| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Kinematic Viscosity at 40°C (104°F) | 146 cSt | 146 cSt | Base Oil; ASTM D445 |
|
Nye Lubricants 759T (NG) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Kinematic Viscosity at 40°C (104°F) | 146 cSt | 146 cSt | ASTM D445 |
|
ExxonMobil Extra Heavy Mobil DTE Oil Double Letter Series
The Mobil DTE Oil Double Letter Series of lubricants are high performance heavy duty circulating oils primarily intended for continuous reuse in circulation lubrication systems for gears and bearing..
|
|||
| Kinematic Viscosity at 40°C (104°F) | 146 cSt | 146 cSt | ASTM D445 |
|
ChevronTexaco Delo® 400 SAE 40
Chevron Delo 400 heavy duty motor oils are exceptional, super premium quality “universal” engine oils which exceed industry and engine manufacturers’ performance requirements.They are formulated ..
|
|||
| Kinematic Viscosity at 40°C (104°F) | 146 cSt | 146 cSt | |
|
ChevronTexaco URSA® SAE 40 Premium TDX
Texaco Ursa Premium TDX delivers value through:Reduced wear — Prolonging component life and providing reduced maintenance costs.Improved engine cleanliness — Providing efficient operation and redu..
|
|||
| Kinematic Viscosity at 40°C (104°F) | 146 cSt | 146 cSt | ASTM D445 |
|
ExxonMobil Extra Heavy Mobil DTE Oil Double Letter Series
The Mobil DTE Oil Double Letter Series of lubricants are high performance heavy duty circulating oils primarily intended for continuous reuse in circulation lubrication systems for gears and bearing..
|
|||
| Kinematic Viscosity at 40°C (104°F) | 146 cSt | 146 cSt | |
|
ConocoPhillips Conoco® El Mar® Grade 40 Mid Ash Supreme Oil
Conoco® El Mar Mid Ash Supreme is a premium quality, mid-ash, dispersant-detergent gas engine oil designed for use in naturally aspirated and moderately to highly turbocharged 4-stroke cycle natura..
|
|||