| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 0.970 - 0.990 g/cc | 0.970 - 0.990 g/cc | ASTM D792 |
|
LG Chemical LUPOL TE5109 PP+Rubber+MF, High Impact
Description: Injection Molding, PP+Rubber+MF, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia, Rear Bumper Step)Information provided by LG Chemical
|
|||
| Specific Gravity | 0.970 - 0.990 g/cc | 0.970 - 0.990 g/cc | |
|
Michelman® Hydrolube™ 723 Paraffin wax emulsion
Description: Nonionic, paraffin wax emulsionUsage: Hydrolube™ 723 is used as a lubricant for fiber sizing applications.Information provided by Michelman®
|
|||
| Specific Gravity | 0.970 - 0.990 g/cc | 0.970 - 0.990 g/cc | |
|
Michelman® Michem® Emulsion 21030 Anionic polyethylene emulsion
Description: Anionic polyethylene emulsionUsage: Michem® Emulsion 21030 provides abrasion resistance and anti-blocking properties as well as slip resistance when used as an additive in floor poli..
|
|||
| Specific Gravity | 0.970 - 0.990 g/cc | 0.970 - 0.990 g/cc | |
|
Michelman® Michem® Emulsion 21930 Anionic Tung Oil emulsion
Description: Anionic Tung Oil emulsionUsage: Michem® Emulsion 21930 is a Tung Oil emulsion that contains 99.5% natural ingredients. It is used an additive that imparts good water bead to wood an..
|
|||
| Specific Gravity | 0.970 - 0.990 g/cc | 0.970 - 0.990 g/cc | |
|
Michelman® Michem® Emulsion 43240 Polypropylene emulsion
Description: Polypropylene emulsionUsage: Michem® Emulsion 43240 is best used as an additive in floor polish and overprint varnish formulations when a high degree of slip resistance is needed.We ..
|
|||
| Specific Gravity | 0.970 - 0.990 g/cc | 0.970 - 0.990 g/cc | |
|
Michelman® Michem® Emulsion 45745P Nonionic Polyethylene wax emulsion
Description: Nonionic Polyethylene wax emulsionUsage: Michem® Emulsion 45745P as an additive is recommended for use in floor polishes, semi-buffable coatings, mold release applications and other ..
|
|||
| Specific Gravity | 0.970 - 0.990 g/cc | 0.970 - 0.990 g/cc | |
|
Michelman® Michem® Emulsion 62330 Anionic paraffin/polyethylene emulsion
Description: Anionic paraffin/polyethylene emulsionUsage: Michem® Emulsion 62330 is a fine particle sized emulsion that provides excellent water repellency when added to varnishes and other coati..
|
|||
| Specific Gravity | 0.970 - 0.990 g/cc | 0.970 - 0.990 g/cc | |
|
Michelman® Michem® Emulsion 65435 Nonionic ethylene acrylic acid emulsion
Description: Nonionic ethylene acrylic acid emulsionUsage: Michem® Emulsion 65435 is an additive which provides good mar resistance and slip properties. This product is best used as an additive i..
|
|||
| Specific Gravity | 0.970 - 0.990 g/cc | 0.970 - 0.990 g/cc | |
|
Michelman® Michem® Guard 55 Nonionic polyethylene dispersion
Description: Nonionic polyethylene dispersionUsage: Michem® Guard 55 is a dispersion which provides mar and flatting properties when used as an additive in paint, coating, ink and graphic art for..
|
|||
| Specific Gravity | 0.970 - 0.990 g/cc | 0.970 - 0.990 g/cc | |
|
Michelman® Michem® Guard 7140 Anionic dispersion of polyethylene wax
Description: Anionic dispersion of polyethylene waxUsage: Michem® Guard 7140 is a water-based, large particle emulsion which improves rub and abrasion resistance in pigmented coatings and semi-gl..
|
|||
| Specific Gravity | 0.970 - 0.990 g/cc | 0.970 - 0.990 g/cc | |
|
Michelman® Michem® Lube 723 Nonionic paraffin wax emulsion
Description: Nonionic paraffin wax emulsionUsage: Michem® Lube 723 provides excellent water repellancy, lubricity, release and wood end check protection when used in the paint and coatings indust..
|
|||
| Specific Gravity | 0.970 - 0.990 g/cc | 0.970 - 0.990 g/cc | |
|
Michelman® Michem® Prime 4983-40R Ethylene acrylic acid dispersion
Description: Ethylene acrylic acid dispersionUsage: Michem® Prime 498340R is a high solids, more economical version of Michem® Prime 4983R. Like Michem® Prime 4983R, this product provides o..
|
|||
| Specific Gravity | 0.970 - 0.990 g/cc | 0.970 - 0.990 g/cc | |
|
Michelman® Michem® Prime 4983R Ethylene acrylic acid dispersion
Description: Ethylene acrylic acid dispersionUsage: Michem® Prime 4983R provides outstanding adhesion to both metallic and cellulosic substrates, and enhances the water, grease, oil and solvent r..
