| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity |
1.30
-
1.32
g/cc <br>@Temperature 25.0 °C
|
1.30
-
1.32
g/cc <br>@Temperature 77.0 °F
|
|
|
Oceanchem Group Resorcinol bis (Diphenyl Phosphate) (RDP)
Molecular Formula: C30H24O8P2Cas No.: 57583-54-7RDP is a halogen-free phosphorus-based flame retardant.Use:RDP flame retardant provides a halogen-free solution for flame retarding PC/ABS, PPO/HIPS a..
|
|||
| Specific Gravity | 1.26 - 1.32 g/cc | 1.26 - 1.32 g/cc | ASTM D792 |
|
S&E Specialty Polymers GA-2285FR PVC
Application: 80°C clear flame retardant PVC compound.Information provided by S&E Specialty Polymers
|
|||
| Specific Gravity | 1.26 - 1.32 g/cc | 1.26 - 1.32 g/cc | ASTM D792 |
|
S&E Specialty Polymers GA-509OR PVC
Application: FR, UV and oil resistant PVC based compound with good low temperature properties.Information provided by S&E Specialty Polymers
|
|||
| Specific Gravity | 1.30 - 1.32 g/cc | 1.30 - 1.32 g/cc | ASTM D792 |
|
Gromax PBT 1100-211D
Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce..
|
|||
| Specific Gravity | 1.30 - 1.32 g/cc | 1.30 - 1.32 g/cc | ASTM D792 |
|
Gromax PBT 1100-211H
Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce..
|
|||
| Specific Gravity | 1.30 - 1.32 g/cc | 1.30 - 1.32 g/cc | ASTM D792 |
|
Gromax PBT 1100-211L
Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce..
|
|||
| Specific Gravity | 1.30 - 1.32 g/cc | 1.30 - 1.32 g/cc | ASTM D792 |
|
Gromax PBT 1100-211M
Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce..
|
|||
| Specific Gravity | 1.30 - 1.32 g/cc | 1.30 - 1.32 g/cc | ASTM D792 |
|
Gromax PBT 1100-211S
Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce..
|
|||
| Specific Gravity | 1.26 - 1.32 g/cc | 1.26 - 1.32 g/cc | ASTM D 792 |
|
Karina 40/418-FC-LMP Green Color Concentrate for PVC
Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. ..
|
|||
| Specific Gravity | 1.28 - 1.32 g/cc | 1.28 - 1.32 g/cc | ASTM D 792 |
|
Karina 501D48/1-D-IS Black PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
|
|||
| Specific Gravity | 1.28 - 1.32 g/cc | 1.28 - 1.32 g/cc | ASTM D 792 |
|
Karina 550-48/1-C-IS Black PVC Compound
Heavy metal free PVC compound recommended for technical parts extrusion and injection.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
|
|||
| Specific Gravity | 1.26 - 1.32 g/cc | 1.26 - 1.32 g/cc | ASTM D 792 |
|
Karina E 36/145-GE Brown Color Concentrate for PVC
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
|
|||
| Specific Gravity | 1.26 - 1.32 g/cc | 1.26 - 1.32 g/cc | ASTM D 792 |
|
Karina E 40/25-FC-LMP Green Color Concentrate for PVC
Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. ..
|
|||
| Specific Gravity | 1.26 - 1.32 g/cc | 1.26 - 1.32 g/cc | ASTM D 792 |
|
Karina E 701D02/128-SD Yellow PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
|
|||
| Specific Gravity | 1.30 - 1.32 g/cc | 1.30 - 1.32 g/cc | ASTM D792 |
|
Gromax PBT 1100-211XG
Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce..
|
|||
| Specific Gravity | 1.30 - 1.32 g/cc | 1.30 - 1.32 g/cc | ASTM D792 |
|
Gromax PBT 1200-211L
Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce..
