| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 2.15 g/cc | 2.15 g/cc | ASTM D792 |
| Quadrant EPP Symalit® PFA Tetrafluoroethylene-perfluoroalkylvinylether (ASTM Product Data Sheet) |
|||
| Specific Gravity | 2.15 g/cc | 2.15 g/cc | ASTM D792 |
| 3M Dyneon™ PFA 6525N Perfluoroalkoxy Fluorothermoplastic
(discontinued **) The excellent chemical temperature resistance of Dyneon™ 6500N PFA is available across a range of melt flow indices, for optimal processability. Dyneon™ PFA 6502N, the highest molecular weight gra.. |
|||
| Specific Gravity | 2.15 - 2.24 g/cc | 2.15 - 2.24 g/cc | ASTM D792 |
| Technetics Group Texolon™ 9406 PTFE
(Unverified Data**) General purpose 25% glass filled PTFE for applications less demandingPTFE CharacteristicsChemical ResistanceThermal StabilityCryogenic PropertiesLow Coefficient of FrictionLow Surface EnergyLow Diel.. |
|||
| Specific Gravity | 2.15 g/cc | 2.15 g/cc | Internal method |
| Shamrock Technologies Fluoro T® 607 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
| Specific Gravity | 2.15 g/cc | 2.15 g/cc | Internal method |
| Shamrock Technologies Fluoro T® 615 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
| Specific Gravity | 2.15 g/cc | 2.15 g/cc | Internal method |
| Shamrock Technologies Fluoro T® 702 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
| Specific Gravity | 2.15 g/cc | 2.15 g/cc | Internal method |
| Shamrock Technologies Fluoro T® 802 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
| Specific Gravity | 2.15 g/cc | 2.15 g/cc | Internal method |
| Shamrock Technologies MicroFLON® 1433FG Thermoplastic Grade PTFE Additive Used with high temperature engineering plastics; food contactThe addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wea.. |
|||
| Specific Gravity | 2.15 g/cc | 2.15 g/cc | ASTM D-792 |
| Saint-Gobain Norton® Fluorglas® Chemfilm® DF1400 Non-Conductive PTFE Tape Description: Chemfilm® Fluoropolymer Cast Films and Tapes for Wire and Cable Industry: Multi-layer cast film process ensures inherently pin-hole free structure, therefore cast films possess super.. |
|||
| Specific Gravity | 2.15 g/cc | 2.15 g/cc | ASTM D-792 |
| Saint-Gobain Norton® T-100 Virgin Skived PTFE Film (0.002" thick) T-100/T-200 Features/Benefits: Outstanding heat and chemical resistance; High dielectric strength; Anti-stick properties; Can be chemically etched for bondability; Applications include laminate rele.. |
|||
| Specific Gravity | 2.15 g/cc | 2.15 g/cc | ASTM D-792 |
| Saint-Gobain Norton® T-100 Virgin Skived PTFE Film (0.006" thick) T-100/T-200 Features/Benefits: Outstanding heat and chemical resistance; High dielectric strength; Anti-stick properties; Can be chemically etched for bondability; Applications include laminate rele.. |
|||
| Specific Gravity | 2.15 g/cc | 2.15 g/cc | ASTM D-792 |
| Saint-Gobain Norton® T-100 Virgin Skived PTFE Sheet (0.125" thick) T-100/T-200 Features/Benefits: Outstanding heat and chemical resistance; High dielectric strength; Anti-stick properties; Can be chemically etched for bondability; Applications include laminate rele.. |
|||
| Specific Gravity | 2.15 g/cc | 2.15 g/cc | ASTM D-792 |
| Saint-Gobain Norton® T-100 Virgin Skived PTFE Sheet (0.250" thick) T-100/T-200 Features/Benefits: Outstanding heat and chemical resistance; High dielectric strength; Anti-stick properties; Can be chemically etched for bondability; Applications include laminate rele.. |
|||
| Specific Gravity | 2.15 g/cc | 2.15 g/cc | ASTM D-792 |
| Saint-Gobain Norton® T-200 Mechanical Grade PTFE Sheet (0.188" thick) Features/Benefits: Outstanding heat and chemical resistance; High dielectric strength; Anti-stick properties; Can be chemically etched for bondability; Applications include laminate release sheets, .. |
