Polymer Property : Kinematic Viscosity at 40°C (104°F) = 2000 cSt Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 2000 cSt
2000 cSt
Base Oil; ASTM D445
Nye Lubricants 520C-2 (NT) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 2000 cSt
2000 cSt
Base Oil; ASTM D445
Nye Lubricants 520M-2 (NT) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 2000 cSt
2000 cSt
Base Oil; ASTM D445
Nye Lubricants 520M-2-UV (NT) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 2000 cSt
2000 cSt
Base Oil; ASTM D445
Nye Lubricants 523V-2-UV (NT) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 2000 cSt
2000 cSt
Base Oil; ASTM D445
Nye Lubricants 779 (NG) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 2000 cSt
2000 cSt
Base Oil; ASTM D445
Nye Lubricants 779ZC (NG) Synthetic Oil
Information provided by Nye Lubricants.