Physical Properties Metric English Comments
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D792
PolyOne Geon™ Vinyl Wire & Cable WJCK504L Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide..
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D792
SABIC Innovative Plastics Lexan® HFD4211 PC
Lexan* HFD4211 is a 10% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release.
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D792
PolyOne Geon™ Vinyl Flexible 90201 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D792
PolyOne Geon™ Vinyl Flexible B7501 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D-792
PlastiComp Complet® LCF30 - PA6 Nylon 6, 30% Long Carbon Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 30% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D792
Ravago Manufacturing Americas Hylon® N1020HL BK Nylon 6/6  (discontinued **)
Available in North America Filler: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedForm: Pellets Processing Method: I..
Specific Gravity 1.27 - 1.33 g/cc
1.27 - 1.33 g/cc
ASTM D 792
Karina 651D10/1-C-IS White PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D 792
SABIC Innovative Plastics Ultem 1010A PEI (Asia Pacific)
Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region.
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D792
SABIC Innovative Plastics ULTEM 1010F PEI
Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contant compliant, NSF 51 listing. Effective June 2007, this grade will no longer b..
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D792
SABIC Innovative Plastics ULTEM 1010K PEI
Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming.
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D 792
SABIC Innovative Plastics Ultem 1010RF PEI
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. US FDA and EU Food Contact Compliant in recognized colors.This data was supplied by SABIC-IP for the Americas reg..
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D792
SABIC Innovative Plastics ULTEM HU1000 PEI
Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI)..
Specific Gravity 1.27 g/cc
1.27 g/cc
23°C; ASTM D792
Teknor Apex APEX® 90-A472R-95-NT Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Medical Applications, Caps, Closures, Valves/Valve Parts Appearance-ClearForms-PelletsProcessing Method-..
Specific Gravity 1.27 g/cc
1.27 g/cc
ISO 1183
Stir SpA Z 70 3 AT (PVC)
Application: Molding for beach footwearInformation provided by STIR SpA
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D792
Styron EMERGEâ„¢ 4701-13 Polycarbonate
EMERGEâ„¢ PC 4701-13 advanced resin is formulated with 10% glass fiber and a proprietary flame retardant package. It provides good ignition resistance, rigidity, dimension stability and heat res..
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP RC006H PA 66
LNP THERMOCOMP* RC006H is a compound based on Nylon 66 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Healthcare
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D792
A. Schulman POLYPUR™ FPU 1152C Thermoplastic Polyurethane
Information provided by A. Schulman.
Specific Gravity 1.27 g/cc

@Temperature 25.0 °C
1.27 g/cc

@Temperature 77.0 °F
Dow Corning LSPYW30 SILICONE MASTERBATCH YELLOW
Information provided by Dow Corning
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D792
Eastman Drystar 0827 Copolyester
This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen..
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D792
Eastman Eastar GN119 Copolyester
Applications:Personal care and CosmeticsProduct Description: Eastar GN119 Copolyester is a low-I.V. PETG, for sale only in Asia as a high-flow formulation. This product has been GREENGUARD INDOOR ..
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D1505
Eastman Spectar® 14471 Copolyester
Spectar copolyester extrudes into plastic sheet that is sparkling clear, tough, chemically resistant, odor-free, versatile, easy to work with and affordable. Its toughness allows fabricators to use ..
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D792
Colorite Polymers 1194B General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
Specific Gravity 1.27 g/cc
1.27 g/cc
Colorite Polymers 9011 Clear Extrusion Vinyl Compound
Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for the extrusion of various components for the production of devices. The vinyl components used in pre..
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D792
Colorite Polymers 9088 Non-Phthalate 88 Series Vinyl Compound
Description: The Colorite 88 series is a family of vinyl non-toxic compounds formulated to provide excellent low temperature flexibility characteristics. These compounds are designed for outside doo..
Specific Gravity 1.27 - 1.31 g/cc
1.27 - 1.31 g/cc
ASTM D-792
Axiall 10641 Wire & Cable Flexible PVC
Non-lead stabilized general purpose jacket compound designed for good flexibility and good low temperature performance.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2..