| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Kinematic Viscosity at 40°C (104°F) | 390 cSt | 390 cSt | Base Oil; ASTM D445 |
|
Nye Lubricants 369VF Grease
Information provided by Nye Lubricants.
|
|||
| Kinematic Viscosity at 40°C (104°F) | 390 cSt | 390 cSt | Base Oil; ASTM D445 |
|
Nye Lubricants 759F (NG) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Kinematic Viscosity at 40°C (104°F) | 390 cSt | 390 cSt | Base Oil; ASTM D445 |
|
Nye Lubricants 759G (NG) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Kinematic Viscosity at 40°C (104°F) | 390 cSt | 390 cSt | Base Oil; ASTM D445 |
|
Nye Lubricants 759X (NG) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Kinematic Viscosity at 40°C (104°F) | 390 cSt | 390 cSt | Base Oil; ASTM D445 |
|
Nye Lubricants 760A (NG) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Kinematic Viscosity at 40°C (104°F) | 390 cSt | 390 cSt | Base Oil; ASTM D445 |
|
Nye Lubricants 760G (NG) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Kinematic Viscosity at 40°C (104°F) | 390 cSt | 390 cSt | Base Oil; ASTM D445 |
|
Nye Lubricants 760H (NG) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Kinematic Viscosity at 40°C (104°F) | 390 cSt | 390 cSt | Base Oil; ASTM D445 |
|
Nye Lubricants 759P (NG) Synthetic Oil
Information provided by Nye Lubricants.
|
|||