| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.14 - 1.20 g/cc | 1.14 - 1.20 g/cc | ASTM D792 |
|
S&E Specialty Polymers GTPE-2203G1 PVC
Application: RoHS compliant, 105° C, flexible, oil resistant TPE jacketing material with extremely good low temperature properties.Information provided by S&E Specialty Polymers
|
|||
| Specific Gravity | 1.15 - 1.20 g/cc | 1.15 - 1.20 g/cc | |
|
Nanocyl EPOCYL™ NC E128-04 Master Batch Liquid Bisphenol-A Resin for Solvent Based Formulation Purposes
EPOCYL™ NC E128-04 is a Mater Batch based on liquid Bisphenol-A (Bis-A) epoxy resin containing high concentration of Carbon Nanotubes (CNT) produced by Nanocyl. It is specifically developed for so..
|
|||
| Specific Gravity | 1.15 - 1.20 g/cc | 1.15 - 1.20 g/cc | |
|
Nanocyl EPOCYL™ NC R128-02 Master Batch Liquid Bisphenol-A Resin for Hot-Melt Formulation Purposes: Dilution Factor 6
EPOCYL™ NC R128-02 is a Master Batch based on liquid Bisphenol-A (Bis-A) epoxy resin containing high concentration of Carbon Nanotubes (CNT) produced by Nanocyl, with a suggested dilution factor of..
|
|||
| Specific Gravity | 1.15 - 1.20 g/cc | 1.15 - 1.20 g/cc | |
|
Nanocyl EPOCYL™ NC R128-04 Master Batch Liquid Bisphenol-A Resin for Solvent Based Formulation Purposes: Dilution Factor 6
EPOCYL™ NC R128-04 is a Master Batch based on liquid Bisphenol-A (Bis-A) epoxy resin containing high concentration of Carbon Nanotubes (CNT) produced by Nanocyl, with a suggested dilution factor of..
|
|||
| Specific Gravity | 1.15 - 1.20 g/cc | 1.15 - 1.20 g/cc | |
|
Nanocyl EPOCYL™ NC R2HM-01 Formulated Epoxy-Carbon Nanotube Pre-preg Resin System
EPOCYL™ NC R2HM-01 is a formulated epoxy based resin system for hot melt pre-preg and pressure molding processes, modified with our own Carbon Nanotubes (CNT), specifically developed to enhance the..
|
|||
| Specific Gravity | 1.00 - 1.20 g/cc | 1.00 - 1.20 g/cc | |
|
PolyChem Alloy FilmStat 3K2
Antistat concentrate based on Lauramide in a LLDPE carrier. Available in pelletized form in 50 lb. Bags
|
|||
| Specific Gravity | 1.00 - 1.20 g/cc | 1.00 - 1.20 g/cc | |
|
PolyChem Alloy FlexGel 4092, 4092D TPE
A Zero Shore Hardness TPE, FlexGel is soft, flexible, and resilient, with excellent chemical and moisture resistance. The material can be decorated, printed, reground, and reprocessed without any si..
|
|||
| Specific Gravity | 1.00 - 1.20 g/cc | 1.00 - 1.20 g/cc | |
|
PolyChem Alloy FlexGel 5007HF TPE
A Zero Shore Hardness TPE, FlexGel is soft, flexible, and resilient, with excellent chemical and moisture resistance. The material can be decorated, printed, reground, and reprocessed without any si..
|
|||
| Specific Gravity | 1.00 - 1.20 g/cc | 1.00 - 1.20 g/cc | |
|
PolyChem Alloy FlexGel 8307 TPE
A Zero Shore Hardness TPE, FlexGel is soft, flexible, and resilient, with excellent chemical and moisture resistance. The material can be decorated, printed, reground, and reprocessed without any si..
|
|||
| Specific Gravity | 1.14 - 1.20 g/cc | 1.14 - 1.20 g/cc | ASTM D 792 |
|
Karina E TR 500D22/173 Honey PVC Compound
Honey PVC compound additivated with nitrile rubber, recommended for injection of general soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
|
|||
| Specific Gravity | 1.16 - 1.20 g/cc | 1.16 - 1.20 g/cc | ASTM D 792 |
|
Karina E TR-600D48/1 Black PVC Compound
PVC compound with nitrile rubber additiveInformation provided by Karina Indústria e Comércio de Plásticos Ltda.
|
|||
| Specific Gravity | 1.02 - 1.20 g/cc | 1.02 - 1.20 g/cc | |
|
LG Chemical IM810 Acrylic impact modifier
Description: LG AIM (Acrylic impact modifier) is a type of additives that improves weather-resistance, impact strength, and processability of thermoplastic resin including PVC, which is used for pro..
|
|||
| Specific Gravity | 1.16 - 1.20 g/cc | 1.16 - 1.20 g/cc | ASTM D792 |
|
LG Chemical LUPOY GP5100 PC/ABS+GF10%
Description: Injection Molding, PC/ABS+GF10%, General Purpose, GF ReinforcedApplication: Electrical Appliance Housing, Automotive I/PCAS: 103598-77-2, 9003-56-9 and 65997-17-3Information provided by..
