| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Kinematic Viscosity at 100°C (212°F) | 31.5 cSt | 31.5 cSt | ASTM D445 |
|
ExxonMobil 34 Mobil Mist Lube Series
Mobil Mist Lube Series are extra high performance oils designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. They are formulated from hig..
|
|||
| Kinematic Viscosity at 100°C (212°F) | 31.5 cSt | 31.5 cSt | ASTM D445 |
|
ChevronTexaco ParaMount™ ELV Paraffinic Process Oil
FeaturesChevron ParaMount ELV Paraffinic Process Oil offers all the advantages of a bright stock including low weight loss and excellent solubility.ELV is exceptional because of its very light color..
|
|||
| Kinematic Viscosity at 100°C (212°F) | 31.5 cSt | 31.5 cSt | ASTM D445 |
|
ExxonMobil 34 Mobil Mist Lube Series
Mobil Mist Lube Series are extra high performance oils designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. They are formulated from hig..
|
|||
| Kinematic Viscosity at 100°C (212°F) | 31.5 cSt | 31.5 cSt | Base Oil |
|
ConocoPhillips 1 HD Calcium Grease NLGI No. 1
Description: Conoco HD Calcium Grease is a formulated product, ideally suited for equipment exposed to corrosive fluids, saltwater or extremely high temperatures. HD Calcium Grease is used exclusive..
|
|||
| Kinematic Viscosity at 100°C (212°F) | 31.5 cSt | 31.5 cSt | Base Oil |
|
ConocoPhillips 2 HD Calcium Grease NLGI No. 2
Description: Conoco HD Calcium Grease is a formulated product, ideally suited for equipment exposed to corrosive fluids, saltwater or extremely high temperatures. HD Calcium Grease is used exclusive..
|
|||