|
|||
| Specific Gravity | 1.28 - 1.32 g/cc | 1.28 - 1.32 g/cc | NBR NM-IEC 60811-1-3 |
|
Karina 600D48/1-C-IS Black PVC Compound
PVC Compound recommended for injection of automotive parts and extrusion of flexible jacket for electrical cablesInformation provided by Karina Indústria e Comércio de Plásticos Ltda.
|
|||
| Specific Gravity | 1.26 - 1.32 g/cc | 1.26 - 1.32 g/cc | ASTM D 792 |
|
Karina E 880-10/136-A-IS-As White PVC Compound
Anti-UV and anti-fungus additivated PVC compound, recommended for general extrusion.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
|
|||
| Specific Gravity | 1.28 - 1.32 g/cc | 1.28 - 1.32 g/cc | ASTM D-792 |
|
Axiall 6741 Moldings & Extrusions Flexible PVC
A low gravity profile extrusion compound recommended for weatherstrips, extruded shapes, hoses and flexible gaskets. Provides good adhesion to rigid PVC in co-extruded products.Information provided..
|
|||
| Specific Gravity | 1.28 - 1.32 g/cc | 1.28 - 1.32 g/cc | ASTM D-792 |
|
Axiall 12812 Moldings & Extrusions Flexible PVC
General purpose, flame retardant extrusion compound formulated for good oil resistance. Also suitable for general purpose 80°C rated jacketing applications.Information provided by Georgia GulfGeor..
|
|||
| Specific Gravity | 1.28 - 1.32 g/cc | 1.28 - 1.32 g/cc | ASTM D-792 |
|
Axiall 14820 Wire & Cable Flexible PVC
Non-lead stabilized drop cable jacketing. Also suitable for 80C rated general purpose jacket applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
|
|||
| Specific Gravity | 1.28 - 1.32 g/cc | 1.28 - 1.32 g/cc | ASTM D-792 |
|
Axiall 8933 Moldings & Extrusions Flexible PVC
General purpose extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
|
|||
| Specific Gravity | 1.28 - 1.32 g/cc | 1.28 - 1.32 g/cc | ASTM D-792 |
|
Axiall 8940 Moldings & Extrusions Flexible PVC
General purpose semi-rigid extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
|
|||
| Specific Gravity | 1.30 - 1.32 g/cc | 1.30 - 1.32 g/cc | ASTM D792 |
|
Adamas Rixon U PEEK, Unreinforced
Information provided by Adamas, HPM
|
|||
| Specific Gravity | 1.28 - 1.32 g/cc | 1.28 - 1.32 g/cc | ASTM D-792 |
|
Axiall 38511 Wire & Cable Flexible PVC
Tray cable jacket with excellent low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
|
|||
| Specific Gravity | 1.28 - 1.32 g/cc | 1.28 - 1.32 g/cc | ASTM D-792 |
|
Axiall 4501 Flexible PVC
Non-lead stabilized, 105C rated automotive harness compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
|
|||
| Specific Gravity | 1.30 - 1.32 g/cc | 1.30 - 1.32 g/cc | ASTM D792 |
|
Gromax CCP PBT 1200-211E
Product Description: PBT unreinforced middle viscosity injection molding grade.Characteristics:Excellent electrical propertyExcellent temperature resistance, high heat distortion temperature.Excelle..
|
|||
| Specific Gravity | 1.30 - 1.32 g/cc | 1.30 - 1.32 g/cc | ASTM D792 |
|
Gromax PBT 1100-211MB
Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce..
|
|||
| Specific Gravity | 1.30 - 1.32 g/cc | 1.30 - 1.32 g/cc | ASTM D792 |
|
Gromax PBT 1200-211M
Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce..
|
|||
| Specific Gravity | 1.26 - 1.32 g/cc | 1.26 - 1.32 g/cc | ASTM D 792 |
|
Karina E 06/591-FC-LMP Blue Color Concentrate for PVC
Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. ..
|
|||