| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.44 g/cc | 1.44 g/cc | ASTM D792 |
|
PolyOne Geon™ Vinyl Wire & Cable W1104L-xx60FRDUV Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide..
|
|||
| Specific Gravity | 1.44 - 1.50 g/cc | 1.44 - 1.50 g/cc | ASTM D792 |
|
S&E Specialty Polymers G-4785E PVC
Application: Flexible, PVC material designed for general-purpose extrusion applications.Information provided by S&E Specialty Polymers
|
|||
| Specific Gravity |
1.44
g/cc @Temperature 22.8 °C |
1.44
g/cc @Temperature 73.0 °F |
ASTM D792 |
|
Quadrant EPP Ketron® HPV PEEK High Pressure Velocity Polyetherether Ketone (ASTM Product Data Sheet)
This bearing grade of extruded Ketron PEEK offers the lowest coefficient of friction and best machinability of all Ketron grades. It is ideal for low wear, high PV parts that require chemical resis..
|
|||
| Specific Gravity | 1.44 g/cc | 1.44 g/cc | ASTM D792 |
|
Solvay Specialty Polymers Cogegum® AFR/960 Polyolefin, Unspecified
(Unverified Data**)
Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without ..
|
|||
| Specific Gravity | 1.44 g/cc | 1.44 g/cc | ISO 1183 |
|
Lehmann & Voss LUVOCOM® 1301/CF/15/TF/5 BK PPS, linear, with carbon fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
|
|||
| Specific Gravity | 1.44 - 1.46 g/cc | 1.44 - 1.46 g/cc | |
|
Michelman® HydroGrease White™ 22 White coating
Description: High performance water and grease resistant white coatingUsage: HydroGrease Whiteâ„¢ 22 is a white coating which imparts water and grease resistance to the substrate. This coating is..
|
|||
| Specific Gravity | 1.44 g/cc | 1.44 g/cc | ISO 1183 |
|
Lehmann & Voss LUVOCOM® 1105-7781/BK PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
|
|||
| Specific Gravity | 1.44 g/cc | 1.44 g/cc | ASTM D794 |
|
Saint-Gobain Meldin® 1357 Thermoplastic Bearing Material
Meldin 1357 offers the lowest wear rate and coefficient of friction, which makes it the best candidate for tribological applications. In addition, its self-lubricating properties allow it to operat..
|
|||
| Specific Gravity | 1.44 g/cc | 1.44 g/cc | ASTM D792 |
|
Teknor Apex HFFR 2002 Polyolefin, Halogen Free
Notes: RoHS Compliant Features: Flame Retardant; Halogen Free Uses: Communication Wire Jacketing; Electronic Cable Jacketing; Security Cable Jacketing Agency Ratings: ICEA Unspecified Rating; IEC Un..
|
|||
| Specific Gravity | 1.44 g/cc | 1.44 g/cc | ASTM D792 |
|
Teknor Apex Monprene® MP-2302 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Specific Gravity | 1.44 g/cc | 1.44 g/cc | ASTM D792 |
|
Teknor Apex Sinvicomp SRF 2703 Polyvinyl Chloride, Rigid
Availability: Asia Pacific Features: Good Weather Resistance; Good Impact Resistance Uses: Fittings Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex
|
|||
| Specific Gravity | 1.44 g/cc | 1.44 g/cc | ASTM D792 |
|
A. Schulman POLYPUR™ FPU 1156 Thermoplastic Polyurethane
Information provided by A. Schulman.
|
|||
| Specific Gravity | 1.44 g/cc | 1.44 g/cc | ASTM D792 |
|
A. Schulman POLYBATCH™ Light Grey LL803366/4 Concentrate Based In LLDPE
DescriptionPOLYBATCH® LL80366/4 is a light grey color concentrate based in LLDPE. This concentrate was designed to provide opacity and color in blow molding applications. POLYBATCH® LL80366/4 is..
|
|||
| Specific Gravity | 1.44 g/cc | 1.44 g/cc | ASTM D792 |
|
A. Schulman POLYBATCH™ Light Grey LL803366/4 Concentrate Based In LLDPE
DescriptionPOLYBATCH® LL80366/4 is a light grey color concentrate based in LLDPE. This concentrate was designed to provide opacity and color in blow molding applications. POLYBATCH® LL80366/4 is..
|
|||
| Specific Gravity | 1.44 g/cc | 1.44 g/cc | ASTM D792 |
|
Lubrizol ESTALOC® 59010 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane
Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas and AsiaInformation provided by Lubrizol
|
|||
| Specific Gravity | 1.44 g/cc | 1.44 g/cc | DIN 53479 |
|
Lubrizol ESTANE® 58563 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
|
|||
| Specific Gravity | 1.44 g/cc | 1.44 g/cc | ASTM D-792 |
|
Axiall PURGOVIN® 8000 Rigid PVC, Extrusion
Georgia Gulf PURGOVIN® 8000 is a unique vinyl based PVC pellet purging compound designed for use in the shutdown or cleaning of extrusion lines, blow molding machines, and injection molding machine..
|
|||
| Specific Gravity | 1.44 g/cc | 1.44 g/cc | silicone property; Arlon SQA-TMS-024 |
|
Arlon 56976XA026 Silicone Rubber/Fiberglass Laminate
Interleave: 3 mil PE; Side 1: cured silicone rubber; Substrate: 1564 fiberglass; Side 2: uncured silicone rubber
|
|||
| Specific Gravity | 1.44 g/cc | 1.44 g/cc | |
|
Aremco Quartz-Coat™ 845 High Temperature Ceramic-Inorganic Coating
Single part, waterborne, silicon-filled, phosphate-bonded, brown-black coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps..
|
|||
| Specific Gravity | 1.44 g/cc | 1.44 g/cc | ASTM D792 |
|
PolyOne Edgetek® ES-06CF-09GF/000 GREEN Polyethersulfone - 6% Carbon - 9% Glass Fiber Reinforced - ESD Applications
&am
Data provided by PolyOne.
|
|||
| Specific Gravity | 1.44 g/cc | 1.44 g/cc | ASTM D792 |
|
A. Schulman POLYPUR™ FPU 1156 Thermoplastic Polyurethane