| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.06 g/cc | 1.06 g/cc | 23/23°C; ASTM D792 |
|
RheTech Products FT5100-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: IP structural componentBody side moldingInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Specific Gravity | 1.06 g/cc | 1.06 g/cc | 23/23°C; ASTM D792 |
|
RheTech Products RCT220-01 20% Talc Reinforced Polypropylene Copolymer, Black, Recycled Content
Applications: Fan shroudsElectrical housingsHush panelsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Specific Gravity | 1.06 g/cc | 1.06 g/cc | 23/23°C; ASTM D792 |
|
RheTech Products T20P104-01 20% Talc Reinforced Polypropylene, Black
Applications: Electronic housingsIP componentsHVAC ducts - air distributionClose out panelDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Specific Gravity | 1.06 g/cc | 1.06 g/cc | 23/23°C; ASTM D792 |
|
RheTech Products G20P252-01 20% Glass Fiber Reinforced Polypropylene Copolymer, Black
Applications: Interior trimArm rest insertConsolesDome light housingInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Specific Gravity | 1.06 g/cc | 1.06 g/cc | |
|
LG Chemical EM500A Impact modifier for Engineering Plastics
Description: LG Chem impact modifiers for Engineering Plastic are developed to enhance the impact strength of Engineering Plastics (PC, PBT, ABS, PC/PBT, PC/ABS, etc). LG Chem has 2 type impact modi..
|
|||
| Specific Gravity |
1.06
-
1.10
g/cc <br>@Temperature 15.5 °C
|
1.06
-
1.10
g/cc <br>@Temperature 59.9 °F
|
|
|
Indium Corp. #66 Wave Solder Flux
Wave Solder Flux #66 is a completely organic, liquid flux containing non-evaporating vehicles and is suitable for tin and all conventional solder alloys. It incorporates a unique fluxing ingredient..
|
|||
| Specific Gravity | 1.06 g/cc | 1.06 g/cc | ASTM-D792 |
|
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (DAM)
Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce..
|
|||
| Specific Gravity | 1.06 g/cc | 1.06 g/cc | ASTM D 792 |
|
SABIC Innovative Plastics Noryl PX6021 PPE+PS (Asia Pacific)
Low heat, flame retardant PPO/HIPS alloy.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Specific Gravity | 1.06 g/cc | 1.06 g/cc | ASTM D792 |
|
SABIC Innovative Plastics NORYL WCA871A PPE (Europe-Africa-Middle East)
Flame retardant performance and mechanical properties capable of meeting UL VW-1 requirement and 105C temperature rating as defined UL1581. UL1581 tests conducted on 1.0mmD wire with AWG28 conductor..
|
|||
| Specific Gravity | 1.06 g/cc | 1.06 g/cc | ASTM D792 |
|
Samsung Cheil Industries Starex® NH-1926 HIPS, Unreinforced FR
Non-halogen flame-retardant HIPS with high-impact that can be used in the exterior of TV and VCR interior/exterior material of OA devicesInformation provided by Samsung Cheil Industries.
|
|||
| Specific Gravity | 1.06 g/cc | 1.06 g/cc | ASTM D 792 |
|
SABIC Innovative Plastics Noryl PX4058 PPE+PS (Asia Pacific)
PPO, polyolefin blend. Improved chemical resistance. 253F (125C) HDT.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Specific Gravity | 1.06 g/cc | 1.06 g/cc | ASTM D792 |
|
SABIC Innovative Plastics NORYL PX500 PPE (Asia Pacific)
Noryl PX500 is an unfilled modified polyphenylene ether resin capable of multiple conversion routes. This resin is designed for lower odor during conversion than many standard modified PPE resins. ..
|
|||
| Specific Gravity | 1.06 g/cc | 1.06 g/cc | ASTM D792 |
|
Samsung Cheil Industries Starex® WR-9310 ASA, Unreinforced Heat Resistant
Heat resistant ASA that is used in the interior/exterior material of automobileInformation provided by Samsung Cheil Industries.
|
|||
| Specific Gravity | 1.06 g/cc | 1.06 g/cc | ASTM D792 |
|
SABIC Innovative Plastics NORYL 731 PPE+PS
PPE+PS blend. Unfilled. NSF listed for potable water use in several colors (Standard 61). FDA compliant in several colors (restrictions apply). UL94 HB rated. Low water absorption. Hydrolytic stabi..
