Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Gravity = 1.05 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
23/23°C; ASTM D792
RheTech Products FT4802-01UV Thermoplastic Polyolefin, UV Stabilized, Black
Applications: Bodyside moldings and claddingsFacia and bumper coversInjection molding conditions reported in table.Information provided by RheTech Products.
Specific Gravity 1.05 g/cc
1.05 g/cc
Liquid State
Palm Labs Adhesives Turbo Fuse Series 115 (20 Viscosity) Rapid Bonding Adhesive
Palm Lab's cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 115 advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performanc..
Specific Gravity 1.05 g/cc
1.05 g/cc
Liquid State
Palm Labs Adhesives TURBO FUSE SERIES 190 CLEAR FLEXIBLE (4000 Viscosity) Rapid Bonding Adhesive
Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 190 CLEAR FLEXIBLE advanced formula is designed to polymerize instantly by absorbing surface moisture. The produ..
Specific Gravity 1.05 g/cc
1.05 g/cc
Liquid State
Palm Labs Adhesives Turbo Fuse Series 280 (SEMI-GEL) Rapid Bonding Adhesive
Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE 280 SERIES SEMI-GEL advanced thixotropic formula is designed to polymerize instantly by absorbing surface moisture. The..
Specific Gravity 1.05 g/cc
1.05 g/cc
Resinlab® CYNERGY CA6005 Adhesive
Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety..
Specific Gravity 1.05 g/cc
1.05 g/cc
Resinlab® CYNERGY CA6007 Adhesive
Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety..
Specific Gravity 1.05 g/cc
1.05 g/cc
Resinlab® CYNERGY CA6008 Adhesive
Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety..
Specific Gravity 1.05 g/cc
1.05 g/cc
Resin Technology Group UV MX-2240 Multi-Functional Hybrid, UV-Curing, Micro-Electronic System
Mix ratio 2 to 1 by volume.UV-MX 2240 is a low-viscosity, water-white photo/ chemical cross-linking encapsulant/sealant designed for micro-electronic applications. This two-part, Hybrid UV-epoxy bas..
Specific Gravity 1.05 g/cc
1.05 g/cc
Resinlab® CYNERGY CA6304 Adhesive
Description: The CYNERGY 6300 SERIES products are for use in applications where a faster set time is desired or low moisture conditions exist. Provides good bonds to a wide variety of materials.Appl..
Specific Gravity 1.05 g/cc
1.05 g/cc
Momentive Performance Materials RTV109 One Component Acetoxy Adhesive Sealant, Aluminum
RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. ..
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
MRC Polymers SATRANâ„¢ 800R ABS Terpolymer, Reprocessed
black onlyInformation provided by MRC Polymers Inc.
Specific Gravity 1.05 g/cc

@Temperature 25.0 °C
1.05 g/cc

@Temperature 77.0 °F
Multibase Dow Corning® MB50-011 Siloxane Additive
DOW CORNING MB50-011 Masterbatch is a pelletized formulation containing 50% of an ultra-high molecular weight siloxane polymer dispersed in PA6 polymer. It is designed to be used as an additive in P..
Specific Gravity 1.05 g/cc

@Temperature 22.8 °C
1.05 g/cc

@Temperature 73.0 °F
ASTM D792
Spartech PP5420 Glass Fiber Reinforced Homopolymer
Provides the maximum strength and heat resistance among polypropylene compounds. Physical properties can approach those of more expensive engineering resins.Information provided by Spartech
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
Samsung Cheil Industries Infino® WP-1041G PC/ABS, Unreinforced Metal Plating Grade
Information provided by Samsung Cheil Industries.
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
Samsung Cheil Industries Starex® NH-0925U ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D 792
SABIC Innovative Plastics Noryl EM6100F PPE+PS
Automotive interiors. 240F HDT. High impact/good property retention after heat ageing. In blowmolding, better sandability of flash, overblow.This data was supplied by SABIC-IP for the Americas re..
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
SABIC Innovative Plastics NORYL EM6101 PPE+PS
Automotive interiors. Improved flow characteristics/overall processing economy. 250F DTUL. Good property retention/wide temperature range.
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
Teknor Apex Telcar® TL-1522G Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
A. Schulman POLYFORT™ FXP 1227U UV Stable Copolymer Polypropylene
DescriptionPolyfort® FXP 1227U is a 20% CAC03 filled UV stable copolymer polypropylene product. Information provided by A. Schulman.
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
A. Schulman POLYFORT™ FPP 1237 CaCO3 filled homopolymer polypropylene
DescriptionPolyfort® FPP 1237 is a 20% CAC03 filled homopolymer polypropylene product. Information provided by A. Schulman.
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
A. Schulman POLYFORT™ FPP 3454F Talc Filled Copolymer
DescriptionPolyfort® FPP 3454F is a 20% talc filled copolymer.Information provided by A. Schulman.
Specific Gravity 1.05 g/cc

@Temperature 25.0 °C
1.05 g/cc

@Temperature 77.0 °F
Dow Corning MOLYKOTE® 44 HIGH TEMPERATURE BEARING GREASE, LIGHT
Phenyl-methyl silicone grease for low to high temperaturesInformation provided by Dow Corning
Specific Gravity 1.05 g/cc

@Temperature 25.0 °C
1.05 g/cc

@Temperature 77.0 °F
Dow Corning SE 738 SILICONE RTV
One-part, white, moisture cure RTV, non-flowing, general purpose, UL 94 HB.Information provided by Dow Corning
Specific Gravity 1.05 g/cc
1.05 g/cc
ISO 2781
ELASTO UK Dryflex® 8006-101 Flame Retardant TPE for Injection Molding, Natural, Halogen Free
Dryflex® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Dryflex® compounds permit sophisticated component design and thu..
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
Diamond Polymers ABS 3501E Natural 1000 S
Description: Extrusion Grade, High ImpactInformation provided by Diamond Polymers, Inc.
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
Clariant Renol SB83642580 ASA Polymer
Data provided by Clariant Masterbatches
Specific Gravity 1.05 g/cc

@Temperature 25.0 °C
1.05 g/cc

@Temperature 77.0 °F
Dow Corning 1-6184 WATER REPELLENT
Dow Corning® 1-6184 Water Repellent is a low-VOC, multifunctional, self-crosslinking, water soluble siloxaneInformation provided by Dow Corning
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
Aaron Industries AVPS H 100-3 Virgin Polystyrene
Melt flow index may be specified.
Specific Gravity 1.05 g/cc
1.05 g/cc
Alcoa KAMA 3202 Freezer Modified High Impact Polystyrene  (discontinued **)
CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableColors availa..