| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Kinematic Viscosity at 40°C (104°F) | 110 cSt | 110 cSt | Base Oil; ASTM D445 |
|
Nye Lubricants 188B (SO) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Kinematic Viscosity at 40°C (104°F) | 110 cSt | 110 cSt | Base Oil; ASTM D445 |
|
Nye Lubricants 740MS(RL) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Kinematic Viscosity at 40°C (104°F) | 110 cSt | 110 cSt | Base Oil; ASTM D445 |
|
Nye Lubricants 740S (RL) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Kinematic Viscosity at 40°C (104°F) | 110 cSt | 110 cSt | ASTM D445 |
|
ExxonMobil 30 Exxon XD-3
Exxon XD-3 20, 30, 40 and 50 are premium diesel engine oils blended from high quality base oils and a balanced additive system to meet or exceed the lubrication protection requirements of American d..
|
|||
| Kinematic Viscosity at 40°C (104°F) | 110 cSt | 110 cSt | |
|
ChevronTexaco URSA® SAE 30 Extra Duty
Texaco Ursa Extra Duty oils deliver value through:Excellent high temperature deposit control. Protects against high temperature oxidation and oil thickening.Special extreme pressure antiwear propert..
|
|||
| Kinematic Viscosity at 40°C (104°F) | 110 cSt | 110 cSt | ASTM D445 |
|
ExxonMobil 30 Exxon XD-3
Exxon XD-3 20, 30, 40 and 50 are premium diesel engine oils blended from high quality base oils and a balanced additive system to meet or exceed the lubrication protection requirements of American d..
|
|||
| Kinematic Viscosity at 40°C (104°F) | 110 cSt | 110 cSt | ASTM D-445 |
|
ConocoPhillips ANDEROL® 40 AA-1 Grease, White Mineral Food Grade NLGI 1
Description: ANDEROL PQ 40 AA Greases are aluminum complex thickened, white mineral oil-based products that meet the former H-1 approval requirements of the USDA where incidental food contact can oc..
|
|||
| Kinematic Viscosity at 40°C (104°F) | 110 cSt | 110 cSt | ASTM D-445 |
|
ConocoPhillips ANDEROL® 40 AA-2 Grease, White Mineral Food Grade NLGI 2
Description: ANDEROL PQ 40 AA Greases are aluminum complex thickened, white mineral oil-based products that meet the former H-1 approval requirements of the USDA where incidental food contact can oc..
|
|||
| Kinematic Viscosity at 40°C (104°F) | 110 cSt | 110 cSt | |
|
ConocoPhillips Hydroclear® El Mar® 15W-40 Ashless Heavy Duty
Description: Conoco Hydroclear El Mar Ashless Heavy Duty is a high-quality, ashless natural gas engine oil formulated from exclusive Conoco hydrocracked base stock. Hydroclear El Mar Ashless Heavy D..
|
|||
| Kinematic Viscosity at 40°C (104°F) | 110 cSt | 110 cSt | |
|
ConocoPhillips Hydroclear® El Mar® 15W-40 Ashless Supreme
Description: Conoco Hydroclear El Mar Ashless Supreme is a premium ashless natural gas engine oil formulated from exclusive Conoco hydrocracked base stock. Hydroclear El Mar Ashless Supreme is speci..
|
|||
| Kinematic Viscosity at 40°C (104°F) | 110 cSt | 110 cSt | |
|
ConocoPhillips Hydroclear® El Mar® 15W-40 Low Ash Heavy Duty
Description: Conoco Hydroclear El Mar Low Ash Heavy Duty is a high-quality low ash natural gas engine oil formulated from exclusive Conoco hydrocracked base stock. Hydroclear El Mar Low Ash Heavy Du..
|
|||
| Kinematic Viscosity at 40°C (104°F) | 110 cSt | 110 cSt | Base Oil |
|
ConocoPhillips Polyurea NLGI Grade No. 1
Polyurea Greases offer significant performance advantages in high temperature, multipurpose, long-life and wet applications over conventional soap thickened greases. The nonsoap, polyurea thickener,..
|
|||
| Kinematic Viscosity at 40°C (104°F) | 110 cSt | 110 cSt | ASTM D445 |
|
ChevronTexaco Delo® 100 Motor Oil, SAE 30
Chevron Delo 100 Motor Oils are high performance crankcase oils for diesel engines.They are manufactured using selected premium paraffinic base oils and detergent, dispersant, wear control, antioxid..
|
|||
| Kinematic Viscosity at 40°C (104°F) | 110 cSt | 110 cSt | ASTM D445 |
|
ChevronTexaco Delo® 1000 Marine Engine Oil, SAE 30
FeaturesChevron Marine Engine Oils Delo 1000 Marine are highquality engine oils developed for use in a wide variety of medium speed trunk piston engines, including the latest design high output engi..
|
|||
| Kinematic Viscosity at 40°C (104°F) | 110 cSt | 110 cSt | Base Oil |
|
ConocoPhillips Polyurea NLGI Grade No. 2
Polyurea Greases offer significant performance advantages in high temperature, multipurpose, long-life and wet applications over conventional soap thickened greases. The nonsoap, polyurea thickener,..
|
|||