Polymer Property : Specific Gravity = 1.29 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Specific Gravity 1.29 g/cc
1.29 g/cc
ASTM D792
PolyOne Geon™ Vinyl Flexible 90451 Polyvinyl Chloride, Flexible (PVC, Flexible)
Automotive OEM approval(s).Information provided by PolyOne
Specific Gravity 1.29 g/cc
1.29 g/cc
ASTM D792
PolyOne Geon™ Vinyl Wire & Cable WY66L Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Specific Gravity 1.29 g/cc
1.29 g/cc
foam molded; ASTM D792
SABIC Innovative Plastics Lexan® FL933 PC
Various weight reductions at 0.250"" wall. 30% GR. Superior flexural strength and modulus; good tensile strength. UV-stabilized.
Specific Gravity 1.29 g/cc
1.29 g/cc
ASTM D792
PolyOne Edgetek® CY-20GF/000 UV FR V0 PC/ABS Blend, Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedIgnition ResistantNon-HalogenatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Specific Gravity 1.29 g/cc
1.29 g/cc
ASTM D792
PolyOne Edgetek® MLS-10GF/000 Polysulfone Alloy - 10% Glass Fiber Reinforced  (discontinued **)
Data provided by PolyOne.
Specific Gravity 1.29 g/cc
1.29 g/cc
ISO 1183
Lehmann & Voss LUVOCOM® 50/TF/15/GY04 Polycarbonate, with PTFE
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper..
Specific Gravity 1.29 g/cc
1.29 g/cc
Sylvin Technologies 9925-70 Natural PVC Molding Compound
Information provided by Sylvin Technologies Inc.
Specific Gravity 1.29 g/cc
1.29 g/cc
ASTM D792
SABIC Innovative Plastics ULTEM 8015 PEI (Asia Pacific)
High flow Polyetherimide blend. Meets FAR 25.853 and OSU 100/100 with low toxicity, smoke, and flame evolution. ECO Conforming.
Specific Gravity 1.29 g/cc
1.29 g/cc
ASTM D 792
SABIC Innovative Plastics LNP Stat-kon DEF13 PC
LNP* Stat-kon* DEF13 is a compound based on Polycarbonate resin containing Glass Fiber, Glass Fiber, Carbon Fiber. Added features of this material include: Electrically Conductive.This data was sup..
Specific Gravity 1.29 g/cc
1.29 g/cc
ASTM D 792
SABIC Innovative Plastics Valox® VAC3001 PBT (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
Specific Gravity 1.29 g/cc
1.29 g/cc
ASTM D 792
SABIC Innovative Plastics LNP Thermocomp ML4351HF PC (Asia Pacific)
LNP* Thermocomp* ML4351HF is a Light Reflecting Grade.This data was supplied by SABIC-IP for the Asia Pacific region.
Specific Gravity 1.29 g/cc
1.29 g/cc
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP RF004XXH PA 66
LNP THERMOCOMP* RF004XXH is a compound based on Nylon 66 resin containing 20% Glass Fiber. Added feature of this grade is: Healthcare.
Specific Gravity 1.29 g/cc
1.29 g/cc
Shin-Etsu Silicones KE-7022U Temperature Resistant Silicone Elastomer
KE7022 U is intended for applications where excellent high heat resistance is required.Product Features: This product is intended for high temperature service as 55 ~+ 300 °C(67 ~ +570 °F).Typ..
Specific Gravity 1.29 g/cc
1.29 g/cc
foam molded; ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP Noryl_FM4025 PPE+PS
LNP* Thermocomp* Noryl_FM4025 compound is GR/MR 40%, high modulus structural foam. 10% weight reduction, 0.250"" wall thickness.
Specific Gravity 1.29 g/cc
1.29 g/cc
ASTM D792
Teknor Apex APEX® 1004 Polyvinyl Chloride, Flexible
Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde..
Specific Gravity 1.29 g/cc
1.29 g/cc
23°C; ASTM D792
Teknor Apex Vidux® CV-1000-91 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-AntistaticForms-PelletsProcessing Method- ExtrusionInformation provided by Teknor Apex Company
Specific Gravity 1.29 g/cc
1.29 g/cc
ASTM D792
A. Schulman POLYPUR™ FPU 1376 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Specific Gravity 1.29 g/cc
1.29 g/cc
ASTM D792
A. Schulman POLYPUR™ FPU 1376 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Specific Gravity 1.29 g/cc
1.29 g/cc
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR Iceberg Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Specific Gravity 1.29 g/cc
1.29 g/cc
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR Suprex Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Specific Gravity 1.29 g/cc

@Temperature 25.0 °C
1.29 g/cc

@Temperature 77.0 °F
Dow Corning SILASTIC® M-3 RTV SILICONE RUBBER BASE & CURING AGENT
Dow Corning Silastic® M-3 RTV Silicone Rubber is an addition cured (platinum catalyzed); high durometer silicone rubber developed for use in prototyping, architectural, and furniture applications w..
Specific Gravity 1.29 g/cc
1.29 g/cc
Colorite Polymers 9611 Clear Extrusion Vinyl Compound
Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for the extrusion of various components for the production of devices. The vinyl components used in pre..
Specific Gravity 1.29 - 1.33 g/cc
1.29 - 1.33 g/cc
ASTM D-792
Axiall 1522 Wire & Cable Flexible PVC
Vinyl elastomer jacket compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.29 g/cc
1.29 g/cc
ASTM D 792
SABIC Innovative Plastics Noryl CRX2201 PPE+HIPS (Europe-Africa-Middle East)
Noryl* CRX2201 resin is a 25% mineral reinforced, injection moldable modified polyphenylene ether resin designed for improved chemical resistance when compared with standard Noryl resins. Noryl CRX..
Specific Gravity 1.29 g/cc
1.29 g/cc
ISO 1183
Lehmann & Voss LUVOCOM® 1-7497 Polyamide 66, with PTFE, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Specific Gravity 1.29 g/cc
1.29 g/cc
ASTM D792
Colorite Polymers 5790 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
Specific Gravity 1.29 g/cc
1.29 g/cc
ASTM D792
Adell HI-10 Impact Modified PBT
Specific Gravity 1.29 g/cc
1.29 g/cc
ASTM D792
PolyOne Syncure™ System S110FV-UV Polyethylene, Crosslinked (XLPE)
Syncure™ systems are two part moisture crosslinkable insulation compounds. S110FV-UV is a UL bulletinized, RoHS compliant, high strength, highly flame retardant insulation compound. Available in bl..