|||
| Specific Gravity | 2.15 g/cc | 2.15 g/cc | Internal method |
| Shamrock Technologies Fluoro T® 603 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
| Specific Gravity | 2.15 g/cc | 2.15 g/cc | at 25°C |
| Daikin NEOFLON AP-211SH PFA Semiconductor Grade NEOFLON PFA semiconductor grade.Applications: Tubing and injection molded parts requiring high stress crack resistance, etc.Information provided by Daikin Industries. |
|||
| Specific Gravity | 2.15 g/cc | 2.15 g/cc | ASTM D792 |
| 3M Dyneon™ FEP 6303Z Fluorinated Ethylene Propylene Fluorothermoplastic Granules Dyneon FEP 6303Z is offered for extrusion, injection molding and transfer molding for the wire and cable and chemical process industries. Their distinguishing features include: Excellent electrical .. |
|||
| Specific Gravity | 2.15 g/cc | 2.15 g/cc | ASTM D792 |
| 3M Dyneon™ FEP 6322Z Fluorinated Ethylene Propylene Fluorothermoplastic Granules Dyneon FEP 6322Z was designed primarily for high-speed extrusion for wire insulation. Its distinguishing features include:High extrusion speedHigh thermal stabilityWide processing windowSuperior ele.. |
|||
| Specific Gravity | 2.15 g/cc | 2.15 g/cc | |
| 3M Dyneon™ PFA 6502 UHPZ Perfluoroalkoxy Fluorothermoplastic Granules Dyneon PFA X 6502 UPH, PFA X 6505 UHP and PFA X 6515 UHP are a new series of ultra-high purity fluorothermoplastics. These resins were developed for high-purity applications requiring ultra-low leve.. |
|||
| Specific Gravity | 2.15 g/cc | 2.15 g/cc | ASTM D792 |
| 3M Dyneon™ PFA 6503PAZ Fluoroplastic Powder 3M™ Dyneon™ Fluoroplastic Powder PFA 6503PAZ is a fluorothermoplastic powder designed for use in thin film powder coatings. Typical applications include non-stick surfaces, chemical vessel and tan.. |
|||
| Specific Gravity | 2.15 g/cc | 2.15 g/cc | Dry Polymer; ASTM D792 |
| 3M Dyneon™ PFA 6910GZ Fluoroplastic Dispersion 3M™ Dyneon™ PFA 6910GZ is a 50% solids fluorothermoplastic aqueous dispersion. It is a copolymer of tetrafluoroethylene and perfluorinated comonomers, with a melt viscosity several orders of magni.. |
|||
| Specific Gravity | 2.15 g/cc | 2.15 g/cc | |
| Bulk Molding Compounds BMC 3001H Mineral Filled Alkyd BMC 3001H molding compound is a mineral filled, glass-fiber reinforced alkyd compound suitable for compression and transfer molding. Because of its soft flow, it is also used extensively in cold spu.. |
|||
| Specific Gravity | 2.15 - 2.17 g/cc | 2.15 - 2.17 g/cc | ASTM D792 |
| Adamas Adalon® 503 PTFE, 0.1% MoS2 Information provided by Adamas, HPM |
|||
| Specific Gravity | 2.15 g/cc | 2.15 g/cc | ASTM D792 |
| 3M Dyneon™ FEP 6307Z Fluorinated Ethylene Propylene Fluorothermoplastic Granules Dyneon FEP 6307Z is offered for extrusion, injection molding and transfer molding for the wire and cable and chemical process industries. Their distinguishing features include: Excellent electrical .. |
|||
| Specific Gravity | 2.15 g/cc | 2.15 g/cc | ASTM D792 |
| 3M Dyneon™ PFA 6515 UHPZ Perfluoroalkoxy Fluorothermoplastic Granules Dyneon PFA X 6502 UPH, PFA X 6505 UHP and PFA X 6515 UHP are a new series of ultra-high purity fluorothermoplastics. These resins were developed for high-purity applications requiring ultra-low leve.. |
|||
| Specific Gravity | 2.15 g/cc | 2.15 g/cc | @ 23°C, Sintering Molding; ASTM D4894-98a |
| 3M Dyneon™ TF 1641 PTFE Meets ASTM D4894 Type IV, Grade 2 resinMolding and ram extrusion powder very good free-flow propertiesGood metering propertiesGood mold filling behaviorGood electrical and mechanical propertiesVery .. |
|||
| Specific Gravity | 2.15 - 2.16 g/cc | 2.15 - 2.16 g/cc | ASTM D792 |
| Adamas Adalon® 600 PTFE, Boro Nitruro Information provided by Adamas, HPM |
|||