|
|||
| Specific Gravity | 0.970 - 0.990 g/cc | 0.970 - 0.990 g/cc | |
|
Michelman® Michem® Shield 422 Anionic dispersion of polyethylene wax
Description: Anionic dispersion of polyethylene waxUsage: Michem® Shield 422 provides superior rub resistance in graphic arts applications.Information provided by Michelman®
|
|||
| Specific Gravity | 0.970 - 0.990 g/cc | 0.970 - 0.990 g/cc | |
|
Michelman® Michem® Tite 445AF Skin packing / heat seal coating
Description: Skin packing / heat seal coatingUsage: Michem® Tite 445AF is a coating which bonds heavily printed corrugated to Surlyn or polyethylene skin pack films, firmly trapping the product i..
|
|||
| Specific Gravity | 0.970 - 0.990 g/cc | 0.970 - 0.990 g/cc | |
|
Michelman® Resisto Coat™ PLUS Abrasion resistance coating
Description: Abrasion resistance coatingUsage: Resisto Coatâ„¢ Plus is a low cost, dilute, non-abrasive coating. It is used throughout the appliance industry as a protective finish on cornerposts..
|
|||
| Specific Gravity | 0.980 - 0.990 g/cc | 0.980 - 0.990 g/cc | |
|
Lucite International Colacryl ® TS1173 Reactive Acrylic Syrup
Lucite® Colacryl® TS1173 is a reactive polymer solution containing dissolved polymers, plasticiser and a polymerisation activator.Information provided by Lucite International
|
|||
| Specific Gravity | 0.970 - 0.990 g/cc | 0.970 - 0.990 g/cc | |
|
Michelman® DigiPrime® 1500LA Primer
Description: Primer for digital printing on paper substratesUsage: DigiPrime®1500LA is a product that can be added to size press treatments or pigment coatings to optimize substrates for HP Indig..
|
|||
| Specific Gravity | 0.970 - 0.990 g/cc | 0.970 - 0.990 g/cc | |
|
Michelman® Michem® Guard 25 Nonionic, polyethylene dispersion
Description: Nonionic, polyethylene dispersionUsage: Michem® Guard 25 is a water based polyethylene dispersion which promotes mar resistance and flatting properties in paint and coating formulati..
|
|||
| Specific Gravity | 0.970 - 0.990 g/cc | 0.970 - 0.990 g/cc | |
|
Michelman® Michem® Guard 60 Nonionic Fischer-Tropsch dispersion
Description: Nonionic Fischer-Tropsch dispersionUsage: Michem® Guard 60 is a dispersion which provides mar resistance properties when used as an additive in paint, coating, ink and graphic art fo..
|
|||
| Specific Gravity | 0.970 - 0.990 g/cc | 0.970 - 0.990 g/cc | |
|
Michelman® Michem® Lube 103DI Anionic polyethylene emulsion
Description: Anionic polyethylene emulsionUsage: Michem® Lube 103DI is a wax emulsion additive which provides lubricity and mar resistance and is well suited for the glass and metal die industrie..
|
|||
| Specific Gravity | 0.970 - 0.990 g/cc | 0.970 - 0.990 g/cc | |
|
Michelman® Michem® Tite 242AF Skin packaging primer
Description: Skin packaging primerUsage: Michem® Tite 242AF is a coating designed to provide a tenacious bond between corrugated and either Surlyn or polyethylene clear skin pack films, firmly tr..
|
|||
| Specific Gravity | 0.970 - 0.990 g/cc | 0.970 - 0.990 g/cc | |
|
Michelman® Michem® Tite 335AF Skin packing / heat seal coating
Description: Skin packing / heat seal coatingUsage: Michem® Tite 335AF is a coating which bonds corrugated to Surlyn or polyethylene skin pack films, firmly trapping the product in between. Adhes..
|
|||
| Specific Gravity |
0.980
-
0.990
g/cc <br>@Temperature 25.0 °C
|
0.980
-
0.990
g/cc <br>@Temperature 77.0 °F
|
|
|
Dow Corning SE 1896 FR KIT
Two-part, translucent, heat cure.Information provided by Dow Corning
|
|||
| Specific Gravity | 0.970 - 0.990 g/cc | 0.970 - 0.990 g/cc | ASTM D792 |
|
Buckeye Polymers BP RPP 1009 GK Polypropylene, 10% Glass Filled
Product Information: 10% chemically coupled glass reinforced polypropyleneProduct Features:Offers improved flex modulus while maintaining a low specific gravity propertyOffers improved heat stabilit..
|
|||
| Specific Gravity | 0.970 - 0.990 g/cc | 0.970 - 0.990 g/cc | ASTM D792 |
|
Buckeye Polymers BP RPP 1209 GR BLK Polypropylene, 12% Glass Filled
Product Information: 12% glass reinforced polypropyleneProduct Features:Offers improved flex modulus while maintaining a low specific gravity propertyOffers improved heat stability and scratch and m..
|
|||