| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.00 g/cc | 1.00 g/cc | 23/23°C; ASTM D792 |
|
RheTech Products GC15P200-00 15% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: Electrical housingsUnderhood componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Specific Gravity | 1.00 g/cc | 1.00 g/cc | 23/23°C; ASTM D792 |
|
RheTech Products HP514-393 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 110D Medium Dark Pewter
Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Specific Gravity | 1.00 g/cc | 1.00 g/cc | 23/23°C; ASTM D792 |
|
RheTech Products HP514-394 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 102E Medium Oak
Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Specific Gravity | 1.00 g/cc | 1.00 g/cc | 23/23°C; ASTM D792 |
|
RheTech Products HP522-00 15% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural
Applications: ConsolesClose out panelInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Specific Gravity | >= 1.00 g/cc | >= 1.00 g/cc | |
|
Parker Chomerics CHO-BOND 586 Conductive Epoxy
Information provided by Chomerics
|
|||
| Specific Gravity | >= 1.00 g/cc | >= 1.00 g/cc | |
|
Parker Chomerics CHO-FORM 5525, Part B Silicone
Information provided by Chomerics
|
|||
| Specific Gravity | <= 1.00 g/cc | <= 1.00 g/cc | |
|
Parker Chomerics CHO-SHIELD® 576 Part B Coating Catalyst
Information provided by Chomerics
|
|||
| Specific Gravity | 1.00 g/cc | 1.00 g/cc | ISO 1183 |
|
GEHR Plastics PP-30PET-F Polypropylene, 30% PET Fiber Reinforced
(discontinued **)
Polypropylene shows a high mechanical strength and a tensile strength, but a low notched impact strength. PP resists stress cracking and it is easy to weld. At minus temperatures it can get brittle...
|
|||
| Specific Gravity | 1.00 - 1.02 g/cc | 1.00 - 1.02 g/cc | |
|
Michelman® DigiPrime® 5100 Primer
Description: Primer for digital printingUsage: DigiPrime® 5100 is a print primer which provides excellent adhesion of HP Indigo electro inks to treated films and paper. It adheres well to many sy..
|
|||
| Specific Gravity | 1.00 - 1.15 g/cc | 1.00 - 1.15 g/cc | |
|
Michelman® Hydrosize® U2022 Nonionic polyurethane emulsion
Description: Nonionic polyurethane emulsionUsage: Hydrosize® U2022 is an APE free, high strength sizing for glass and carbon chopped fiber, with excellent adhesion.Information provided by Michelm..
|
|||
| Specific Gravity | 1.00 g/cc | 1.00 g/cc | ASTM D792 |
|
LG Chemical LUPOL HF5157 PP+Rubber+MF, High Flow and Stiffness, High Impact
Description: Injection Molding, PP+Rubber+MF, High Flow and Stiffness, High Impact, Good Weatherability, Scratch ResistanceApplication: Automotive Exterior (Slim wall Bumper Fascia)Information provi..
|
|||
| Specific Gravity | 1.00 g/cc | 1.00 g/cc | True |
|
Shin-Etsu Silicones KSP-100 Fluid
Information Provided by Shin-Etsu Silicones of America, Inc.
|
|||
| Specific Gravity | 1.00 g/cc | 1.00 g/cc | |
|
Struktol TPW 709 Processing Additive
A unique proprietary blend of non-metal internal/external processing aids.Applications: STRUKTOL® TPW 709 has shown excellent results in producing extruded polymer/wood composites with or without..
|
|||
| Specific Gravity | 1.00 g/cc | 1.00 g/cc | ASTM D792 |
|
Teknor Apex Monprene® MP-2990 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Specific Gravity | 1.00 g/cc | 1.00 g/cc | ASTM D792 |
|
A. Schulman POLYFORT™ FPP 2067HU UV Stabilized, High Heat Resistant Impact Polypropylene
DescriptionPolyfort® FPP 2067HU is a unique high flow, UV stabilized high heat resistant impact polypropylene available in matched automotive colors. It molds to a fine appearance with good scrat..
|
|||
| Specific Gravity | 1.00 g/cc | 1.00 g/cc | |
|
Zeon Chemicals Nipol® 1041 Nitrile Elastomer
Nipol® nitrile elastomers are recommended when oil or solvent resistance is needed for the proper functioning of rubber parts. Fuel, oil and solvent resistance improves as acrylonitrile content is ..