|
|||
| Specific Gravity | 1.06 g/cc | 1.06 g/cc | ASTM D792 |
|
SABIC Innovative Plastics NORYL EXNL0143 PPE+PS
Noryl PX1736 Resin is a blend of PPE and PS, that provides high strength, increased heat resistance, and translucency. The material has melt strenght suitable for Extrusion and Blow Molding applica..
|
|||
| Specific Gravity | 1.06 g/cc | 1.06 g/cc | ASTM D792 |
|
Chase Plastics CP Pryme® N100STL (DAM) Nylon 6, Super Toughened, Internally Lubricated
Information provided by Chase Plastics.
|
|||
| Specific Gravity | 1.06 g/cc | 1.06 g/cc | ASTM D792 |
|
A. Schulman POLYBATCH™ Mahogany 50381 Concentrate Based in Polyethylene
DescriptionPOLYBATCH® 50381 is a mahogany color concentrate based in linear low density polyethylene. This product was formulated to offer color in polyethylene film applications. POLYBATCH® 50..
|
|||
| Specific Gravity | 1.06 g/cc | 1.06 g/cc | ASTM D792 |
|
ELASTO UK Dryflex® 650800 TPE, Improved Compression Set and High Temperature Resistance, 80A Hardness
The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. This grade is designed with improved compressi..
|
|||
| Specific Gravity | 1.06 g/cc | 1.06 g/cc | Part A |
|
Epoxy Technology EPO-TEK® 301-2FL Low Stress, Optical Epoxy
Product Description: EPO-TEK® 301-2FL is a two component optical, medical, and semiconductor grade epoxy resin. It is a more flexible version of EPO-TEK® 301-2.Advantages & Application Notes: Sug..
|
|||
| Specific Gravity | 1.06 g/cc | 1.06 g/cc | ASTM D792 |
|
Diamond Polymers DIAMALOY WPE 2000 Wood Filled HDPE
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
|
|||
| Specific Gravity | 1.06 g/cc | 1.06 g/cc | 23°C; ASTM D792 |
|
Asahi Kasei Xyron® X05516 Modified Polyphenylene Ether
AutomotiveInformation provided by Asahi Kasei
|
|||
| Specific Gravity | 1.06 g/cc | 1.06 g/cc | ASTM D792 |
|
Asahi Kasei Thermofil P-20TC-1156 20% Talc Filled, Heat Stabilized
Information provided by Asahi Thermofil
|
|||
| Specific Gravity | 1.06 g/cc | 1.06 g/cc | 23/23°C; ASTM D792 |
|
RheTech Products GC20P255-01 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: BracketsUnderhood componentsElectrical housingsHeadlamp bracketsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Specific Gravity | 1.06 g/cc | 1.06 g/cc | ASTM D792 |
|
Diamond Polymers ABS 1100
Description: Injection Molding Grade, Extra High GlossInformation provided by Diamond Polymers, Inc.
|
|||
| Specific Gravity | 1.06 g/cc | 1.06 g/cc | ASTM D792 |
|
Diamond Polymers ABS 3500B
Description: Blow Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc.
|
|||
| Specific Gravity | 1.06 g/cc | 1.06 g/cc | Mixed; TM R050-16 |
|
Resinlab® EP1282 Black Unfilled Electronic Grade Epoxy Encapsulant
Resinlab™ EP1282 Black is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It is recognized under the Component Recognition Program of Underwriters Laborat..
|
|||
| Specific Gravity | 1.06 g/cc | 1.06 g/cc | Mixed; TM R050-16 |
|
Resinlab® EP1305LV Black Epoxy Casting Resin
Resinlab™ EP1305LV Black is a black two-part epoxy casting resin designed to give good adhesion to metals and especially PVC. It has good wetting to most surfaces and is free flowing to penetrate c..
|
|||
| Specific Gravity | 1.06 g/cc | 1.06 g/cc | 23/23°C; ASTM D792 |
|
RheTech Products M20P100-01A 20% Mica Reinforced Polypropylene, Black
Applications: Fan shroudsFiller panelsAir ductsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Specific Gravity | 1.06 g/cc | 1.06 g/cc | ASTM D792 |
|
SABIC Innovative Plastics PREVEX W20 PPE+PS
Automotive. PPE alloy. High flow/impact. Instrument panels and interior trim components. HDT 210F.
|
|||