| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.28 - 1.34 g/cc | 1.28 - 1.34 g/cc | ASTM D 792 |
|
Karina E CAK 65 Ivory PVC Compound
Reclaimed PVC compound, recommended for injection of footwear soles. Color it is not guaranteed. CAK = alternative compound.Information provided by Karina Indústria e Comércio de Plástico..
|
|||
| Specific Gravity | 1.30 - 1.34 g/cc | 1.30 - 1.34 g/cc | ASTM D 792 |
|
Karina E CAK 75-48/1 Black PVC Compound
Reclaimed PVC compound recommended for injection of footwear soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
|
|||
| Specific Gravity | 1.28 - 1.34 g/cc | 1.28 - 1.34 g/cc | NBR NM-IEC 60811-1-3 |
|
Karina 40/67-FC-LMP (SDB) Green Color Concentrate for PVC
Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. ..
|
|||
| Specific Gravity | 1.28 - 1.34 g/cc | 1.28 - 1.34 g/cc | ASTM D 792 |
|
Karina 813-IS-SD Clear PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
|
|||
| Specific Gravity | 1.28 - 1.34 g/cc | 1.28 - 1.34 g/cc | ASTM D 792 |
|
Karina 842-IS-SD Crystal PVC Compound
PVC compound recommended for extrusion of sheet for vacuum forming (blister).Information provided by Karina Indústria e Comércio de Plásticos Ltda.
|
|||
| Specific Gravity | 1.28 - 1.34 g/cc | 1.28 - 1.34 g/cc | NBR NM-IEC 60811-1-3 |
|
Karina E 39/87-FC-LMP Pink Color Concentrate for PVC
Color concentrate recommended for application in PVC compounds for electrical wires and cables. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes.Important con..
|
|||
| Specific Gravity | 1.28 - 1.34 g/cc | 1.28 - 1.34 g/cc | NBR NM-IEC 60811-1-3 |
|
Karina E 42/268-FC-LMP Red Color Concentrate for PVC
Color concentrate recommended for application in PVC compounds for electrical wires and cables. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes.Important con..
|
|||
| Specific Gravity | 1.28 - 1.34 g/cc | 1.28 - 1.34 g/cc | ASTM D 792 |
|
Karina E 70/222-D-IS-SD Clear PVC Compound
PVC compound recommended for rolled mill of notebook covering.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
|
|||
| Specific Gravity | 1.28 - 1.34 g/cc | 1.28 - 1.34 g/cc | NBR NM-IEC 60811-1-3 |
|
Karina 39/87-FC-LMP (SDB) Pink Color Concentrate for PVC
Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. ..
|
|||
| Specific Gravity | 1.30 - 1.34 g/cc | 1.30 - 1.34 g/cc | ASTM D792 |
|
Compuestos Dominicanos Polycom BD-320699 PVC Compound
The polycom BD series are compounds for blow molding of PVC bottles suitable for the packaging of edible oil, water, cleaning products and lubricants. These compounds produce bottles with high clar..
|
|||
| Specific Gravity | 1.30 - 1.34 g/cc | 1.30 - 1.34 g/cc | ASTM D792 |
|
Compuestos Dominicanos Polycom BD-330699 PVC Compound
The polycom BD series are compounds for blow molding of PVC bottles suitable for the packaging of edible oil, water, cleaning products and lubricants. These compounds produce bottles with high clar..
|
|||
| Specific Gravity | 1.30 - 1.34 g/cc | 1.30 - 1.34 g/cc | ASTM D-792 |
|
Axiall 10751 Wire & Cable Flexible PVC
High quality jacket compound recommended for a maximum service temperature of 80°C.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
|
|||
| Specific Gravity | 1.30 - 1.34 g/cc | 1.30 - 1.34 g/cc | ASTM D-792 |
|
Axiall 12881 Wire & Cable Flexible PVC
Flame retardant, specialty grade, 75°C rated jacket compound. Designed to present a unique clear, sparkling appearance to the finished cable.Information provided by Georgia GulfGeorgia Gulf became..
|
|||
| Specific Gravity | 1.30 - 1.34 g/cc | 1.30 - 1.34 g/cc | ASTM D-792 |
|
Axiall 17890 Wire & Cable Flexible PVC
Non-lead stabilized insulation compound recommended for THW and 90C Class 43 applications. UL recognized component for THW and TW.Information provided by Georgia GulfGeorgia Gulf became Axiall Corp..