|
|||
| Specific Gravity | 1.00 g/cc | 1.00 g/cc | ASTM D792 |
|
A. Schulman POLYBATCH™ Red 5500 Concentrate Based In Polyethylene
DescriptionPOLYBATCH® 5500 is a red color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 5500 is heavy ..
|
|||
| Specific Gravity |
1.00
g/cc @Temperature 25.0 °C |
1.00
g/cc @Temperature 77.0 °F |
|
|
Dow Corning ANTIFOAM C EMULSION, FOOD GRADE
Dow Corning Antifoam C Emulsion is a 30 percent food-grade silicone emulsion. This antifoam is water dilutable and effective in a variety of systems.Information provided by Dow Corning
|
|||
| Specific Gravity |
1.00
g/cc @Temperature 25.0 °C |
1.00
g/cc @Temperature 77.0 °F |
|
|
Dow Corning DB-310 ANTIFOAM EMULSION
30 percent active silicone emulsion designed to control foam in aqueous systems over wide pH ranges.Information provided by Dow Corning
|
|||
| Specific Gravity | 1.00 g/cc | 1.00 g/cc | |
|
Dow Corning SYL-OFF® SL 7688 CROSSLINKER
Minimizes mist at speeds up to 1600 m/min, good anchorage to and stability with many paper substrates, suitable for lamination with a variety of adhesives.Information provided by Dow Corning
|
|||
| Specific Gravity | 1.00 g/cc | 1.00 g/cc | ISO 2781 |
|
ELASTO UK Dryflex® 8004-101 Flame Retardant TPE for Injection Molding, Black, Halogen Free
Dryflex® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Dryflex® compounds permit sophisticated component design and thu..
|
|||
| Specific Gravity |
1.00
g/cc @Temperature 25.0 °C |
1.00
g/cc @Temperature 77.0 °F |
|
|
Dow Corning 1510-US ANTIFOAM
Dow Corning Antifoam 1510-US was specifically formulated for food contact applications.Information provided by Dow Corning
|
|||
| Specific Gravity | 1.00 g/cc | 1.00 g/cc | Uncatalyzed, QM CAT PURPLE |
|
ACC QM128 QSI Quantum Silicones 28 Durometer Condensation Cured Moldmaking Material
QM 128 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and shelf-life stability. This material is an excellent choice f..
|
|||
| Specific Gravity | >= 1.00 g/cc | >= 1.00 g/cc | |
|
Blue River Coatings Acrylic 4000D Topcoat
BLUE RIVER COATINGS ACRYLIC 4000 TOPCOAT is a hard, flexible, economical coating designed for multiple substrates. BLUE RIVER COATINGS ACRYLIC 4000 TOPCOAT offers good application properties, low fo..
|
|||
| Specific Gravity | 1.00 - 1.10 g/cc | 1.00 - 1.10 g/cc | ASTM D792 |
|
Aaron Industries AAROPRENE® ATPR 1000 80A Elastomeric Compound
AAROPRENE® ATPR 1000 Series Elastomeric CompoundDurometer values may be specified. Color may be specified.
|
|||
| Specific Gravity | 1.00 g/cc | 1.00 g/cc | ASTM D1475 |
|
Asia Technology Pioneers CAN 102 Acrylic Hi-Compound Resin
Description: ACN 102 is hi-tech compounded Acrylic Resin. This hi-composite is produced by Nano-Technology and used widely in paint and Coating industryAdvantages:High abrasion and corrosion resista..
|
|||
| Specific Gravity | 1.00 - 1.10 g/cc | 1.00 - 1.10 g/cc | |
|
Michelman® Michem® Coat 1548 Water and grease resistant, gluable coating
Description: Water and grease resistant, gluable coatingUsage: Michem® Coat 1548 is a machine ready coating which imparts good water, grease and oil resistance to the substrate. This product has be..
|
|||
| Specific Gravity | 1.00 g/cc | 1.00 g/cc | |
|
Elisto THERMOSTAR® MD 100 Pattern material
Densified laminated woodInformation provided by elisto
|
|||