Polymer Property : Specific Gravity = 1.26 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
PolyOne Geon™ Vinyl Rigid Extrusion L4230 Polyvinyl Chloride, Rigid (PVC, Rigid)
Extrusion capstock for darker colors. This product is not recommended for horizontal, outdoor applications.Information provided by PolyOne
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
PolyOne Geon™ Vinyl Wire & Cable JLC31A Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
PolyOne Synprene™ RT-5180 RoHS Natural Styrene Butadiene Block Copolymer (SBC)
Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom..
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
SABIC Innovative Plastics Lexan® 505RU PC
Lexan* 505RU is a glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEEE/Ro..
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
SABIC Innovative Plastics Lexan® 505RU PC (Europe-Africa-Middle East)
Lexan* 505RU is a 10% glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEE..
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
PolyOne Geon™ HC 2180G Polyvinyl Chloride, Flexible (PVC, Flexible)
Geon HC 2180G is a 80 Shore A non-phthalate, gamma-stable flexible vinyl compound made from FDA sanctioned ingredients. HC 2180G can be used for extrusion and injection molding healthcare applicatio..
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
PolyOne Geon™ Vinyl Flexible A4D02 Polyvinyl Chloride, Flexible (PVC, Flexible)
A flexible transparent PVC Compound designed primarily for indoor mats.Information provided by PolyOne
Specific Gravity 1.26 g/cc

@Temperature 23.0 °C
1.26 g/cc

@Temperature 73.4 °F
ASTM D792
Kingfa JH710 G10 Flame Retardant & 10% Glass Reinforced PC
Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:CD-ROM, DVDPrinter, photocopier cabinetSc..
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
LG Chemical KEYFLEX BT 1072D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D 792
SABIC Innovative Plastics Ultem HATX200 PEI+PCE
High flow Polyetherimide blend. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compli..
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
Teknor Apex APEX® 3800-90 Polyvinyl Chloride, Flexible
Features: DEHP Plasticizer; Ethylene Oxide Sterilizable; High Heat Resistance Uses: Medical/Healthcare Applications Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor ..
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
SABIC Innovative Plastics NORYL GTX GTX8720 PPE+PA (Europe-Africa-Middle East)
Noryl GTX* GTX8720 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-..
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
Samsung Cheil Industries Infino® SI-3109GL PC, Glass Filled High Impact
Information provided by Samsung Cheil Industries.
Specific Gravity 1.26 g/cc
1.26 g/cc
Absolute Drying; ASTM-D792
Toyobo GLAMIDE® T-663G15 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
A. Schulman POLYFORT™ FPP 1842 Homopolymer Polypropylene
DescriptionPolyfort® FPP 1842 is a high stiffness, high heat resistant filled homopolymer polypropylene developed especially for instrument panel clusters. It is opaque to high intensity light.Inf..
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
A. Schulman SCHULAMID® 66 PTFE20 HS 20% PTFE Lubricated, Heat Stabilized Nylon 6/6
Information provided by A. Schulman.
Specific Gravity 1.26 g/cc
1.26 g/cc
ISO 1183/1
A. Schulman FORMION™ FI 225 30% Glass Fiber Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 225 is an injection molding grade, 30% glass fiber reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness..
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
A. Schulman COMTUF® 420 Impact Modified PBT
Information provided by A. Schulman.
Specific Gravity 1.26 g/cc
1.26 g/cc
ISO 1183/1
A. Schulman FORMION™ FI 225 30% Glass Fiber Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 225 is an injection molding grade, 30% glass fiber reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness..
Specific Gravity 1.26 g/cc
1.26 g/cc
ISO 2781
ELASTO UK Dryflex® 8013-101 Flame Retardant TPE for Injection Molding, Black
Dryflex® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Dryflex® compounds permit sophisticated component design and thu..
Specific Gravity 1.26 - 1.30 g/cc
1.26 - 1.30 g/cc
ASTM D-792
Axiall 8780 Moldings & Extrusions Flexible PVC
Low gravity, general purpose extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.26 g/cc
1.26 g/cc
BCC Products BC 9060 Silicone RTV Rubber
BC 9060 is a blue colored, two-component, flowable compound that, regardless of thickness or confinement, cures at room temperature or by application heat. The cured rubber is high strength and high..
Specific Gravity 1.26 g/cc
1.26 g/cc
Part A; TM R050-16
Resinlab® EP11HTFS Gray Filled Epoxy Adhesive
Resinlab™ EP11HTFS Gray is a two part filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-rigid material. It has good wetting to most surfa..
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
SABIC Innovative Plastics NORYL PX2922 PPE (Asia Pacific)
GF20% FR-V0
Specific Gravity 1.26 - 1.30 g/cc
1.26 - 1.30 g/cc
NBR NM-IEC 60811-1-3
Karina 02/223-G Yellow Color Concentrate for PVC
Color concentrate recommended for application in PVC compounds for general purposes injection. Recommended to use 2%.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
PolyOne Edgetek® AM-20CF/000 Polyphthalamide (PPA), Carbon Fiber Reinforced  (discontinued **)
Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
SABIC Innovative Plastics Lexan® HFD4471 PC (Asia Pacific)
Lexan* HFD4471 is a 10% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4417 has enhanced mold release, impact ductili..