| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | ASTM D792 |
|
PolyOne Maxxam™ FR WC-P85 NHFR RoHS Natural Polyolefin, Unspecified
Maxxam™ HFFR WC-P85 RoHS Natural is a halogen-free flame retardant polyolefin compound characterized by low smoke, low flame spread, excellent spring-back, no plate-out and high extrusion line spee..
|
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | ASTM D792 |
|
Polymax® Maxelast® A9860M TPE, ABS/PC Overmold
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform..
|
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | ASTM D792 |
|
SABIC Innovative Plastics Cycoloy® MC8200 PC+ABS (Asia Pacific) |
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | ET510A, Epoxy Resin |
|
Permabond ET510 Epoxy Resin
PERMABOND ET510 is a two-part, 1:1 mixable epoxy adhesive. ET510 is a semi-flexible toughened epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plas..
|
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | ASTM D792 |
|
Fiberfil® J-60/30/E/HF Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled, improved flow
Information provided by FIBERFIL Engineered Plastics
|
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | ASTM D792 |
|
Fiberfil® J-60/30/E8/M Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
|
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | |
|
Momentive Performance Materials Siloprenâ„¢ LSR 2742 Liquid Silicone Rubber - Self-Bonding
This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur..
|
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | |
|
Momentive Performance Materials Siloprenâ„¢ LSR 2750 Liquid Silicone Rubber - Self-Bonding
This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur..
|
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | |
|
Indium Corp. Indalloy® 84157 Flux #5-0A Clear Liquid Flux
Indalloy Flux #5-0A is a clear liquid flux formulated for the purpose of soldering moderately easy to difficult metallizations such as nickel, oxidized copper, Kovar and brass. This flux contains o..
|
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | |
|
Shin-Etsu Silicones LIMSâ„¢ KE2001-40A/B Elastomer
Information Provided by Shin-Etsu Silicones of America, Inc.
|
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | 23°C; ASTM D792 |
|
Teknor Apex Flexalloy® 9900-55 Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Oil Resistant, Ultra High MWUses- Footwear, Tubing, Gaskets, Tools (Power/Others), Hose, Wire and ..
|
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | ASTM D792 |
|
Supreme Petrochem SP 553 Flame Retardant Polystyrene
Characteristics High flow properties Good balance of toughness and rigidity Available in any color Processing MoldingApplications Large size T.V. Cabinets VCR cabinets Electrical boxes, electric..
|
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | ASTM D792 |
|
Teknor Apex Sinpolene CPP1030 Polypropylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Calcium Carbonate Filler, 30% Filler by Weight Features: Homopolymer Uses: Appliance Components; Furniture; Housings F..
|
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | ASTM D792 |
|
A. Schulman POLYBATCH™ Blue LL40434 Concentrate Based In LLDPE
DescriptionPOLYBATCH® LL40434 is a blue concentrate based in LLDPE. This concentrate was designed to provide opacity and color in blow molding applications. POLYBATCH® LL40434 is heavy metal fre..
|
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | ASTM D792 |
|
A. Schulman POLYFORT™ FPP 3452 Mineral Filled Copolymer Polypropylene
DescriptionPolyfort® FPP 3452 is a 30% mineral filled copolymer polypropylene.Information provided by A. Schulman.
|
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | Mixed |
|
Tra-Con Tra-Bond FDA2 Food and Drug Application Epoxy Adhesive
TRA-BOND FDA-2 is a medium viscosity epoxy resin system specifically developed for medical device applications. It has been tested in accordance with USP biological reactivity tests, in vivo and rec..
|
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | Mixed |
|
Tra-Con Tra-Bond FDA8T Food and Drug Application Thixotropic Flexible Epoxy Adhesive
TRA-BOND FDA-8T EPOXY ADHESIVE is a thixotropic epoxy resin system specifically developed for bonding applications in accordance with Title 21, U.S. Code of Federal Regulations, Food and Drug Admini..
|
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | ASTM D792 |
|
Lubrizol ESTANE® 58887 Ether Based Thermoplastic Polyurethane
Features: Excellent hydrolysis resistance, low temperature performance, clarity and wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and blow molding; cab..
|
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | ASTM D792 |
|
A. Schulman POLYFLAM™ E-14526-31 30% Glass Reinforced Chemically Coupled Polypropylene
DescriptionPolyfort® E-14526-31 is a 30% glass reinforced chemically coupled polypropylene black. Information provided by A. Schulman.
|
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | ASTM D792 |
|
A. Schulman POLYBATCH™ Blue LL40299U/3 Concentrate Based In LLDPE
DescriptionPOLYBATCH® LL40299U/3 is a blue color concentrate based in LLDPE. This concentrate was designed to provide opacity, color and UV stability in blow molding applications. POLYBATCH® LL4..
|
|||
| Specific Gravity |
1.12
g/cc @Temperature 25.0 °C |
1.12
g/cc @Temperature 77.0 °F |
|
|
Dow Corning SILASTIC® P-1 RTV SILICONE RUBBER & CLEAR CURING AGENT
High strength silicone rubber suited for prototyping, production tooling, artistic and renovation applications. Silastic P-1 is recommended for use with polyesters, cement and rigid polyurethanes; a..
|
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | ASTM D792 |
|
Cheng Yu Plastic C1100 PC/ABS |
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | |
|
Momentive Performance Materials TUFEL™ III 92506 Biocompatible Extrusion Heat Cured Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
|
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | |
|
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR N650 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
|
|||
| Specific Gravity |
1.12
g/cc @Temperature 22.8 °C |
1.12
g/cc @Temperature 73.0 °F |
ASTM D792 |
|
Spartech EP6430 Filled and Reinforced Copolymer
Filled copolymers offer a higher level of impact performance than homopolymer materials, and higher stiffness than unfilled copolymers. Copolymer based materials retain much of their impact strength..
|
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | |
|
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR N774 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
|
|||
| Specific Gravity | 1.12 g/cc | 1.12 g/cc | Part B; TM R050-16 |
|
Resinlab® EP1026 Black Epoxy Adhesive
Resinlab™ EP1026 Black is a two part unfilled epoxy adhesive designed for high speed bonding of metals, ceramics, and most plastics. It cures to a tough semi-rigid material, and is free flowing in ..
|
|||