Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Gravity = 1.10 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Specific Gravity 1.04 - 1.10 g/cc
1.04 - 1.10 g/cc
ASTM D792
S&E Specialty Polymers TufPrene™ EXC-11-016 405 Black SEBS
Information provided by S&E Specialty Polymers
Specific Gravity 1.05 - 1.10 g/cc
1.05 - 1.10 g/cc
PolyChem Alloy AquaGard™ 4504P
AquaGard products are designed to improve the flame retardency of polyolefins without the use of halogen additives, such as bromine or chlorine. AquaGard products are available in a polyethylene ..
Specific Gravity 1.06 - 1.10 g/cc
1.06 - 1.10 g/cc
LG Chemical CP-ST
Advantage: Super slump retention; Low concrete viscosity; Good combination with water reducer (WRM, WB, RS)Main Uses: Super slump retentionInformation provided by LG Chemical
Specific Gravity 1.06 - 1.10 g/cc

@Temperature 15.5 °C
1.06 - 1.10 g/cc

@Temperature 59.9 °F
Indium Corp. #66 Wave Solder Flux
Wave Solder Flux #66 is a completely organic, liquid flux containing non-evaporating vehicles and is suitable for tin and all conventional solder alloys. It incorporates a unique fluxing ingredient..
Specific Gravity 1.00 - 1.10 g/cc
1.00 - 1.10 g/cc
Michelman® Michem® Coat 95 Water and grease resistant, heat sealable coating
Description: Water and grease resistant, heat sealable coatingUsage: Michem® Coat 95 is a good multi-purpose coating that provides excellent water, oil and grease resistance. This product is heat..
Specific Gravity 1.00 - 1.10 g/cc
1.00 - 1.10 g/cc
Michelman® U-Nyte™ Set 201 Solid epoxy powder
Description: Solid epoxy powderUsage: U-Nyteâ„¢ Set 201 is designed to be a glass mat or preform binder with high adhesive properties and excellent thermal stability.Information provided by Miche..
Specific Gravity 1.00 - 1.10 g/cc
1.00 - 1.10 g/cc
ASTM D792
Loxim 820 01 HB Polypropylene Compound, Flame Retardant
Information provided by Loxim Industries
Specific Gravity 1.00 - 1.10 g/cc
1.00 - 1.10 g/cc
ASTM D792
Loxim 820 01 HBCC Polypropylene Compound, 20% Chemically Coupled, Flame Retardant
Information provided by Loxim Industries
Specific Gravity 1.00 - 1.10 g/cc
1.00 - 1.10 g/cc
ASTM D792
Loxim 820 02C HB Polypropylene Compound, 20% Calcite Filled, Flame Retardant
Information provided by Loxim Industries
Specific Gravity 1.00 - 1.10 g/cc
1.00 - 1.10 g/cc
ASTM D792
Loxim 820 02T HB Polypropylene Compound, 20% Talc Filled, Flame Retardant
Information provided by Loxim Industries
Specific Gravity 1.00 - 1.10 g/cc
1.00 - 1.10 g/cc
ASTM D792
Loxim 820 12 HB Polypropylene Compound, Flame Retardant
Information provided by Loxim Industries
Specific Gravity 1.00 - 1.10 g/cc
1.00 - 1.10 g/cc
ASTM D792
Loxim 821 02T HB Polypropylene Compound, 20% Talc Filled, Flame Retardant
Information provided by Loxim Industries
Specific Gravity 1.00 - 1.10 g/cc
1.00 - 1.10 g/cc
ASTM D792
Aaron Industries AAROPRENE® ATPR 1000 50A Elastomeric Compound
AAROPRENE® ATPR 1000 Series Elastomeric CompoundDurometer values may be specified. Color may be specified.
Specific Gravity 1.00 - 1.10 g/cc
1.00 - 1.10 g/cc
ASTM D792
Aaron Industries AAROPRENE® ATPR 1000 80A Elastomeric Compound
AAROPRENE® ATPR 1000 Series Elastomeric CompoundDurometer values may be specified. Color may be specified.
Specific Gravity 1.00 - 1.10 g/cc
1.00 - 1.10 g/cc
ASTM D792
Aaron Industries AAROPRENE® ATPR 1000 60A Elastomeric Compound
AAROPRENE® ATPR 1000 Series Elastomeric CompoundDurometer values may be specified. Color may be specified.
Specific Gravity 1.00 - 1.10 g/cc
1.00 - 1.10 g/cc
ASTM D792
Aaron Industries AAROPRENE® ATPR 1000 70A Elastomeric Compound
AAROPRENE® ATPR 1000 Series Elastomeric CompoundDurometer values may be specified. Color may be specified.
Specific Gravity 1.00 - 1.10 g/cc
1.00 - 1.10 g/cc
Michelman® Michem® Coat 1548 Water and grease resistant, gluable coating
Description: Water and grease resistant, gluable coatingUsage: Michem® Coat 1548 is a machine ready coating which imparts good water, grease and oil resistance to the substrate. This product has be..
Copyright © lookpolymers.com All Rights Reserved