| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.54 g/cc | 1.54 g/cc | ASTM D-792 |
|
PlastiComp Complet® LCF15/LGF35 – PA66 BLK Polyamide 66, 50% Long Carbon/Glass Fiber
Composite PelletsInformation provided by PlastiComp, Inc.
|
|||
| Specific Gravity | 1.54 g/cc | 1.54 g/cc | ASTM D792 |
|
PolyOne Edgetek® PK-30GF/000 Polyetheretherketone (PEEK)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
|
|||
| Specific Gravity | 1.54 g/cc | 1.54 g/cc | ASTM D792 |
|
Solvay Specialty Polymers Amodel® A-1340 HS Polyphthalamide (PPA) Resin, 40% Mineral/Glass Reinforced, at 50% RH
&n
AMODEL® A-1340 HS is a 40% mineral/glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, high tensile strength and low warpage..
|
|||
| Specific Gravity | 1.54 g/cc | 1.54 g/cc | ASTM D792 |
|
Gromax PET 9030-104E 30% Glass/Mineral Filled
Product Description: PET glass 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excellent wear..
|
|||
| Specific Gravity | 1.54 - 1.60 g/cc | 1.54 - 1.60 g/cc | ASTM D 792 |
|
Karina E 820-10/1-D-TR White PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
|
|||
| Specific Gravity | 1.54 g/cc | 1.54 g/cc | ASTM D792 |
|
SABIC Innovative Plastics Valox® 830F PBT+PET
PBT+PET, 30% Glass, Mold Release, Heat Stabilized, For food contact applications
|
|||
| Specific Gravity | 1.54 g/cc | 1.54 g/cc | ASTM D792 |
|
SABIC Innovative Plastics Valox® 830F PBT+PET (Asia Pacific)
PBT+PET, 30% Glass, Mold Release, Heat Stabilized, For food contact applications
|
|||
| Specific Gravity | 1.54 g/cc | 1.54 g/cc | ASTM D792 |
|
SABIC Innovative Plastics Valox® 830F PBT+PET (Europe-Africa-Middle East)
PBT+PET, 30% Glass, Mold Release, Heat Stabilized, For food contact applications
|
|||
| Specific Gravity | 1.54 g/cc | 1.54 g/cc | |
|
Shin-Etsu Silicones KE-1204 B Silicone, Potting/Encapsulation RTV
Information Provided by Shin-Etsu Silicones of America, Inc.
|
|||
| Specific Gravity | 1.54 g/cc | 1.54 g/cc | ASTM D792 |
|
SABIC Innovative Plastics LNP STAT-KON OEL36A PPS - BRANCHED
LNP* STAT-KON* OEL36A is a compound based on PPS - Branched resin containing 15% PTFE, 30% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive.
|
|||
| Specific Gravity | 1.54 g/cc | 1.54 g/cc | ASTM D792 |
|
Samsung Cheil Industries Infino® VB-5150GL PBT, 15% Glass Filled FR
Information provided by Samsung Cheil Industries.
|
|||
| Specific Gravity | 1.54 g/cc | 1.54 g/cc | ASTM D792 |
|
Teknor Apex APEX® 65007 Polyvinyl Chloride, Flexible
Notes: 90°C Jacket; RoHS Compliant Uses: Wire and Cable ApplicationsForms: PelletsInformation Provided by Teknor Apex
|
|||
| Specific Gravity | 1.54 g/cc | 1.54 g/cc | ASTM D792 |
|
SABIC Innovative Plastics LNP THERMOCOMP RX10408H PA 66
LNP* Thermocomp* RX10408H is a compound based on Nylon 66 containing Proprietary Fillers. Characteristics are: Radiopacity and Healthcare.
|
|||
| Specific Gravity | 1.54 g/cc | 1.54 g/cc | ASTM D792 |
|
SABIC Innovative Plastics Valox® 451E PBT (Europe-Africa-Middle East)
VALOX 451E is 20% glass reinforced, flame retardant PBT injection moulding resin.
|
|||
| Specific Gravity |
1.54
g/cc @Temperature 25.0 °C |
1.54
g/cc @Temperature 77.0 °F |
|
|
Dow Corning SILASTIC® HV 1666/65 GRAY SILICONE RUBBER
65 Durometer, gray, peroxide cure, high voltage grade Silicone Rubber Compound for manufacturing High Voltage insulators weather shed insulators or surge arrestors. Superior wet electrical propertie..
|
|||
| Specific Gravity | 1.54 g/cc | 1.54 g/cc | DAM; ASTM D792 |
|
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66
(Unverified Data**)
Zytel® FR70G25V0 NC010 is a 25% glass fiber reinforced, heat stabilized, flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Specific Gravity | 1.54 g/cc | 1.54 g/cc | ASTM D792 |
|
Gromax PBT 4115-201D 15% Glass Fiber Filled
Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
|
|||
| Specific Gravity | 1.54 g/cc | 1.54 g/cc | ASTM D792 |
|
Solvay Specialty Polymers Amodel® A-1240 L Polyphthalamide (PPA)
(discontinued **)
Amodel A-1240 L is a 40% mineral filled polyphthalamide (PPA) that offers low warpage and excellent dimensional stability. This resin also has a high deflection temperature, flexural modulus and ten..
|
|||
| Specific Gravity | 1.54 g/cc | 1.54 g/cc | ASTM D792 |
|
SABIC Innovative Plastics LNP THERMOCOMP JF004L PES
LNP* THERMOCOMP* JF004L is a compound is based on Polyethersulfone containing 20% Glass Fiber. Characteristics of this grade is: Low Extractible
|
|||