| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.54 g/cc | 1.54 g/cc | ASTM D792 |
|
PolyOne LubriOne™ PS-30GF/2S Natural Polybutylene Terephthalate (PBT)
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
|
|||
| Specific Gravity | 1.54 g/cc | 1.54 g/cc | (Dry) |
|
Radici Radilon® S RV500 (cond.) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
|
|||
| Specific Gravity | 1.54 g/cc | 1.54 g/cc | ASTM D792 |
|
Polymer Resources TP-FRG15 Polybutylene Terephthalate, 15% Glass Reinforced, Flame Retardant
Polybutylene Terephthalate, 15% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples..
|
|||
| Specific Gravity | 1.54 g/cc | 1.54 g/cc | ISO 1183 |
|
PolyOne Bergadur™ PB400 G30 H UF UV Polybutylene Terephthalate (PBT)
Information provided by PolyOne
|
|||
| Specific Gravity | 1.54 g/cc | 1.54 g/cc | ISO 1183 |
|
Lehmann & Voss LUVOCOM® 80-7112/BK Polyacetal-copolymer, with glass fiber and carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically ..
|
|||
| Specific Gravity | 1.54 - 1.60 g/cc | 1.54 - 1.60 g/cc | ASTM D 792 |
|
Karina E 820-10/1-D-TR White PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
|
|||
| Specific Gravity |
1.54
g/cc @Temperature 23.0 °C |
1.54
g/cc @Temperature 73.4 °F |
ASTM D792 |
|
Kingfa PBT-RG15 Flame Retardant, 15% Glass Fiber Reinforced PBT
Features:Flame retardantHigh strengthHigh temperature propertiesOutstanding electrical propertiesGood heat resistanceApplications:Injection moldingConnectorsRelayBobbins, plugsE & E partsInformation..
|
|||
| Specific Gravity | 1.54 g/cc | 1.54 g/cc | ASTM D792 |
|
Greene Tweed Orthetek® RP Polyketone, Random Carbon Fiber
Greene Tweed offers precision-molded thermoplastic components made form out high-performance Orthtek® composite materials for a variety of demanding medical device applications. Orthtek RP is id..
|
|||
| Specific Gravity | 1.54 g/cc | 1.54 g/cc | ASTM D792 |
|
Greene Tweed WRâ„¢ 575 PEEK, Bi-Directional Carbon Fiber Filled
WR®575 is a thermoplastic composite consisting of bi-directionally oriented carbon fibers in a PEEK matrix. The excellent wear resistance and the fiber orientation of WR575 makes this material i..
|
|||
| Specific Gravity | 1.54 g/cc | 1.54 g/cc | ASTM D792 |
|
SABIC Innovative Plastics LNP LUBRICOMP RFL36U PA 66
LNP* LUBRICOMP* RFL36U is a compound based on Nylon 66 resin containing 15% PTFE, 30% Glass Fiber. Added features of this grade include: Wear Resistant, UV Stabilized.
|
|||
| Specific Gravity | 1.54 g/cc | 1.54 g/cc | ASTM D792 |
|
SABIC Innovative Plastics Valox® 4031 PBT (Europe-Africa-Middle East)
VALOX 4031 is a 30% high strength glass fibre reinforced PBT injection moulding resin with excellent strength, stiffness and heat resistance. Applications: appliance handles, spotlights, electric mo..
|
|||
| Specific Gravity | 1.54 g/cc | 1.54 g/cc | ASTM D792 |
|
SABIC Innovative Plastics Valox® 830F PBT+PET (Asia Pacific)
PBT+PET, 30% Glass, Mold Release, Heat Stabilized, For food contact applications
|
|||
| Specific Gravity | 1.54 g/cc | 1.54 g/cc | |
|
Shinil Chemical SHINFLAME PC/PBT GF Flame Retardant Polymer Appliance
SHINFLAME is a flame retardant (FR) compound which exhibits inherent flame retardant properties during fire. Shinil uses its patented dispersion blending technology with variety of polymers to prod..
|
|||
| Specific Gravity | 1.54 g/cc | 1.54 g/cc | ASTM D792 |
|
Samsung Cheil Industries Infino® VB-5150GL PBT, 15% Glass Filled FR
Information provided by Samsung Cheil Industries.
|
|||
| Specific Gravity | 1.54 g/cc | 1.54 g/cc | ASTM D792 |
|
Teknor Apex APEX® 65005 Polyvinyl Chloride, Flexible
Notes: 75°C Jacket; RoHS Compliant Features: Flame Retardant Uses: Communication Wire Jacketing Forms: Pellets Agency Ratings: NEC Article 725; NEC Article 760; NEC Article 770; NEC Article 800; ..
|
|||
| Specific Gravity | 1.54 g/cc | 1.54 g/cc | ASTM D792 |
|
SABIC Innovative Plastics Valox® IQ420HP PBT
Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production..
|
|||
| Specific Gravity | 1.54 g/cc | 1.54 g/cc | ASTM D792 |
|
SABIC Innovative Plastics Valox® SHF4930 PBT (Europe-Africa-Middle East)
Super high flow FR PBT grade with 15% Glass reinforced
|
|||
| Specific Gravity | 1.54 g/cc | 1.54 g/cc | ASTM D792 |
|
Teknor Apex APEX® 65011 Polyvinyl Chloride, Flexible
Notes: 75°C Jacket; RoHS Compliant Uses: Wire and Cable ApplicationsForms: PelletsInformation Provided by Teknor Apex
|
|||
| Specific Gravity | 1.54 g/cc | 1.54 g/cc | ASTM D792 |
|
Adell HR-36 30% Glass Reinforced Heat Stabilized PBT |
|||
| Specific Gravity | 1.54 g/cc | 1.54 g/cc | |
|
Aremco Corr-Paint™ CP3015-BL High Temperature Protective Coating Inorganic, Mixed Oxides Filled
These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. High emissivity, inorganic black pigmented coating to 15..
|
|||
| Specific Gravity | 1.54 g/cc | 1.54 g/cc | ASTM D792 |
|
BLUESTAR 201G20 PBT, 20% Glass Filled
Typical Applications: Energy saving lightingInformation provided by Polymer Technology and Services, LLC (PTS).
|
|||