| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
|
PolyOne Maxxam™ MX5210-0040 RS Natural Polypropylene Homopolymer (PP Homopolymer)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
|
|||
| Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
|
SABIC Innovative Plastics Cycoloy® RCM6134 PC+ABS (Asia Pacific)
Cycoloy* RCM6134 resin is an injection moldable filled PC/ABS blend with non-brominated and non-chlorinated flame retardant. It contains 35% post consumer recycle content with a UL-94 V0 rating @ 1...
|
|||
| Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
|
Polymer Resources NY6-G13 Nylon 6, 13% Glass Reinforced
Nylon 6, 13% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste..
|
|||
| Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
|
Polymer Resources PC/TP-GP2-[color]-UV PC/Polyester Alloy, UV-stabilized
High Impact, Excellent Chemical Resistance, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa..
|
|||
| Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
|
Polymer Resources PC-GP3-TFE10 Polycarbonate, 10% PTFE, High Flow, Wear Resistant
Polycarbonate, General Purpose, High Flow, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa..
|
|||
| Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
|
SABIC Innovative Plastics Lexan® EXL4016H PC Copolymer (Asia Pacific)
6% GF reinforced opaque polycarbonate-siloxane copolymer with good impact strength, stiffness and hydrolytic stability.
|
|||
| Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
|
PolyOne Geon™ HTX Ultra LA426 Black 2880 Polyvinyl Chloride Alloy (PVC Alloy)
Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical properties measured on LA426 Black 2880.Information provided by PolyOne
|
|||
| Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
|
PolyOne Geon™ HC 2170G Polyvinyl Chloride, Flexible (PVC, Flexible)
Geon HC 2170G is a 70 Shore A non-phthalate, gamma-stable flexible vinyl compound made from FDA sanctioned ingredients. HC 2170G can be used for extrusion and injection molding healthcare applicatio..
|
|||
| Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
|
PolyOne Lubri-Tech™ AS-15CF/15T Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced, PTFE Lubricated
&nb
Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
|
|||
| Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
|
LG Chemical Lupox® TE5000H PBT+PC
Description: Injection Molding, PBT+PC, High Impact, Dimensional StabilityApplication: Automotive ItemCAS No. 9003-01-04, 24968-12-5 and 103598-77-2Information provided by LG Chemical
|
|||
| Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
|
Gromax CCP PBT 1100-220S
Product Description: PBT unreinforced and impact-modified injection molding grade. Characteristics:Low warp age, high toughness and excellent dimensional stabilityExcellent glossy surface and less-g..
|
|||
| Specific Gravity | 1.22 - 1.28 g/cc | 1.22 - 1.28 g/cc | ASTM D 792 |
|
Karina 603-48/1-Y-BZ Black PVC Compound
For footware.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
|
|||
| Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
|
SABIC Innovative Plastics LNP STAT-KON DX05301C PC (Asia Pacific)
Low Ionic, Low Outgassing, Low LPC and ESD safe Polycarbonate compound suitable for Semiconductor and Hard Disk Drive (HDD) application.Added features of this material include: Clean Compounding Sys..
|
|||
| Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
|
Spartech SP-9013 FR/ABS Flame Retardant Sheet
Description: Flame Retardant SheetInformation provided by Spartech.
|
|||
| Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D 792 |
|
SABIC Innovative Plastics Xenoy® 1731J PBT+PC (Asia Pacific)
PBT+PC, Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
|
SABIC Innovative Plastics Xenoy® X6800BM PBT (Asia Pacific)
Blow moldable, impact modifed XENOY
|
|||
| Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D 792 |
|
SABIC Innovative Plastics LNP Thermocomp C7410 PC+ABS (Asia Pacific)
LNP* Thermocomp* C7410 compound is a talc-filled PC+ABS, nonhalogenated FR for thinwall molding applications.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
|
SABIC Innovative Plastics LNP THERMOCOMP Cycoloy_C7210A PC+ABS
LNP* Thermocomp* Cycoloy_C7210A isa a talc-filled PC+ABS, nonhalogenated FR for thinwall molding applications. Very good modulus-ductility balance.
|
|||
| Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
|
A. Schulman POLYFORT™ FPP 3717 Talc Filled Homopolymer Polypropylene (39.6% Mineral Content)
DescriptionPolyfort® FPP 3717 is a 40% talc filled homopolymer polypropylene product. Information provided by A. Schulman.
|
|||
| Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
|
A. Schulman POLYFORT™ FPP 3460 Glass-Mineral Hybrid Filled Copolymer
DescriptionPolyfort® FPP 3460 is a 40% glass-mineral hybrid filled copolymer.Information provided by A. Schulman.
|
|||
| Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
|
A. Schulman POLYFORT™ FPP 3460 Glass-Mineral Hybrid Filled Copolymer
DescriptionPolyfort® FPP 3460 is a 40% glass-mineral hybrid filled copolymer.Information provided by A. Schulman.
|
|||
| Specific Gravity | 1.22 g/cc | 1.22 g/cc | DIN 53479 |
|
Lubrizol ESTANE® 58092 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
|
|||
| Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
|
Colorite Polymers Elastichem 7511TX-02 Vinyl Compound
Description: All components in Elastichem are sanctioned by the U.S. Food & Drug Administration for food packaging applications under Title 21 of the Code of Federal Regulations. For medical use, co..
|
|||
| Specific Gravity | 1.22 - 1.26 g/cc | 1.22 - 1.26 g/cc | ASTM D-792 |
|
Axiall 8823 Moldings & Extrusions Flexible PVC
A UL certified flame retardant, clear flexible PVC compound recommended for a maximum service temperature of 60°C. Exhibits good migration resistance properties. UL approved for 94 V-0 at 2.30 mm..
|
|||
| Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
|
Aaron Industries AAROPRENE® GFABS 4020 Glass Filled Acrylonitrile-Butadiene Styrene
AAROPRENE® GFABS 4000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified.
|
|||
| Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
|
Teknor Apex Sinpolene CPP1040 Polypropylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Calcium Carbonate Filler, 40% Filler by Weight Features: Homopolymer Uses: Appliance Components; Furniture; Housings F..
|
|||
| Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
|
A. Schulman POLYBLAK™ 3123 Premium Black Color Concentrate, 50% Carbon Black Based In LDPE
DescriptionPOLYBLAK® Black 3123 is a premium black color concentrate containing 50% carbon black in LDPE. This masterbatch is designed to provide good opacity and a regular blue undertone with pig..
|
|||