| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 0.990 - 1.01 g/cc | 0.990 - 1.01 g/cc | |
|
Michelman® Catalyst P1 Catalyst portion of a two-part silicone release coating
Description: Catalyst portion of a two-part silicone release coatingUsage: Catalyst P1 is one part of a two part silicone release coating. This coating system provides release for virgin-rubber, asp..
|
|||
| Specific Gravity | 0.990 - 1.01 g/cc | 0.990 - 1.01 g/cc | |
|
Michelman® DigiPrime® 4431 Primer
Description: Primer for digital printingUsage: DigiPrime® 4431 is a patented flexo and gravure ready coating which provides excellent adhesion of HP Indigo ElectroInks® to a variety of films. ..
|
|||
| Specific Gravity | 0.990 - 1.01 g/cc | 0.990 - 1.01 g/cc | |
|
Michelman® Licomer® R 20 Ammonia solution of a rosin, modified with maleic acid
Description: Ammonia solution of a rosin, modified with maleic acidUsage: Licomer® R 20 is an additive for floor polish formulations.Information provided by Michelman®
|
|||
| Specific Gravity | 0.990 - 1.01 g/cc | 0.990 - 1.01 g/cc | |
|
Michelman® Licomer® W 485 Cationic montan emulsion
Description: Cationic montan emulsionUsage: Licomer® W 485 is a high gloss emulsion that improves the performance of floor crystalllizers.Information provided by Michelman®
|
|||
| Specific Gravity | 0.990 - 1.01 g/cc | 0.990 - 1.01 g/cc | |
|
Michelman® Michem® Emulsion 09625 Cationic ethylene acrylic acid emulsion
Description: Cationic ethylene acrylic acid emulsionUsage: Michem® Emulsion 09625 provides excellent chemical resistance. Michem® Emulsion 09625 has proven most useful in floor and other polis..
|
|||
| Specific Gravity | 0.990 - 1.01 g/cc | 0.990 - 1.01 g/cc | |
|
Michelman® Michem® Emulsion 13025 Slip and anti-block additive
Description: Slip and anti-block additiveUsage: Michem® Emulsion 13025 provides slip and block resistance in a wide variety of coatings and formulas. It has a very broad global food contact compl..
|
|||
| Specific Gravity | 0.990 - 1.01 g/cc | 0.990 - 1.01 g/cc | |
|
Michelman® Michem® Emulsion 27720 Nonionic slip and anti-block additive
Description: Nonionic slip and anti-block additiveUsage: Michem® Emulsion 27720 is a nonionic, amide emulsion used for anti-blocking, slip and mar resistant properties.We serve many markets throu..
|
|||
| Specific Gravity | 0.990 - 1.01 g/cc | 0.990 - 1.01 g/cc | |
|
Michelman® Michem® Emulsion 37135 Nonionic polyethylene emulsion
Description: Nonionic polyethylene emulsionUsage: Michem® Emulsion 37135 provides mar and scratch resistance as well as some slip resistance when used as an additive in polishes and coatings.We s..
|
|||
| Specific Gravity | 0.990 - 1.01 g/cc | 0.990 - 1.01 g/cc | |
|
Michelman® Michem® Emulsion 39235 Nonionic high density polyethylene emulsion
Description: Nonionic high density polyethylene emulsionUsage: Michem® Emulsion 39235 is best used as an additive in water based coatings where improved slip, rub resistance, hardness and/or bloc..
|
|||
| Specific Gravity | 0.990 - 1.01 g/cc | 0.990 - 1.01 g/cc | |
|
Michelman® Michem® Emulsion 43040 Nonionic polypropylene emulsion
Description: Nonionic polypropylene emulsionUsage: Michem® Emulsion 43040 is effectively used as an additive in floor polish and overprint varnish formulations when a high degree of slip resistan..
|
|||
| Specific Gravity | 0.990 - 1.01 g/cc | 0.990 - 1.01 g/cc | |
|
Michelman® Michem® Emulsion 61335 Anionic polyethylene emulsion
Description: Anionic polyethylene emulsionUsage: Michem® Emulsion 61335 is an additive which provides excellent slip and mar resistance and anti-blocking properties. This product can be used as a..
|
|||
| Specific Gravity | 0.990 - 1.01 g/cc | 0.990 - 1.01 g/cc | |
|
Michelman® Michem® Emulsion 91240 Nonionic polyethylene emulsion
Description: Nonionic polyethylene emulsionUsage: Michem® Emulsion 91240 is an additive which provides excellent anti-blocking, slip properties and mar resistance. This product is also used as an..
|
|||
| Specific Gravity | 0.990 - 1.01 g/cc | 0.990 - 1.01 g/cc | |
|
Michelman® Michem® Emulsion 91240G Nonionic polyethylene emulsion
Description: Nonionic polyethylene emulsionUsage: Michem® Emulsion 91240G is an additive which provides excellent anti-blocking, slip properties and mar resistance. It is also used as an additive..
|
|||
| Specific Gravity | 0.980 - 1.01 g/cc | 0.980 - 1.01 g/cc | |
|
Michelman® Michem® Emulsion 91840 Nonionic HD polyethylene / paraffin wax emulsion
Description: Nonionic HD polyethylene / paraffin wax emulsionUsage: Michem® Emulsion 91840 is a wax emulsion that provides superior rub resistance and gloss when used as an additive in overprint ..
|
|||
| Specific Gravity | 0.990 - 1.01 g/cc | 0.990 - 1.01 g/cc | |
|
Michelman® Michem® Emulsion 93335 Nonionic polyethylene emulsion
Description: Nonionic polyethylene emulsionUsage: Michem® Emulsion 93235 is a phenol free additive best used in water based coatings where improved slip, rub resistance, hardness and/or block res..
