| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.30 - 1.36 g/cc | 1.30 - 1.36 g/cc | ASTM D792 |
|
S&E Specialty Polymers TufTech™ GA-1050-02LF PVC Compound
Application: A 105°C, AWM, 90°C AWM 1,000 volt, flame retardant compound.Information provided by S&E Specialty Polymers
|
|||
| Specific Gravity | 1.30 - 1.36 g/cc | 1.30 - 1.36 g/cc | |
|
Dow BETADAMP™ 32HT
(discontinued **)
BETADAMP™ 32HT is a high temperature vibration damper that can be applied to the exterior of cast aluminum or steel engine valve, transmission, and crankcase (oil pan) covers or electro-coat substr..
|
|||
| Specific Gravity | 1.32 - 1.36 g/cc | 1.32 - 1.36 g/cc | NBR NM-IEC 60811-1-3 |
|
Karina E MCP 520 Black PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
|
|||
| Specific Gravity | 1.32 - 1.36 g/cc | 1.32 - 1.36 g/cc | NBR NM-IEC 60811-1-3 |
|
Karina E810-40/312-IS-RG Green PVC Compound
Non toxic PVC compound, recommended for blow molding of bottles for alcoholic beverages.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
|
|||
| Specific Gravity | 1.30 - 1.36 g/cc | 1.30 - 1.36 g/cc | NBR NM-IEC 60811-1-3 |
|
Karina 36/234-FC-LMP (SDB) Brown Color Concentrate for PVC
Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. ..
|
|||
| Specific Gravity | 1.32 - 1.36 g/cc | 1.32 - 1.36 g/cc | ASTM D 792 |
|
Karina 651D28/29-D-IS ICE PVC Compound
Fungi resistant PVC compound, recommended for injection of bathroom carpet.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
|
|||
| Specific Gravity | 1.30 - 1.36 g/cc | 1.30 - 1.36 g/cc | ASTM D 792 |
|
Karina 851D48/1-A-IS-LMP Black PVC Compound
Heavy metal free PVC compound class 70C (ST1), recommended for electrical flexible cables jacketing. Also suitable for injection of plug.Information provided by Karina Indústria e Comércio de..
|
|||
| Specific Gravity | 1.32 - 1.36 g/cc | 1.32 - 1.36 g/cc | ASTM D 792 |
|
Karina 970-DA-48/1-B-IS Black PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
|
|||
| Specific Gravity | 1.30 - 1.36 g/cc | 1.30 - 1.36 g/cc | ASTM D 792 |
|
Karina E 18/35-FC-LMP Gray Color Concentrate for PVC
Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. ..
|
|||
| Specific Gravity | 1.30 - 1.36 g/cc | 1.30 - 1.36 g/cc | ASTM D 792 |
|
Karina E 74/240-D-IS-SD-TR Compound PVC Crystal
Films, laminated shrinkInformation provided by Karina Indústria e Comércio de Plásticos Ltda.
|
|||
| Specific Gravity | 1.30 - 1.36 g/cc | 1.30 - 1.36 g/cc | NBR NM-IEC 60811-1-3 |
|
Karina 750-DM-48/1-B-IS Black PVC Compound
PVC compound recommended for opaque jacketing of retractable telephone wiresInformation provided by Karina Indústria e Comércio de Plásticos Ltda.
|
|||
| Specific Gravity | 1.32 - 1.36 g/cc | 1.32 - 1.36 g/cc | ASTM D792 |
|
Compuestos Dominicanos Polycom VN-050485 PVC
Description: Compuestos Dominicanos manufactures the polycom VN products for the extrusion printable sheets and banners having good printing quality.Application: Sheet and bannersAppearance: Natural..
|
|||
| Specific Gravity | 1.32 - 1.36 g/cc | 1.32 - 1.36 g/cc | ASTM D-792 |
|
Axiall 8571 Moldings & Extrusions Flexible PVC
High quality, semi-rigid extrusion compound especially formulated for extruded T-moldings and other shapes where uniform flow through the die is required.Information provided by Georgia GulfGeorgia ..
|
|||
| Specific Gravity | 1.32 - 1.36 g/cc | 1.32 - 1.36 g/cc | ASTM D-792 |
|
Axiall 15642 Wire & Cable Flexible PVC
Non-lead stabilized semi-rigid insulation compound recommended for Style #1061 applications. Maximum service temperature of 105°C.Information provided by Georgia GulfGeorgia Gulf became Axiall Cor..
