Polymer Property : Kinematic Viscosity at 100°C (212°F) = 6.1 cSt Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Kinematic Viscosity at 100°C (212°F) 6.1 cSt
6.1 cSt
Base Oil; ASTM D445
Nye Lubricants 113 (DMO) Delicate Machinery Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 6.1 cSt
6.1 cSt
ASTM D445
ExxonMobil 10W Mobil Hydraulic
Mobil Hydraulic 10W is a high performance hydraulic oil formulated from advanced base oils and a balanced additive system designed to satisfy a wide range of heavy-duty hydraulic equipment requireme..
Kinematic Viscosity at 100°C (212°F) 6.1 cSt
6.1 cSt
ASTM D445
ExxonMobil 13M Mobil DTE 10M Series
Mobil DTE 10M Series oils are supreme performance anti-wear hydraulic oils engineered for wide temperature range applications. They exhibit optimum flow characteristics at sub-zero temperatures and ..
Kinematic Viscosity at 100°C (212°F) 6.1 cSt
6.1 cSt
ASTM D445
ExxonMobil 766 Mobilmet 760 Series
Mobilmet 760 Series are extra high performance oil based cutting oils. They are chlorine-free and are intended for severe cutting operations especially on difficult to machine steels. They are corro..
Kinematic Viscosity at 100°C (212°F) 6.1 cSt
6.1 cSt
ASTM D445
ChevronTexaco Mechanism LPS® ISO 32 Hydraulic Oil
Chevron Mechanism LPS Hydraulic Oils are highly refined, paraffinic oils containing oxidation and rust inhibitors, and special antiwear additives to extend the life of hydraulic pumps and motor part..
Kinematic Viscosity at 100°C (212°F) 6.1 cSt
6.1 cSt
ChevronTexaco Transultex® CF D
Texaco Transultex CF metalworking fluids deliver value through:Excellent antiweld properties from active sulfur and chlorine-free EP compounding which reduce frictional heat, prevent welding of meta..
Kinematic Viscosity at 100°C (212°F) 6.1 cSt
6.1 cSt
ASTM D445
ExxonMobil 10W Mobil Hydraulic
Mobil Hydraulic 10W is a high performance hydraulic oil formulated from advanced base oils and a balanced additive system designed to satisfy a wide range of heavy-duty hydraulic equipment requireme..
Kinematic Viscosity at 100°C (212°F) 6.1 cSt
6.1 cSt
ASTM D445
ExxonMobil 13M Mobil DTE 10M Series
Mobil DTE 10M Series oils are supreme performance anti-wear hydraulic oils engineered for wide temperature range applications. They exhibit optimum flow characteristics at sub-zero temperatures and ..
Kinematic Viscosity at 100°C (212°F) 6.1 cSt
6.1 cSt
ASTM D445
ExxonMobil 766 Mobilmet 760 Series
Mobilmet 760 Series are extra high performance oil based cutting oils. They are chlorine-free and are intended for severe cutting operations especially on difficult to machine steels. They are corro..