| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Kinematic Viscosity at 40°C (104°F) | 103 cSt | 103 cSt | Base Oil; ASTM D445 |
|
Nye Lubricants 186 (SO) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Kinematic Viscosity at 40°C (104°F) | 103 cSt | 103 cSt | |
|
ExxonMobil Mobil Clean 10W-40 High Mileage
Mobil Clean High Mileage is formulated from high quality base stocks combined with the modern performance additives, including a seal conditioner to help prevent leaks in higher mileage vehicles and..
|
|||
| Kinematic Viscosity at 40°C (104°F) | 103 cSt | 103 cSt | |
|
ConocoPhillips 100 FR Hydraulic Fluid ISO
Description: Conoco FR Hydraulic Fluid is a fire-resistant, water-in-oil, invert-emulsion fluid for hydraulic systems, such as those found in underground mining equipment in which fire hazard and pe..
|
|||
| Kinematic Viscosity at 40°C (104°F) | 103 cSt | 103 cSt | Base Oil Property |
|
ConocoPhillips ANDEROL® Assembly Lube Premium Quality White Mineral Oil Food Grade Grease, NLGI 1.5
Description: ANDEROL PQ Assembly Lube grease is made from pure white mineral oil and additives to produce a general purpose food grade grease for lubrication of enclosed bearings, o-rings and other ..
|
|||
| Kinematic Viscosity at 40°C (104°F) | 103 cSt | 103 cSt | |
|
ConocoPhillips El Mar® 2000 Oil SAE Grade 15W-40
Conoco® El Mar 2000 is a high-quality, very low-ash, dispersant detergent gas engine oil designed for use in naturally aspirated and moderately turbocharged, low- to medium-speed 2-stroke cycle and..
|
|||
| Kinematic Viscosity at 40°C (104°F) | 103 cSt | 103 cSt | |
|
ExxonMobil Mobil Clean 10W-40 High Mileage
Mobil Clean High Mileage is formulated from high quality base stocks combined with the modern performance additives, including a seal conditioner to help prevent leaks in higher mileage vehicles and..
|
|||