| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Kinematic Viscosity at 40°C (104°F) | 35.9 cSt | 35.9 cSt | ASTM D445 |
|
ChevronTexaco ATF+3® Automatic Transmission Fluid
General DescriptionDaimlerChrysler has had their own ATF specifications for many years, but as of 1997, Chrysler owners manuals no longer list DEXRON as an acceptable replacement. ATF+3 is a readily..
|
|||
| Kinematic Viscosity at 40°C (104°F) | 35.9 cSt | 35.9 cSt | |
|
ChevronTexaco Transultex® CF D
Texaco Transultex CF metalworking fluids deliver value through:Excellent antiweld properties from active sulfur and chlorine-free EP compounding which reduce frictional heat, prevent welding of meta..
|
|||
| Kinematic Viscosity at 40°C (104°F) | 35.9 cSt | 35.9 cSt | |
|
ChevronTexaco Havoline® ATF+3® Automatic Transmission Fluid
Havoline Automatic Transmission Fluid ATF+3 delivers value through:Correct viscosity and frictional characteristics to ensure smooth operation in Chrysler transmissions.Long-lasting viscosity modifi..
|
|||