Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Kinematic Viscosity at 40°C (104°F) = 22 cSt Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 22 cSt
22 cSt
Base Oil; ASTM D445
Nye Lubricants 716R (RL) Rheolube Grease
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 22 cSt
22 cSt
ASTM D445
ExxonMobil 12M Mobil DTE 10M Series
Mobil DTE 10M Series oils are supreme performance anti-wear hydraulic oils engineered for wide temperature range applications. They exhibit optimum flow characteristics at sub-zero temperatures and ..
Kinematic Viscosity at 40°C (104°F) 22 cSt
22 cSt
ASTM D445
ExxonMobil 424 Mobilmet 400 Series
Mobilmet 400 Series products are high-performance multi-purpose cutting oils. They are chlorine-free, non-staining and non-corrosive. They are designed for light to moderate duty cutting operation..
Kinematic Viscosity at 40°C (104°F) 22 cSt
22 cSt
ConocoPhillips Syncon® 22 Synthetic AW Hydraulic Fluid 22
Syncon AW Hydraulic Fluid is a premium quality, synthetic antiwear hydraulic fluid developed for use in industrial and mobile equipment operating at extreme temperatures. It is particularly recommen..
Kinematic Viscosity at 40°C (104°F) 22 cSt
22 cSt
ASTM D445, DIN 51 561
Chesterton 601 Chain Drive Pin & Bushing Lubricant
Description: Chesterton® 601 Chain Drive Pin & Bushing Lubricant is and has been the premium quality light lubricant of choice in industry for over thirty years. This superior lubricant was special..
Kinematic Viscosity at 40°C (104°F) 22 cSt
22 cSt
ASTM D445
ChevronTexaco RPM® NLGI 1 Arctic Grease
Chevron RPM Arctic Grease is a premium quality grease.It is manufactured using a polyurea acetate complex thickener, special low viscosity base oil, and rust and oxidation inhibitors. It is black in..
Kinematic Viscosity at 40°C (104°F) 22 cSt
22 cSt
ASTM D445
ExxonMobil 12M Mobil DTE 10M Series
Mobil DTE 10M Series oils are supreme performance anti-wear hydraulic oils engineered for wide temperature range applications. They exhibit optimum flow characteristics at sub-zero temperatures and ..
Kinematic Viscosity at 40°C (104°F) 22 cSt
22 cSt
ASTM D445
ExxonMobil 424 Mobilmet 400 Series
Mobilmet 400 Series products are high-performance multi-purpose cutting oils. They are chlorine-free, non-staining and non-corrosive. They are designed for light to moderate duty cutting operation..
Kinematic Viscosity at 40°C (104°F) 22 cSt
22 cSt
ASTM D445
ExxonMobil Mobil Velocite 10
The Mobil Velocite Oil Numbered Series oils are premium performance products primarily designed for the lubrication of high-speed spindles in machine tools. They are also used in some critical hydra..
Kinematic Viscosity at 40°C (104°F) 22 cSt
22 cSt
ConocoPhillips Hydroclear® 22 AW Hydraulic Fluid
Description: Conoco Hydroclear AW Hydraulic Fluid is specifically designed for use in high-pressure systems which require greater wear protection and deposit control than that provided by standard a..
Kinematic Viscosity at 40°C (104°F) 22 cSt
22 cSt
ConocoPhillips Hydroclear® 22 Quench Oil
Description: Conoco Hydroclear® Quench Oil is a high-quality metal heat-treating and quenching oil formulated from premium Conoco hydrocracked base stocks. Hydroclear Quench Oil is specially formul..
Kinematic Viscosity at 40°C (104°F) 22 cSt
22 cSt
ConocoPhillips 22 Super Hydraulic Oil
Description: Conoco Super Hydraulic Oil is a high-quality antiwear hydraulic fluid formulated from premium Conoco hydrocracked base stocks to provide superior water separation, antiwear protection, ..
Kinematic Viscosity at 40°C (104°F) 22 cSt
22 cSt
ConocoPhillips Hydroclear® 115 Industrial Oil
Description: Conoco Hydroclear Industrial Oil is a high-quality, general-purpose industrial lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Industrial Oil is recommende..
Kinematic Viscosity at 40°C (104°F) 22 cSt
22 cSt
ASTM D445, DIN 51 561
Chesterton 651 Detergent Lubricating Oil
Description: Chesterton® 651 Detergent Lubricating Oil is the plant-wide product of choice for superior-quality, low-viscosity, industrial lubricating needs. It is a cost-effective oil with high de..
Kinematic Viscosity at 40°C (104°F) 22 cSt
22 cSt
ASTM D445
ExxonMobil Mobil Velocite 10
The Mobil Velocite Oil Numbered Series oils are premium performance products primarily designed for the lubrication of high-speed spindles in machine tools. They are also used in some critical hydra..
Kinematic Viscosity at 40°C (104°F) 22 cSt
22 cSt
ASTM D445, DIN 51 561
Chesterton 652 Pneumatic Lubricant & Conditioner
Description: Chesterton® 652 Pneumatic Lubricant & Conditioner is a high performance, low viscosity, lubricating formula designed to creep into the internal workings of air tools, reduce wear and e..
Kinematic Viscosity at 40°C (104°F) 22 cSt
22 cSt
ASTM D445, DIN 51 561
Chesterton 690 FG Lubricant
Description: Chesterton® 690 FG Lubricant is a high-quality, cost-effective penetrating lubricant. Used in food processing, beverage and pharmaceutical plants, 690 FG Lubricant can go where few pro..
Copyright © lookpolymers.com All Rights Reserved