| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Kinematic Viscosity at 100°C (212°F) | 5.6 cSt | 5.6 cSt | Base Oil; ASTM D445 |
|
Nye Lubricants UniFlor 8950 (497) (UF) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Kinematic Viscosity at 100°C (212°F) | 5.6 cSt | 5.6 cSt | Base Oil; ASTM D445 |
|
Nye Lubricants UniFlor 8951 (897-1) (UF) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Kinematic Viscosity at 100°C (212°F) | 5.6 cSt | 5.6 cSt | Base Oil; ASTM D445 |
|
Nye Lubricants UniFlor 8951R (897RP-1) (UF) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Kinematic Viscosity at 100°C (212°F) | 5.6 cSt | 5.6 cSt | ASTM D445 |
|
ExxonMobil Gargoyle Arctic 224 SHC 200 Series
Gargoyle Arctic SHC 200 Series are fully synthetic, supreme performance lubricants, specifically designed for use in refrigeration compressors and heat pumps. They are formulated from wax-free, synt..
|
|||
| Kinematic Viscosity at 100°C (212°F) | 5.6 cSt | 5.6 cSt | |
|
ConocoPhillips Conoflex® 32 SRI Lubricant ISO
Description: Conoco Conoflex SRI Lubricant is an excellent wire rope lubricant and preservative for any metal product, particularly when protecting from saltwater. It lubricates and preserves the wi..
|
|||
| Kinematic Viscosity at 100°C (212°F) | 5.6 cSt | 5.6 cSt | ASTM D445 |
|
ChevronTexaco Clarity® ISO 32 Hydraulic Oil AW
FeaturesChevron Clarity Hydraulic Oils AW are designed to give maximum protection to hydraulic pumps in highperformance industrial applications as well as in environmentally sensitive areas.They are..
|
|||
| Kinematic Viscosity at 100°C (212°F) | 5.6 cSt | 5.6 cSt | ASTM D445 |
|
ChevronTexaco Saturating Wax 2
FeaturesChevron Saturating Wax 2 is a food grade blend of fully refined paraffin wax and a wet strength additive. It is specifically formulated to impart moisture resistance and structural strength..
|
|||
| Kinematic Viscosity at 100°C (212°F) | 5.6 cSt | 5.6 cSt | ASTM D445 |
|
ExxonMobil Gargoyle Arctic 224 SHC 200 Series
Gargoyle Arctic SHC 200 Series are fully synthetic, supreme performance lubricants, specifically designed for use in refrigeration compressors and heat pumps. They are formulated from wax-free, synt..
|
|||
| Kinematic Viscosity at 100°C (212°F) | 5.6 cSt | 5.6 cSt | |
|
ConocoPhillips Hydroclear® 32 Rock Oil
Description: Conoco Hydroclear Rock Drill Oil is a high-quality, heavy-duty, extreme-pressure pneumatic tool lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Rock Drill ..
|
|||
| Kinematic Viscosity at 100°C (212°F) | 5.6 cSt | 5.6 cSt | |
|
ChevronTexaco Rando® HD 32 Ashless
Texaco Rando HD Ashless oils deliver value through:Premium performance — Ashless formulation meets or exceeds pump manufacturer requirements for viscosity, rust and corrosion protection, hydrolytic..
|
|||