|
|||
| Specific Gravity | 1.30 - 1.34 g/cc | 1.30 - 1.34 g/cc | ASTM D-792 |
|
Axiall 18754 Wire & Cable Flexible PVC
Non-lead stabilized jacket compound with excellent low temperature performance. Maximum service temperature of 105°C at 40+ mil wall thickness.Information provided by Georgia GulfGeorgia Gulf beca..
|
|||
| Specific Gravity | 1.30 - 1.34 g/cc | 1.30 - 1.34 g/cc | ASTM D-792 |
|
Axiall 19900 Wire & Cable Flexible PVC
105°C; VW-1 rated non-lead stabilized insulation with good flexibility. Ideally suited for 1/64 wall (18 AWG and larger). UL approved for TW, THW, THHW applications.Information provided by Georgi..
|
|||
| Specific Gravity | 1.30 - 1.34 g/cc | 1.30 - 1.34 g/cc | ASTM D-792 |
|
Axiall 2134N Moldings & Extrusions Flexible PVC
105C plug molding compound. UL recognized component for 94 V-2 in all colors (0.75 mm min. thickness) and 94 V-0 in black and white (1.5 mm min. thickness). UL QMFZ2 recognized component.Informati..
|
|||
| Specific Gravity | 1.30 - 1.34 g/cc | 1.30 - 1.34 g/cc | ASTM D-792 |
|
Axiall 21540 Coax & Telecom Flexible PVC
Semi-rigid flame retardant insulation compound with good electrical properties for minimum transmission interference. Suitable for use in riser insulation.Information provided by Georgia GulfGeorgi..
|
|||
| Specific Gravity | 1.30 - 1.34 g/cc | 1.30 - 1.34 g/cc | ASTM D-792 |
|
Axiall 21540 Coax & Telecom Flexible PVC Black 307
Semi-rigid flame retardant insulation compound with good electrical properties for minimum transmission interference. Suitable for use in riser insulation. Max service temperature rating of 80°C ..
|
|||
| Specific Gravity | 1.30 - 1.34 g/cc | 1.30 - 1.34 g/cc | ASTM D-792 |
|
Axiall 36431 Coax & Telecom Flexible PVC
80°C rated, semi-rigid insulation compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
|
|||
| Specific Gravity | 1.30 - 1.34 g/cc | 1.30 - 1.34 g/cc | ASTM D-792 |
|
Axiall 10701 Wire & Cable Flexible PVC
General purpose 80°C compound with good low temperature properties recommended for 15 mil wall and larger.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
|
|||
| Specific Gravity | 1.30 - 1.34 g/cc | 1.30 - 1.34 g/cc | ASTM D-792 |
|
Axiall 10703 Wire & Cable Flexible PVC
Non-lead stabilized general purpose jacketing compound with good low temperature properties. Recommended for a maximum service temperature of 80°C at a 15 mil wall thickness.Information provided b..
|
|||
| Specific Gravity | 1.30 - 1.34 g/cc | 1.30 - 1.34 g/cc | ASTM D-792 |
|
Axiall 10706 Wire & Cable Flexible PVC
Non-lead stabilized 80C compound with good low temperature properties. Formulated for increased line speed and reduced surface gloss.Information provided by Georgia GulfGeorgia Gulf became Axiall C..
|
|||
| Specific Gravity | 1.30 - 1.34 g/cc | 1.30 - 1.34 g/cc | ASTM D-792 |
|
Axiall 12862 Wire & Cable Flexible PVC
Non-lead 80C liquid tight conduit compound according to UL360.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
|
|||
| Specific Gravity | 1.30 - 1.34 g/cc | 1.30 - 1.34 g/cc | ASTM D-792 |
|
Axiall 18750 Wire & Cable Flexible PVC
Jacketing compound with excellent low temperature performance. Maximum 105°C service temperature at 40+ mil thickness.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in ..
|
|||
| Specific Gravity | 1.30 - 1.34 g/cc | 1.30 - 1.34 g/cc | ASTM D-792 |
|
Axiall 18752 Wire & Cable Flexible PVC
Electrical grade extrusion compound with excellent low temperature performance. Maximum service temperature of 105°CInformation provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 20..
|
|||
| Specific Gravity | 1.32 - 1.34 g/cc | 1.32 - 1.34 g/cc | 23°C; ASTM D792 |
|
UBE UPIMOL® SA201 Heat-Resistant Polyimide Shape
Description: UPIMOL SA201 is an excellent heat-resistant polyimide shape, based on Biphenyl tetracarboxilic dianhydride(BPDA) originally developed by UBE. UPIMOL SA201 can save costs, and suit vario..
|
|||