|
|||
| Specific Gravity | 1.32 - 1.36 g/cc | 1.32 - 1.36 g/cc | ASTM D-792 |
|
Axiall 16860 Wire & Cable Flexible PVC
Battery booster jacket compound and general purpose jacket.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
|
|||
| Specific Gravity | 1.32 - 1.36 g/cc | 1.32 - 1.36 g/cc | ASTM D-792 |
|
Axiall 17883 Wire & Cable Flexible PVC
UV resistant, 90C insulation compound with good low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
|
|||
| Specific Gravity | 1.32 - 1.36 g/cc | 1.32 - 1.36 g/cc | ASTM D-792 |
|
Axiall 19450 Wire & Cable Flexible PVC
105°C rated insulation compound with very good migration and oil resistance. Recommended for toner resistant applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation..
|
|||
| Specific Gravity | 1.32 - 1.36 g/cc | 1.32 - 1.36 g/cc | ASTM D-792 |
|
Axiall 2010 Wire & Cable Flexible PVC
General purpose insulation and jacketing compound recommended for 75°C applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
|
|||
| Specific Gravity | 1.32 - 1.36 g/cc | 1.32 - 1.36 g/cc | ASTM D-792 |
|
Axiall 312 Wire & Cable Flexible PVC
General purpose jacketing and insulation compound. UL recognized for 720 hour sunlight resistance in all colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
|
|||
| Specific Gravity | 1.32 - 1.36 g/cc | 1.32 - 1.36 g/cc | ASTM D-792 |
|
Axiall 38702 Moldings & Extrusions Flexible PVC
Flame retardant CATV and general purpose jacket with excellent low temperature properties. UL approved for 720 hour sunlight resistance in all colors. UL approved for 94 V-0 at 1.5 mm in all color..
|
|||
| Specific Gravity | 1.32 - 1.36 g/cc | 1.32 - 1.36 g/cc | ASTM D-792 |
|
Axiall 8552 Moldings & Extrusions Flexible PVC
A soft extrusion compound recommended for profiles, weatherstrips and sheeting. Also suitable for injection molding.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 201..
|
|||
| Specific Gravity | 1.32 - 1.36 g/cc | 1.32 - 1.36 g/cc | ASTM D-792 |
|
Axiall 18731 Wire & Cable Flexible PVC
Non-lead stabilized, UL recognized 720 hour sunlight resistant in all colors, 105 C rated jacket compound with good low temperature performance.Information provided by Georgia GulfGeorgia Gulf becam..
|
|||
| Specific Gravity | 1.32 - 1.36 g/cc | 1.32 - 1.36 g/cc | ASTM D-792 |
|
Axiall 19470 Wire & Cable Flexible PVC
Semi-rigid, 105°C insulation compound recommended for a minimum wall thickness of 10 mils. Designed to meet the performance criteria of military spec. MIL-W-16878D.Information provided by Georgia ..
|
|||
| Specific Gravity | 1.32 - 1.36 g/cc | 1.32 - 1.36 g/cc | ASTM D-792 |
|
Axiall 19481 Wire & Cable Flexible PVC
105°C, VW-1 rated non-lead stabilized insulation. Best suited for small gauge, 1/64 wall applications. UL approved for TW, THW, THHW, THHN-THWN insulation.Information provided by Georgia GulfGeor..
|
|||
| Specific Gravity | 1.32 - 1.36 g/cc | 1.32 - 1.36 g/cc | ASTM D-792 |
|
Axiall 19854 Wire & Cable Flexible PVC
Non-lead stabilized, 105°C rated insulation compound. Recognized by UL for TW and THW applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
|
|||
| Specific Gravity | 1.32 - 1.36 g/cc | 1.32 - 1.36 g/cc | ASTM D-792 |
|
Axiall 10702 Wire & Cable Flexible PVC
General purpose 80°C compound with good low temperature properties. Formulated for increased line speed and reduced surface gloss.Information provided by Georgia GulfGeorgia Gulf became Axiall Cor..
|
|||
| Specific Gravity | 1.32 - 1.36 g/cc | 1.32 - 1.36 g/cc | ASTM D-792 |
|
Axiall 19471 Wire & Cable Flexible PVC
Semi-rigid, 105°C insulation compound recommended for a minimum wall thickness of 10 mils. Designed to meet the performance criteria of military spec. MIL-W-16878D.Information provided by Georgia ..
|
|||
| Specific Gravity | 1.32 - 1.36 g/cc | 1.32 - 1.36 g/cc | ASTM D-792 |
|
Axiall 4441 Flexible PVC
85C non-lead stabilized wire harness. SAE J1128.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
|
|||
| Specific Gravity | 1.32 - 1.36 g/cc | 1.32 - 1.36 g/cc | ASTM D-792 |
|
Axiall 18840 Wire & Cable Flexible PVC
Non-lead stabilized 105C jacket compound for use in SPTO, SJTO and SVTO applications. Best suited for 30 mil walls and larger.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporat..
|
|||
| Specific Gravity | 1.32 - 1.36 g/cc | 1.32 - 1.36 g/cc | ASTM D-792 |
|
Axiall 8918 Moldings & Extrusions Flexible PVC
Non-lead migration resistant extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
|
|||