| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | ASTM D792 |
|
PolyOne Maxxam™ DC-818.G001-8000 Polypropylene, Unspecified (PP, Unspecified)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
|
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | ASTM D792 |
|
PolyOne Maxxam™ MD 4245-59770 Polypropylene Copolymer (PP Copolymer)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
|
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | ASTM D792 |
|
Nylene® NX4528 Unfilled Nylon 6,6/6
Description: Nylene® NX 4528 is an unfilled specialty nylon. 4528 is FDA/NSF approved. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Pol..
|
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | ISO 1183 |
|
Lehmann & Voss LUVOCOM® 3-7281/PL/HI/BK Polyamide 6, with PTFE, toughness-modified
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce..
|
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | |
|
Momentive Performance Materials Siloprenâ„¢ LIM 6061 Liquid Silicone Rubber - Fast Cure / High Tear
This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera..
|
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | |
|
Momentive Performance Materials Siloprenâ„¢ LSR 2040 Liquid Silicone Rubber - General Purpose
This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera..
|
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | |
|
Momentive Performance Materials Siloprenâ„¢ LSR 3285/50 Liquid Silicone Rubber - Self-Lubricating / Standard
This LSR elastomer is a self-lubricating, standard, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at eleva..
|
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | |
|
Momentive Performance Materials Siloprenâ„¢ LSR 4640 Liquid Silicone Rubber - Healthcare
LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding ..
|
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | ASTM D 792 |
|
SABIC Innovative Plastics Noryl PX5622 PPE+PS
PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. Good flow and surface aesthetics. UL94 V0/5VA/5VB. RTI Elec/Imp/Str 65. Suitable for E/E market indoor/outdoor applications.This da..
|
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | ASTM D792 |
|
SABIC Innovative Plastics NORYL RN0401 PPE+PS (Asia Pacific)
RN0401 is an unfilled Post Consumer Recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 20% PCR styrenic series resin content. Available in black only.
|
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | ASTM D792 |
|
SABIC Innovative Plastics LNP LUBRILOY RF203H PA 66
LNP LUBRILOY* RF203H is a compound based on Nylon 66 resin containing 15% Glass Fiber, Proprietary Lubricant. Added features of this material include: Wear Resistant, Healthcare.
|
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | ASTM D792 |
|
Samsung Cheil Industries Starex® VG-4910 ABS, Glass Filled FR
Information provided by Samsung Cheil Industries.
|
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | 23°C; ASTM D792 |
|
Teknor Apex Flexalloy® 9100-55 Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, General Purpose, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather..
|
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | ASTM D792 |
|
A. Schulman POLYBATCH™ Blue LL40434 Concentrate Based In LLDPE
DescriptionPOLYBATCH® LL40434 is a blue concentrate based in LLDPE. This concentrate was designed to provide opacity and color in blow molding applications. POLYBATCH® LL40434 is heavy metal fre..
|
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | ASTM D792 |
|
A. Schulman POLYFORT™ FPP 1606 Glass Filled Chemically Coupled Impact Copolymer Polypropylene
DescriptionPolyfort® FPP 1606 is a 30% glass filled chemically coupled impact copolymer polypropylene product. Information provided by A. Schulman.
|
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | ASTM D792 |
|
A. Schulman POLYFORT™ FPP 3452 Mineral Filled Copolymer Polypropylene
DescriptionPolyfort® FPP 3452 is a 30% mineral filled copolymer polypropylene.Information provided by A. Schulman.
|
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | Mixed |
|
Tra-Con Tra-Bond FDA2T Food and Drug Application Epoxy Adhesive
TRA-BOND FDA-2T is a thixotropic epoxy resin system specifically developed for medical device applications. It has been tested in accordance with USP biological reactivity tests, in vivo and receive..
|
|||
| Specific Gravity |
1.12
g/cc @Temperature 25.0 °C |
1.12
g/cc @Temperature 77.0 °F |
|
|
Dow Corning SILASTIC® T-2 RTV SILICONE TRANSLUCENT BASE & CURING AGENT
Translucent, high strength silicone mold making rubber suited for prototype design and production tooling. Silastic T-2 is recommended for use with rigid polyurethane and can be used with polyesters..
|
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | |
|
Esstech X-747-0000 Ethoxylated Bis Phenol A Dimethacrylate, C35H48O10
This form of EBPADMA has 6 units of ethoxylation. Increasing the ethoxylated chain length increases the mobility of the molecule and therefore it reactivity and degree of conversion. CAS # 41637-38-..
|
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | ASTM D471; ISO 2781 |
|
Advanced Polymer Alloys Alcryn® 2060 CL Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
|
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | Laminate; ISO 1183 |
|
Azdel Plus C327-B01 31% Chopped Fiber Mat / PP Resin Matrix
AZDEL® C327-B01 is a glass mat thermoplastic laminate based upon a random oriented chopped fiber mat contained within a polypropylene resin matrix. This composite material features high flow prope..
|
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | ASTM D471; ISO 2781 |
|
Advanced Polymer Alloys Alcryn® 2060 NC Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
|
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | Part B; TM R050-16 |
|
Resinlab® EP1026 Clear Epoxy Adhesive
Resinlab™ EP1026 Clear is a two part unfilled epoxy adhesive designed for high speed bonding of metals, ceramics, and most plastics. It cures to a tough semi-rigid material, and is free flowing in ..
|
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | 23/23°C; ASTM D792 |
|
RheTech Products GC30P104-00 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural
Applications: BracketsHead lamp housingsBattery trayInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Specific Gravity |
1.12
g/cc @Temperature 22.8 °C |
1.12
g/cc @Temperature 73.0 °F |
ASTM D792 |
|
Spartech EP6430 Filled and Reinforced Copolymer
Filled copolymers offer a higher level of impact performance than homopolymer materials, and higher stiffness than unfilled copolymers. Copolymer based materials retain much of their impact strength..
|
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | Part B; TM R050-16 |
|
Resinlab® EP1026 Black Epoxy Adhesive
Resinlab™ EP1026 Black is a two part unfilled epoxy adhesive designed for high speed bonding of metals, ceramics, and most plastics. It cures to a tough semi-rigid material, and is free flowing in ..
|
|||