|
|||
| Specific Gravity | 1.10 - 1.20 g/cc | 1.10 - 1.20 g/cc | ASTM D792 |
|
Loxim 840 02T HB Polypropylene Compound, 40% Talc Filled, Flame Retardant
Information provided by Loxim Industries
|
|||
| Specific Gravity | 1.10 - 1.20 g/cc | 1.10 - 1.20 g/cc | ASTM D792 |
|
Loxim 841 02T HB Polypropylene Compound, 40% Talc Filled, Flame Retardant
Information provided by Loxim Industries
|
|||
| Specific Gravity | 1.14 - 1.20 g/cc | 1.14 - 1.20 g/cc | ASTM D 792 |
|
Karina 350-02/249 Yellow PVC Compound
For footware.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
|
|||
| Specific Gravity | 1.14 - 1.20 g/cc | 1.14 - 1.20 g/cc | ASTM D 792 |
|
Karina 550D32/13-AT-IS Orange PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
|
|||
| Specific Gravity | 1.14 - 1.20 g/cc | 1.14 - 1.20 g/cc | ASTM D 792 |
|
Karina 550D42/10-AT-IS Red PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
|
|||
| Specific Gravity | 1.16 - 1.20 g/cc | 1.16 - 1.20 g/cc | ASTM D 792 |
|
Karina BT-0002/17 White PVC Compound
PVC compound with addition of nitrile rubber, recommended for injection of boots, soles, and butcher shop bootsInformation provided by Karina Indústria e Comércio de Plásticos Ltda.
|
|||
| Specific Gravity | 1.10 - 1.20 g/cc | 1.10 - 1.20 g/cc | IEC 1212-2 7.2 |
|
Hippe PF CP 21 Cellulose Paper Reinforced Phenolic Resin - Round, Rolled Tube
Used in mechanical and low-voltage electrical applications. Good electrical properties when exposed to normal relative humidity.Information provided by Hippe.
|
|||
| Specific Gravity | 1.10 - 1.20 g/cc | 1.10 - 1.20 g/cc | IEC 1212-2 7.2 |
|
Hippe PF CP 23 Cellulose Paper Reinforced Phenolic Resin - Round, Rolled Tube
Used in mechanical and low-voltage electrical applications. Good electrical properties when exposed to normal and high relative humidity.Information provided by Hippe.
|
|||
| Specific Gravity | 1.10 - 1.20 g/cc | 1.10 - 1.20 g/cc | IEC 1212-2 7.2 |
|
Hippe PF CP 24 Cellulose Paper Reinforced Phenolic Resin - Round, Rolled Tube
Used in electrical and mechanical applications. Very good electrical properties when exposed to high relative humidity. Much higher mechanical strength and insulation resistance than type PF CP 21..
|
|||
| Specific Gravity | 1.16 - 1.20 g/cc | 1.16 - 1.20 g/cc | ASTM D792 |
|
Compuestos Dominicanos Polycom CH-550055-01 PVC Compound
Compuestos Dominicanos SA produces a wide variety of PVC compounds for the injection molding of footwear products; everything from full injection, shoe soles, boots, and PVC compounds for oil resist..
|
|||
| Specific Gravity | 1.16 - 1.20 g/cc | 1.16 - 1.20 g/cc | ASTM D792 |
|
Compuestos Dominicanos Polycom ME-333660 PVC Compound
Applications: Seals for caps Appearance: Clear pelletsInformation provided by Compuestos Dominicanos
|
|||
| Specific Gravity | 1.16 - 1.20 g/cc | 1.16 - 1.20 g/cc | ASTM D-792 |
|
Axiall 59996J Moldings & Extrusions Flexible PVC
Injection and molding compound with excellent low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
|
|||
| Specific Gravity | 1.16 - 1.20 g/cc | 1.16 - 1.20 g/cc | ASTM D-792 |
|
Axiall 8610 Moldings & Extrusions Flexible PVC
A high quality, low gravity, clear extrusion and molding compound with excellent low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
|
|||
| Specific Gravity | 1.14 - 1.20 g/cc | 1.14 - 1.20 g/cc | ASTM D792 |
|
Buckeye Polymers BP FLEX D6509 CU BLK Thermoplastic Polyolefin
Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist..
|
|||
| Specific Gravity | 1.16 - 1.20 g/cc | 1.16 - 1.20 g/cc | ASTM D792 |
|
Buckeye Polymers BP FLEX A6810 BLK Thermoplastic Elastomer SEBS
Product Information: BP Flex Thermoplastic Elastomers are based on SEBS polymers (Styrene-ethylene/butylene-styrene) providing increased oxidation and weather resistance, higher service temperatures..
|
|||
| Specific Gravity | 1.02 - 1.20 g/cc | 1.02 - 1.20 g/cc | |
|
LG Chemical IM812 Acrylic impact modifier
Description: LG AIM (Acrylic impact modifier) is a type of additives that improves weather-resistance, impact strength, and processability of thermoplastic resin including PVC, which is used for pro..
|
|||
| Specific Gravity | 1.16 - 1.20 g/cc | 1.16 - 1.20 g/cc | ASTM D792 |
|
Compuestos Dominicanos Polycom CO-160355 PVC Compound
Compuestos Dominicanos SA produces a wide variety of PVC compounds for the injection molding of footwear products; everything from full injection, shoe soles, boots, and PVC compounds for oil resist..
|
|||