| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.34 g/cc | 1.34 g/cc | ASTM D792 |
|
Ovation Polymers OpteSTAT™ NC PK 8010 Polyetheretherketone based Carbon Nanotube Compound
Material resistivity can be tailored to the application, while retaining the physical and thermal properties of the base polymer. Applications include components of disk drives, business machines or..
|
|||
| Specific Gravity | 1.34 g/cc | 1.34 g/cc | ASTM D792 |
|
PolyOne Edgetek® PC-20GF/000 Polycarbonate (PC)
Information provided by PolyOne
|
|||
| Specific Gravity | 1.34 g/cc | 1.34 g/cc | ASTM D792 |
|
PolyOne Geon™ Vinyl Wire & Cable WR3792CL Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
|
|||
| Specific Gravity | 1.34 g/cc | 1.34 g/cc | ASTM D792 |
|
PolyOne Geon™ Vinyl Flexible G92C Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
|
|||
| Specific Gravity | 1.34 g/cc | 1.34 g/cc | |
|
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR Suprex Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
|
|||
| Specific Gravity | 1.34 g/cc | 1.34 g/cc | Method A; ASTM D792 |
|
LNP Stat-Kon® EC-1004 Polyetherimide, Carbon Fiber Reinforcement
(discontinued **)
Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades..
|
|||
| Specific Gravity | 1.34 g/cc | 1.34 g/cc | ASTM D792 |
|
SABIC Innovative Plastics LNP LUBRICOMP BX02715 SAN
LNP* LUBRICOMP* BX02715 is a compound based on SAN containing proprietary fillers. Added features of this grade include: Wear Resistant, Tight Dimensional Tolerance, Good for Water Meter Applicati..
|
|||
| Specific Gravity | 1.34 g/cc | 1.34 g/cc | ISO 1183 |
|
GEHR Plastics POM-10PE Acetal Copolymer
Polyoxymethylene can be used in temperatures up to 100°C. The high surface strength is only surpassed by a few materials. POM shows good sliding properties and high resistance to wear and tear be..
|
|||
| Specific Gravity | 1.34 g/cc | 1.34 g/cc | ISO 1183 |
|
Lehmann & Voss LUVOCOM® 1105/GY7993 PEEK, unreinforced
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan..
|
|||
| Specific Gravity | 1.34 g/cc | 1.34 g/cc | ISO 1183 |
|
Lehmann & Voss LUVOCOM® 1105-0950/RD PEEK, unreinforced
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan..
|
|||
| Specific Gravity | 1.34 g/cc | 1.34 g/cc | ASTM D792 |
|
Kostat ICP-STAT ICD-1001 PET Sheet
KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas..
|
|||
| Specific Gravity | 1.34 g/cc | 1.34 g/cc | ASTM D792 |
|
SABIC Innovative Plastics Xenoy® X4870HH PC+PET (Europe-Africa-Middle East)
Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st..
|
|||
| Specific Gravity | 1.34 g/cc | 1.34 g/cc | 23°C; ASTM D792 |
|
Teknor Apex APEX® 3311-60 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To..
|
|||
| Specific Gravity | 1.34 g/cc | 1.34 g/cc | 23°C; ASTM D792 |
|
Teknor Apex APEX® 3311-75 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To..
|
|||
| Specific Gravity | 1.34 g/cc | 1.34 g/cc | ASTM D792 |
|
Teknor Apex APEX® 84863 Polyvinyl Chloride Compound
Notes: General Insulation Compound Uses: PVC Insulation; Semi Rigid Temperature Rating: 105°CInformation Provided by Teknor Apex
|
|||
| Specific Gravity | 1.34 g/cc | 1.34 g/cc | ASTM D792 |
|
A. Schulman POLYBATCH™ Opaque Blue 40356 Concentrate Based In LLDPE
DescriptionPOLYBATCH® 40356 is a blue color concentrate based in LLDPE. This concentrate was designed to provide color and opacity in blow molding applications. POLYBATCH® 40356/4 is typically ..
|
|||
| Specific Gravity | 1.34 g/cc | 1.34 g/cc | ASTM D792 |
|
Bayshore Vinyl Compounds BRC R7550 CLR 223V Extrusion Compound
R7550 CLR 223V is a general purpose medium/high impact profile extrusion compound developed for ease of process, sparkling clarity and gloss. It has been formulated for UV resistance for interior a..
|
|||
| Specific Gravity | 1.34 - 1.38 g/cc | 1.34 - 1.38 g/cc | ASTM D-792 |
|
Axiall 14840 Wire & Cable Flexible PVC
General purpose jacketing compound recommended for a maximum service temperature of 80°C.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
|
|||
| Specific Gravity | 1.34 - 1.38 g/cc | 1.34 - 1.38 g/cc | ASTM D-792 |
|
Axiall 19840 Wire & Cable Flexible PVC
105°C rated insulation suitable for 1/64 wall. Recommended for AWM applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
|
|||
| Specific Gravity | 1.34 g/cc | 1.34 g/cc | ASTM D792 |
|
Aaron Industries AAROPRENE® GFPC 5020 Glass Filled Polycarbonate
AAROPRENE® GFPC 5000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified.
|
|||
| Specific Gravity | 1.34 g/cc | 1.34 g/cc | ASTM D792 |
|
Techmer Lehvoss Compounds Luvotech™ J-4/30/V0 BK2989 PA6/12
(discontinued **)
Techmer Lehvoss Compounds, a JV between Techmer ES and Lehmann&Voss&Co. has been terminated.
|
|||
| Specific Gravity | 1.34 g/cc | 1.34 g/cc | ASTM D792 |
|
Techmer Lehvoss Compounds Luvotech™ J-4/30/V0 RD6922 PA6/12
(discontinued **)
Techmer Lehvoss Compounds, a JV between Techmer ES and Lehmann&Voss&Co. has been terminated.
|
|||
| Specific Gravity | 1.34 g/cc | 1.34 g/cc | ASTM D792 |
|
Techmer Lehvoss Compounds Luvotech™ J-4/35 NAT PA6/12
(discontinued **)
Techmer Lehvoss Compounds, a JV between Techmer ES and Lehmann&Voss&Co. has been terminated.
|
|||
| Specific Gravity | 1.34 g/cc | 1.34 g/cc | ASTM D792 |
|
Techmer Lehvoss Compounds Luvotech™ J-4/35/HS NAT PA6/12
(discontinued **)
Techmer Lehvoss Compounds, a JV between Techmer ES and Lehmann&Voss&Co. has been terminated.
|
|||
| Specific Gravity | 1.34 g/cc | 1.34 g/cc | ASTM D792 |
|
A. Schulman POLYBATCH™ Opaque Blue 40356 Concentrate Based In LLDPE
DescriptionPOLYBATCH® 40356 is a blue color concentrate based in LLDPE. This concentrate was designed to provide color and opacity in blow molding applications. POLYBATCH® 40356/4 is typically ..
|
|||
| Specific Gravity | 1.34 g/cc | 1.34 g/cc | ASTM D792 |
|
SABIC Innovative Plastics ULTEM 2110 PEI
10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing.
|
|||
| Specific Gravity | 1.34 g/cc | 1.34 g/cc | ASTM D792 |
|
LG Chemical LUPOL GP-2201F General Purpose Polypropylene, 20% Glass Fiber Reinforced, Flame Retardant
LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner..
|
|||