|
|||
| Specific Gravity | 0.990 - 1.01 g/cc | 0.990 - 1.01 g/cc | |
|
Michelman® Michem® Emulsion 93935 Nonionic polyethylene emulsion
Description: Nonionic polyethylene emulsionUsage: Michem® Emulsion 93935 is a phenol and formaldehyde free wax emulsion used mainly in floor polish formulations where it imparts black heel resist..
|
|||
| Specific Gravity | 0.990 - 1.01 g/cc | 0.990 - 1.01 g/cc | |
|
Michelman® Michem® Emulsion 94340 Nonionic polypropylene emulsion
Description: Nonionic polypropylene emulsionUsage: Michem® Emulsion 94340 a phenol free additive, is best used in floor polish and overprint varnish formulations when a high degree of slip resist..
|
|||
| Specific Gravity | 0.990 - 1.01 g/cc | 0.990 - 1.01 g/cc | |
|
Michelman® Michem® Flex HS-100 Water based heat seal coating
Description: Water based heat seal coatingUsage: Michem® Flex HS-100 is a self-priming, low temperature, heat seal coating for plastic films for Flexible Packaging applications. Patent PendingApp..
|
|||
| Specific Gravity | 0.990 - 1.01 g/cc | 0.990 - 1.01 g/cc | |
|
Michelman® Michem® Flex P1831 Water based primer
Description: Water based primer for liquids and extrusion coated resins.Usage: Michem® Flex P1831 is a primer for metal and paper substrates to promote adhesion to extrusion coated resins resulti..
|
|||
| Specific Gravity | 0.990 - 1.01 g/cc | 0.990 - 1.01 g/cc | |
|
Michelman® Michem® Flex P2300 Water based primer for extrusion coating
Description: Water based primer for extrusion coating.Usage: Michem® Flex P2300 is a primer for film, metalized film and paper substrates to promote adhesion to extrusion coated resins resulting ..
|
|||
| Specific Gravity | 0.990 - 1.01 g/cc | 0.990 - 1.01 g/cc | |
|
Michelman® Michem® In-Line Primer 30 Primer
Description: Primer for Digital PrintingUsage: Michem® In-Line Primer 030 imparts a print-receptive surface to paper substrates to improve the ink transfer and adhesion of HP Indigo Electroinks. ..
|
|||
| Specific Gravity | 0.950 - 1.01 g/cc | 0.950 - 1.01 g/cc | |
|
Lord Adhesives Flocklok® P11 Adhesive
Flocklok® P11 is a moisture curing, flexible polyurethane adhesive used for automotive weatherstrip sealing profiles to flock. This adhesive will adhere polyester or polyamide flock to a variety ..
|
|||
| Specific Gravity | 0.980 - 1.01 g/cc | 0.980 - 1.01 g/cc | |
|
Michelman® Michem® Lube 156 Nonionic carnauba wax emulsion
Description: Nonionic carnauba wax emulsionUsage: Michem® Lube 156 can be used as an additive in polishes (specifically car polish), cosmetics, paints, coatings and graphic arts to increase scrat..
|
|||
| Specific Gravity | 0.990 - 1.01 g/cc | 0.990 - 1.01 g/cc | |
|
Michelman® Michem® Lube 160PF Anionic carnauba wax emulsion
Description: Anionic carnauba wax emulsionUsage: Michem® Lube 160PF is an APEO-free additive which imparts slip, abrasion resistance and anti-block properties, in a variety of coatings and varnis..
|
|||
| Specific Gravity | 0.990 - 1.01 g/cc | 0.990 - 1.01 g/cc | |
|
Michelman® Michem® Lube 193 Slip and anti-block additive
Description: Slip and anti-block additive for latex systemsCompatible with ingredients used in many industries, including: Automotive care products; Building materials; Can and coil coatings; Concre..
|
|||
| Specific Gravity | 0.990 - 1.01 g/cc | 0.990 - 1.01 g/cc | |
|
Michelman® Michem® Prime 5931 Modified ethylene acrylic acid dispersion
Description: Modified ethylene acrylic acid dispersionUsage: Michem®Prime 5931 is a modified ethylene acrylic acid dispersion which provides improved adhesion to polyolefin substrates. It also ex..
|
|||
| Specific Gravity | 0.990 - 1.01 g/cc | 0.990 - 1.01 g/cc | |
|
Michelman® VaporCoat® 1500
Description: Water, oil and moisture resistant product for paperUsage: VaporCoat® 1500 is a coating which provides excellent water, oil and grease resistance along with excellent MVTR properties...
|
|||
| Specific Gravity | 0.990 - 1.01 g/cc | 0.990 - 1.01 g/cc | |
|
Michelman® Michem® Emulsion 79535 Nonionic polyethylene / polypropylene blend
Description: Nonionic polyethylene / polypropylene blend Usage: Michem® Emulsion 79535 is a nonionic, polyethylene blend wax emulsion for floor polish formulations. It provides excellent mar and ..
|
|||
| Specific Gravity | 0.990 - 1.01 g/cc | 0.990 - 1.01 g/cc | |
|
Michelman® Michem® Lube 160 Anionic carnauba wax emulsion
Description: Anionic carnauba wax emulsionUsage: Michem® Lube 160 provides superior slip and mar resistance on a variety of substrates such as metal, wood, film and paper. Anti-block properties a..
|
|||
| Specific Gravity | 0.970 - 1.01 g/cc | 0.970 - 1.01 g/cc | ASTM D792 |
|
Buckeye Polymers BP RPP 1509 GK BLK Polypropylene, 15% Glass Filled
Product Information: 15% glass reinforced polypropyleneProduct Features:Offers improved flex modulus while maintaining a low specific gravity propertyChemically coupled for improvved physical proper..
|
|||