Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Gravity = 1.08 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
Polymax® Maxelast® P2745 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
Polymax® Maxelast® P2750 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
Polymax® Maxelast® P3672 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D 792
SABIC Innovative Plastics Cycolac® GHT3330 ABS (Asia Pacific)
High heat grade of ABS used for interior automotive components.This data was supplied by SABIC-IP for the Asia Pacific region.
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
Network Polymers SAN 277 Blue Tint Color
Description: SAN - Styrene Acrylonitrile Transparent Engineering ThermoplasticInformation provided by Network Polymers Inc.
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D 792
NOVA Chemicals Dylark® FG7300 High-Heat Styrenic Copolymer
Product Description and Features: Styrene/maleic anhydride copolymer with high-heat resistance and high modulus. Resins designed for use in foam extrusion.Processing: Contact NOVA Chemicals techn..
Specific Gravity 1.08 g/cc
1.08 g/cc
Resinlab® TL5041 Anaerobic Threadlocking Compound
The TL5000 Series anaerobic threadlocking compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. They form a ..
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
SABIC Innovative Plastics Cycolac® INP581 ABS+SAN
High flow, low molecular weight SAN. Can be used as compounding additives for polymer blends. Can be blended with high rubber graft modifier resins to produce customized ABS properties. Suitable for..
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
LG Chemical TR-558 Transparent ABS, Humidity Resistance, Natural and Colored Pellets
LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron..
Specific Gravity 1.08 g/cc
1.08 g/cc
Momentive Performance Materials Siloprenâ„¢ Electro 242-2 Electrically Insulating Liquid Silicone Rubber
This LSR elastomer is an electrically insulating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate..
Specific Gravity 1.08 g/cc
1.08 g/cc
Momentive Performance Materials Siloprenâ„¢ LSR 2020 Liquid Silicone Rubber - General Purpose
This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera..
Specific Gravity 1.08 g/cc
1.08 g/cc
Momentive Performance Materials Siloprenâ„¢ LSR 2345/06 Electrically-Conductive Liquid Silicone Rubber
This LSR elastomer is an electrically conductive, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate..
Specific Gravity 1.08 g/cc
1.08 g/cc
Momentive Performance Materials Siloprenâ„¢ LSR 2620 Liquid Silicone Rubber - Fast Cure / High Tear
This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera..
Specific Gravity 1.08 g/cc
1.08 g/cc
Momentive Performance Materials TSE 221-3U Heat Cured Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
SABIC Innovative Plastics NORYL TPN9221 PPE+PS (Asia Pacific)
Transparent Noryl grade with 90dc and V-2 FR
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
SABIC Innovative Plastics NORYL GTX GTX974 PPE+PA
NORYL GTX974 is a material especially designed for in- or on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity for electro-static paintin..
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
SABIC Innovative Plastics NORYL HNA055 PPE+HIPS
>PPE+PS-HI< Autoclavable engineering thermoplastic. Biocompatible per ISO10993 (color dependent).
Specific Gravity 1.08 g/cc
1.08 g/cc
Shin-Etsu Silicones LIMSâ„¢ KE2004-5A/B Elastomer
Information Provided by Shin-Etsu Silicones of America, Inc.
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
Shinkong Synthetic Fibers Shinite® P301T20 PP, 20% Talc Filled
Information from Shinkong Synthetic Fibers Corp.
Specific Gravity 1.08 g/cc
1.08 g/cc
Teknor Apex Tekbond® TB 1415A Thermoplastic Elastomer
Notes: Tekbond® TPEs are a functional series of elastomer compounds designed to not only bond to the most difficult neat and reinforced engineering substrates with no primer or surface treatment, b..
Specific Gravity 1.08 g/cc
1.08 g/cc
ISO 1183/1
A. Schulman FORMION™ FI 231 5% Mineral Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 231 is an injection molding grade, 5% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. Ap..
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
A. Schulman POLYBATCH™ Green 3012E Concentrate Based In Polyethylene
DescriptionPOLYBATCH® 3012E is a green color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 3012E is he..
Specific Gravity 1.08 g/cc
1.08 g/cc
Zeon Chemicals Zetpol® PBZ-123 Hydrogenated Nitrile Elastomomer
PBZ-123 is a polyblend of hydrogenated nitrile polymer, Zetpol 1020, and polyvinyl chloride, Nippon Zeon 101EP. This material is mechanically fluxed to create a unique polyblend which exhibits good..
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
Diamond Polymers ASA 91802
Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc.
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
Clariant Renol PA133GN-109 Nylon 66, High Impact, Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
Specific Gravity 1.08 g/cc
1.08 g/cc
Abatron Primkote G A/B Waterborne Epoxy Primer/Sealer for Green Concrete
Primkote G is a waterborne epoxy system for priming and sealing floors. It contains a gray resin compound (Part A) and a clear hardener (Part B). It conditions concrete and other substrates for epox..
Specific Gravity 1.08 g/cc
1.08 g/cc
23°C; ASTM D792
Asahi Kasei Xyron® 340Z Modified Polyphenylene Ether
Flame RetardantInformation provided by Asahi Kasei
Specific Gravity 1.08 g/cc
1.08 g/cc
23°C; ASTM D792
Asahi Kasei Xyron® 500V Modified Polyphenylene Ether
Flame RetardantInformation provided by Asahi Kasei
Specific Gravity 1.08 g/cc
1.08 g/cc
Resinlab® TL5090 Anaerobic Threadlocking Compound
The TL5000 Series anaerobic threadlocking compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. They form a ..