Physical Properties Metric English Comments
Specific Gravity 3.00 - 3.60 g/cc
3.00 - 3.60 g/cc
Parker Chomerics CHO-BOND SV712 Conductive Epoxy
CHO-BOND® 700 Series Adhesives for Microelectronics Packaging; these pure silver-filled epoxy pastes are designed to meet the demanding requirements of semiconductor and microelectronic packaging. ..
Specific Gravity 3.00 g/cc
3.00 g/cc
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP 9H0300C
LNP* Thermocomp* 9H0300C is a High Specific Gravity compound containing proprietary fillers.
Specific Gravity 3.00 g/cc
3.00 g/cc
Master Bond MB600SCN Aqueous Based Electrically Conductive Sodium Silicate Coating
Master Bond MB600SCN is an aqueous based, sodium silicate system with a silver coated nickel filler. It is intended for use in applications where very good shielding effectiveness is required and co..
Specific Gravity 3.00 g/cc
3.00 g/cc
Unifrax Fiberfrax® Fibermax® Mat Ceramic Fiber Insulator
Fibermax Mat is a high-temperature, flexible mat product that is lightweight (1.5 lb/ft3 density) and highly resilient. It is composed entirely of Fibermax polycrystalline mullite fibers to produce..
Specific Gravity 3.00 g/cc
3.00 g/cc
Unifrax Fibermax® Needled Blanket
Fibermax® Needled Blankets are high temperature, light weight and flexible products manufactured from polycrystalline mullite fiber that can be exposed to temperatures up to 1600°C (2912°F). Fib..
Specific Gravity 3.00 g/cc
3.00 g/cc
Mixed, degassed
Tra-Con Tra-Duct 29121 Snap Cure Conductive Silver Epoxy Adhesive
TRA-DUCT 29121 is 100% solids, two component silver filled epoxy designed for chip bonding in microelectronic and optoelectronic applications. TRA-DUCT 29121 is a soft, smooth paste. This two-part f..
Specific Gravity 3.00 g/cc
3.00 g/cc
Unifrax Fiberfrax® Fibermax Bulk Mullite High-Temperature Fiber
In addition to Fiberfrax Bulk Fibers, Unifrax has the ability to produce many different specialty fibers that provide a variety of desirable performance properties for certain applications. These f..
Specific Gravity 3.00 g/cc
3.00 g/cc
at 25°C
Daikin DAI-EL G-952 Fluoroelastomer Terpolymer, Peroxide Curable Grade, 69% Fluorine Content
Offers excellent chemical and steam resistance. Offers good mechanical characteristics.Features: Good solvent resistance and low-temperature characteristics.Information provided by Daikin Industrie..
Specific Gravity 3.00 g/cc
3.00 g/cc
ISO 1183
Ecomass® 705ZC75 Stainless Steel Filled ABS
Nontoxic Alternative to traditional metals, weighting and balancing applicationsModerate Specific GravityStainless Steel Powder Filled ABSInformation provided by Technical Polymers
Specific Gravity 3.00 g/cc
3.00 g/cc
ISO 1183
Ecomass® 705ZD70 Tungsten Filled ABS
Nontoxic Alternative to Lead (Pb) for radiation shielding applicationsHigh specific GravityTungsten Filled ABS compoundRigidGood ToughnessInformation provided by Technical Polymers
Specific Gravity 3.00 g/cc
3.00 g/cc
Aremco AREMCOLOX™ 502-1400 (Bisque-fired) Machinable Alumina
Good corrosion electrical and thermal shock resistance. Plates from 1/4" to 3/4" thick; rods from 1/4" to 3" diameter. Easily machined using conventional tools, no firing required.
Specific Gravity 3.00 g/cc
3.00 g/cc
Aremco AREMCOLOX™ 502-400 Machinable Glass Ceramic
High dielectric and mechanical strength. For high voltage insulators, coil forms, soldering fixtures, arc barriers. Readily machined, no firing required. Plates from 1/8" to 1" thick; rods from 1..