| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.46 g/cc | 1.46 g/cc | ASTM D792 |
|
Nylene® 9543 , 43% Glass Reinforced Nylon 6/12
Description: Nylene® 9543 s a 43% glass fiber reinforced specialty nylon. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resour..
|
|||
| Specific Gravity | 1.46 g/cc | 1.46 g/cc | ASTM D792 |
|
PolyOne Geon™ Vinyl Flexible R7545H Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
|
|||
| Specific Gravity | 1.46 - 1.52 g/cc | 1.46 - 1.52 g/cc | ASTM D 792 |
|
Karina Karintox 70/2 Polyolefin Compound
Halogen free, fire retardant, low smoke and fume polyolefinic compound. Recommended for insulation of electrical cables up to 1KV.Information provided by Karina Indústria e Comércio de Plá..
|
|||
| Specific Gravity | 1.46 g/cc | 1.46 g/cc | ISO 1183 |
|
Lehmann & Voss LUVOCOM® 19-7221/OR Polyamide 46, with glass fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Highly dimensionally stable at elevated temperatures.Gear parts for automot..
|
|||
| Specific Gravity | 1.46 g/cc | 1.46 g/cc | ISO 1183 |
|
Lehmann & Voss LUVOCOM® 80-8511 Polyacetal-copolymer, with carbon fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage.High dimensionally..
|
|||
| Specific Gravity | 1.46 g/cc | 1.46 g/cc | ISO 1183 |
|
Lehmann & Voss LUVOCOM® TPI-0953 Thermoplastic polyimide, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile machinery, apparatus- and precision engineering medical- and electrical enineering, aircraft- and aerospace industry.Very high continuous use and heat dist..
|
|||
| Specific Gravity | 1.46 g/cc | 1.46 g/cc | ASTM D792 |
|
Greene Tweed Arlon® 1555 PEEK, Carbon, Graphite Filled
Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprie..
|
|||
| Specific Gravity | 1.46 g/cc | 1.46 g/cc | ISO 1183 |
|
Lanxess Durethan® BKV 40 H2.0 901510 Nylon 6, Glass Fiber Reinforced
PA 6, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS.
|
|||
| Specific Gravity | 1.46 g/cc | 1.46 g/cc | ISO 1183 |
|
Lehmann & Voss LUVOCOM® 1106-7227 Polyether imide, with carbon fiber and PTFE
Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.Hig..
|
|||
| Specific Gravity | 1.46 g/cc | 1.46 g/cc | ISO 1183 |
|
Lehmann & Voss LUVOCOM® 1100-8134 Polyether sulfone, with carbon fiber
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
|
|||
| Specific Gravity | 1.46 g/cc | 1.46 g/cc | ASTM D792 |
|
SABIC Innovative Plastics Valox® ENH8530 PBT+PET (Europe-Africa-Middle East)
Non-Brominated & Non-Chlorinated Flame Retardant, 15% Glass fiber reinforced PBT/PET blend
|
|||
| Specific Gravity | 1.46 g/cc | 1.46 g/cc | ASTM D792 |
|
Shinil Chemical SHINCON PPS-CF, Comp. "Y"-2 LCD Rack
LCD Rack is used to transfer or bake LCD frame in the electronic assembly or LCD packaging assembly line. Current LCD Rack is made of poly ether ether ketone (PEEK) with carbon fiber (CF). Since b..
|
|||
| Specific Gravity | 1.46 g/cc | 1.46 g/cc | |
|
Silberline 4-Allâ„¢ E 3064AR
The 4-Allâ„¢ series of passivated aluminum pigments is designed for use in waterborne automotive and industrial coatings. In the 4-Allâ„¢ system, the aluminum pigment is passivated using a pr..
|
|||
| Specific Gravity | 1.46 g/cc | 1.46 g/cc | |
|
Silberline Sparkle Silver® 5742
Sparkle Silver® 5742 is a fine, bright, regular purity, non-leafing aluminum pigment with good opacity for solvent-based general industrial coatings.Applications: Automotive
|
|||
| Specific Gravity | 1.46 g/cc | 1.46 g/cc | ASTM D792 |
|
SABIC Innovative Plastics LNP THERMOCOMP RFB53XXZ PA 66
LNP* THERMOCOMP* RFB53XXZ is a compound based on Nylon 66 resin containing 15% Glass Fiber, 25% Glass Bead.
|
|||
| Specific Gravity | 1.46 g/cc | 1.46 g/cc | ASTM D 792 |
|
SABIC Innovative Plastics LNP Thermocomp LF004 PEEK
LNP THERMOCOMP* LF004 is a compound based on Polyetheretherketone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Specific Gravity | 1.46 g/cc | 1.46 g/cc | ASTM D792 |
|
Teknor Apex Sinvicomp SSH 5509 Polyvinyl Chloride, Flexible
Availability: Asia Pacific Features: Good Flexibility Uses: Cable Jacketing; Wire and Cable Applications Wire Types: ST1; ST2; Type 9; Class 1/3 Agency Ratings: BS 6746; IEC 60502; JIS 6723 Forms: ..
|
|||
| Specific Gravity | 1.46 - 1.50 g/cc | 1.46 - 1.50 g/cc | ASTM D-792 |
|
Axiall 22951 Coax & Telecom Flexible PVC
Non-lead stabilized, 75C rated jacket compound suitable for riser constructions over HDPE.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
|
|||
| Specific Gravity | 1.46 g/cc | 1.46 g/cc | ASTM D792 |
|
Colorite Polymers 6718 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
|
|||
| Specific Gravity | 1.46 g/cc | 1.46 g/cc | ASTM D792 |
|
E-Polymers SEPAZ® LA40 PA66 LFT Resin
Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver..
|
|||
| Specific Gravity | 1.46 g/cc | 1.46 g/cc | ASTM D 792 |
|
SABIC Innovative Plastics LNP Thermocomp MF0069S PP
LNP* Thermocomp* MF0069S is a compound based on Polypropylene resin containing Glass Fiber, Flame Retardant. Added features of this material include: Chemically Coupled, Flame Retardant, Heat Stabi..
|
|||
| Specific Gravity | 1.46 g/cc | 1.46 g/cc | ASTM D792 |
|
SABIC Innovative Plastics Valox® VX4930 PBT (Europe-Africa-Middle East)
VALOX VX4930 is a 30% glass reinforced nucleated PBT/ASA blend with excellent mechanical properties, high dimensional stability and low density. Applications: connectors and automotive industry.
|
|||
| Specific Gravity | 1.46 g/cc | 1.46 g/cc | ASTM D792 |
|
Solvay Specialty Polymers Amodel® A-4133 L Polyphthalamide (PPA), Dry
(discontinued **)
Amodel A-4133L polyphthalamide (PPA) is a 33% glass reinforced resin designed to offer high crystallinity when molded in water-cooled molds. Key properties include high heat resistance, reduced outg..
|
|||