| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.42 g/cc | 1.42 g/cc | ASTM D792 |
|
Polymer Resources NY6/12-G43 Nylon 612, 43% Glass Reinforced
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
|
|||
| Specific Gravity | 1.42 g/cc | 1.42 g/cc | B |
|
Reltek BONDiT™ B-481TH Adhesive and Sealant
Key PropertiesHigh strength and toughness with excellent thermal stability to 400 deg F. Outstanding chemical resistance. Excellent electrical, and mechanical properties. Ease of use. ApplicationsBo..
|
|||
| Specific Gravity | 1.42 g/cc | 1.42 g/cc | ASTM D792 |
|
Gharda Chemicals GATONE™ 5630FC Polyetheretherketone (PEEK)
(discontinued **)
Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric..
|
|||
| Specific Gravity |
1.42
g/cc @Temperature 23.0 °C |
1.42
g/cc @Temperature 73.4 °F |
ISO 1183 |
|
Victrex® APTIV® 2102-100M Polyetheretherketone (PEEK) Polymer Film, Amorphous, Mineral Filled
APTIV® 2100 series films are the mineral filled amorphous films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance applications. APTIV ..
|
|||
| Specific Gravity | 1.42 g/cc | 1.42 g/cc | ASTM D792 |
|
PolyOne Lubri-Tech™ ATH-000/2T Acetal-Homopolymer, PTFE Lubricated
(discontinued **)
Description/Features:PTFE LubricatedInformation provided by PolyOne Corporation.
|
|||
| Specific Gravity | 1.42 g/cc | 1.42 g/cc | ASTM D792 |
|
PolyOne Geon™ Vinyl Fittings M1012 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
|
|||
| Specific Gravity | 1.42 g/cc | 1.42 g/cc | ASTM D792 |
|
PolyOne Geon™ Vinyl Fittings M1015 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
|
|||
| Specific Gravity | 1.42 g/cc | 1.42 g/cc | ASTM D792 |
|
Mitsui AURUM® JCN3030 Polyimide, Carbon Fiber Filled
(discontinued **)
AURUM JCN3030 is a high-performance polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, carbon fiber reinforced AU..
|
|||
| Specific Gravity | 1.42 g/cc | 1.42 g/cc | ISO 1183 |
|
Lehmann & Voss LUVOCOM® PEKK-7299 Polyether ketone, with carbon fiber, easy flowing
Applications: Automotive industry, mechanical- and precision engineering.Improved strength and stiffnes at elevated temperatures.Suitable for discharging of statically generated electricity.Thermic,..
|
|||
| Specific Gravity | 1.42 g/cc | 1.42 g/cc | |
|
Momentive Performance Materials Siloprenâ„¢ FFSL 7071 Fully Fluorinated Liquid Silicone Rubber
This LSR elastomer is a fully fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempe..
|
|||
| Specific Gravity | 1.42 g/cc | 1.42 g/cc | |
|
Momentive Performance Materials TSE 221-8U Heat Cured Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
|
|||
| Specific Gravity | 1.42 g/cc | 1.42 g/cc | ISO 1183 |
|
Lehmann & Voss LUVOCOM® 1105-8127-1 PEEK, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio..
|
|||
| Specific Gravity | 1.42 g/cc | 1.42 g/cc | |
|
Sylvin Technologies 9077-85 LMW Natural PVC for Injection Molding
Information provided by Sylvin Technologies Inc.
|
|||
| Specific Gravity | 1.42 g/cc | 1.42 g/cc | ASTM D792 |
|
SABIC Innovative Plastics ULTEM 2200 PEI (Asia Pacific)
20% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification in recognized colors.
|
|||
| Specific Gravity | 1.42 g/cc | 1.42 g/cc | ASTM D 792 |
|
SABIC Innovative Plastics Ultem CRS5211 PEI (Asia Pacific)
20% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming, UL94 V0 and 5VA listing.Thi..
|
|||
| Specific Gravity | 1.42 g/cc | 1.42 g/cc | ASTM D792 |
|
Teknor Apex APEX® 65004 Polyvinyl Chloride, Flexible
Notes: 75°C Jacket; RoHS Compliant Features: Flame Retardant; Sunlight Resistant (720 hours) Uses: Communication Wire JacketingForms: Pellets Agency Ratings: NEC Article 725; NEC Article 760; NEC..
|
|||
| Specific Gravity | 1.42 g/cc | 1.42 g/cc | ASTM D792 |
|
Teknor Apex APEX® RS 9011A Polyvinyl Chloride, Rigid
Forms: PelletsInformation Provided by Teknor Apex
|
|||
| Specific Gravity | 1.42 g/cc | 1.42 g/cc | ASTM D792 |
|
Samsung Cheil Industries Infino® LH-1070W PC, FR
Information provided by Samsung Cheil Industries.
|
|||
| Specific Gravity | 1.42 g/cc | 1.42 g/cc | ASTM D792 |
|
A. Schulman POLYBATCH™ Green 3251V Concentrate Based In Polyethylene
DescriptionPOLYBATCH® 3251V is a green color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 3251V conta..
|
|||
| Specific Gravity | 1.42 g/cc | 1.42 g/cc | ASTM D792 |
|
Teknor Apex Sinvicomp SRF 3707 Polyvinyl Chloride, Rigid
Availability: Asia Pacific Features: Good Impact Resistance Uses: Fittings Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex
|
|||
| Specific Gravity | 1.42 g/cc | 1.42 g/cc | ASTM D792 |
|
DuPont Performance Polymers VESPEL TP-8130 Polyimide
DuPont Vespel TP-8130 parts are specified for mechanical, thermal, and tribological properties. TP-8130 parts exhibits excellent strength and toughness, dimensional stability, low outgassing, radiat..
|
|||
| Specific Gravity | 1.42 g/cc | 1.42 g/cc | ASTM D792 |
|
E-Polymers TEKASTER® F101FR Un-Reinforced Flame Retardant PBT
Polyester Resin: TEKASTER is thermoplastic polyester resins (PBT, PET) mostly injection molding. PBT has excellent mechanical properties and well balanced engineering plastics with an electrical pe..
|
|||
| Specific Gravity | 1.42 g/cc | 1.42 g/cc | ASTM D792 |
|
Quadrant EPP Ketron® CM CA30 PEEK Polyetheretherketone, 30% carbon fiber reinforced, compression molded (ASTM Product Data Sheet)
Data provided by Quadrant Engineering Plastic Products Excellent chemical resistance Very low moisture absorption Inherently good wear and abrasion resistance Unaffected by continuous exposure to ho..
|
|||