HU is a high flow, fortified, impact resistant polypropylene, stabilized for UV resistance, and available in automotive matched colors. Information provided by A. Schul..
|
|||
| Specific Gravity | 0.990 g/cc | 0.990 g/cc | ASTM D792 |
|
A. Schulman POLYFORT™ FPP 1902HU Talc Fortified Polypropylene
DescriptionPolyfort® FPP 1902 HU is a 10% talc fortified polypropylene. It exhibits high flow and is stabilized for UV resistance. Information provided by A. Schulman.
|
|||
| Specific Gravity | 0.990 - 0.996 g/cc | 0.990 - 0.996 g/cc | ASTM D792 |
|
A. Schulman POLYFORT™ FPP 2181HU High Flow, Fortified, Impact Resistant Polypropylene
DescriptionPolyfort® FPP 2181HU is a high flow, fortified, impact resistant polypropylene, stabilized for UV resistance, and available in automotive matched colors. Information provided by A. Schul..
|
|||
| Specific Gravity |
0.990
g/cc @Temperature 25.0 °C |
0.990
g/cc @Temperature 77.0 °F |
|
|
Dow Corning 62 PRINTERS' SOLUTION
55% active emulsion of medium viscosity polydimethylsiloxane fluid; contains antistat.Information provided by Dow Corning
|
|||
| Specific Gravity |
0.990
g/cc @Temperature 25.0 °C |
0.990
g/cc @Temperature 77.0 °F |
|
|
Dow Corning FZ-2233
Its primary function is to produce water-in-silicone and water-in-silicone and oil emulsions with a creamy and rich appearance but leaving a light, non greasy after feel on the skin. The addition le..
|
|||
| Specific Gravity |
0.990
g/cc @Temperature 25.0 °C |
0.990
g/cc @Temperature 77.0 °F |
|
|
Dow Corning SLYGARD® 3-6636 SILICONE DIELECTRIC GEL KIT
Two-part, transparent, LED encapsulant which is a lower-viscosity version of EG-6301.Information provided by Dow Corning
|
|||
| Specific Gravity |
0.990
g/cc @Temperature 25.0 °C |
0.990
g/cc @Temperature 77.0 °F |
|
|
Dow Corning SYL-OFF® 7689 CROSSLINKER
Syl-Off® 7689 Crosslinker is a solvent-free silicone crosslinker for polyester substrates.Information provided by Dow Corning
|
|||
| Specific Gravity | 0.990 g/cc | 0.990 g/cc | ASTM D471; ISO 2781 |
|
Advanced Polymer Alloys DuraGrip™ DGR 6060 NC Thermoplastic Elastomer (TPE)
DuraGrip® DGR 6060NC is designed to be a general purpose Thermoplastic Elastomer (TPE) that is easy to use in injection molding and extrusion processes. DGR 6060NC has an
excellent soft touch feel,..
|
|||
| Specific Gravity | 0.990 g/cc | 0.990 g/cc | 23°C; ASTM D792 |
|
ExxonMobil Vyram™ 9201-75 Thermoplastic Elastomer
(discontinued **)
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character..
|
|||
| Specific Gravity | 0.990 g/cc | 0.990 g/cc | ASTM D792 |
|
PolyOne Synprene® IT 62-002 BLACK 2001 Thermoplastic Elastomer - SBC
(discontinued **)
Description/Features:Over-Molding GradeUV StabilizedApplications: Multi-PurposeProcessing Method: Injection MoldingInformation provided by PolyOne Corporation
|
|||
| Specific Gravity | 0.990 g/cc | 0.990 g/cc | ASTM D792 |
|
PolyOne Synprene® RT-3615 Thermoplastic Elastomer - SBC
(discontinued **)
Description/Features:Multi-Purpose Thermoplastic ElastomerNaturalApplications:General PurposeInteriorMarket:Consumer GoodsIndustrialProcessing Method:Injection MoldingPolyOne First ChoiceInformation..
|
|||
| Specific Gravity | 0.990 g/cc | 0.990 g/cc | Part B; TM R050-16 |
|
Resinlab® EP1305 Black Highly Toughened Urethane Modified Epoxy
Resinlab™ EP1305 Black is a highly toughened urethane modified epoxy designed for bonding PVC, metals, ceramics and other difficult to bond substrates. The system has a thixotropic non-sag viscosi..
|
|||