| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Kinematic Viscosity at 100°C (212°F) | 7.6 cSt | 7.6 cSt | ASTM D445 |
|
ExxonMobil Mobil 1 Synthetic ATF
Mobil 1 Synthetic ATF is a multi-vehicle, fully synthetic fluid designed to meet the demanding requirements of modern passenger vehicles.Mobil 1 Synthetic ATF is a multi-vehicle formula recommended ..
|
|||
| Kinematic Viscosity at 100°C (212°F) | 7.6 cSt | 7.6 cSt | |
|
ConocoPhillips Syncon® 46 Synthetic AW Hydraulic Fluid 46
Description: Conoco Syncon Synthetic AW Hydraulic Fluid is a synthetic polyalphaolefin (PAO) antiwear fluid for hydraulic systems that operate at extreme temperatures. It is available in four ISO vi..
|
|||
| Kinematic Viscosity at 100°C (212°F) | 7.6 cSt | 7.6 cSt | ASTM D445 |
|
ChevronTexaco ATF+3® Automatic Transmission Fluid
General DescriptionDaimlerChrysler has had their own ATF specifications for many years, but as of 1997, Chrysler owners manuals no longer list DEXRON as an acceptable replacement. ATF+3 is a readily..
|
|||
| Kinematic Viscosity at 100°C (212°F) | 7.6 cSt | 7.6 cSt | |
|
ChevronTexaco URSA® SAE 10W Super Plus
Texaco Ursa Super Plus oils deliver value through:Oil lasts longer between drains — Good oxidation stability protects against oil thickening during manufacturers recommended oil drain periods.Vital..
|
|||
| Kinematic Viscosity at 100°C (212°F) | 7.6 cSt | 7.6 cSt | ASTM D445 |
|
ExxonMobil Mobil 1 Synthetic ATF
Mobil 1 Synthetic ATF is a multi-vehicle, fully synthetic fluid designed to meet the demanding requirements of modern passenger vehicles.Mobil 1 Synthetic ATF is a multi-vehicle formula recommended ..
|
|||
| Kinematic Viscosity at 100°C (212°F) | 7.6 cSt | 7.6 cSt | |
|
ConocoPhillips Hydroclear® ATF Type F Automatic Transmission Fluid
Description: Conoco Hydroclear ATF Type F Automatic Transmission Fluid is a high-static-friction fluid developed for Ford automatic transmissions manufactured during the 1960s and 1970s. (Newer Ford..
|
|||
| Kinematic Viscosity at 100°C (212°F) | 7.6 cSt | 7.6 cSt | |
|
ChevronTexaco Havoline® ATF+3® Automatic Transmission Fluid
Havoline Automatic Transmission Fluid ATF+3 delivers value through:Correct viscosity and frictional characteristics to ensure smooth operation in Chrysler transmissions.Long-lasting viscosity modifi..
|
|||
| Kinematic Viscosity at 100°C (212°F) | 7.6 cSt | 7.6 cSt | |
|
ChevronTexaco URSA® SAE 10W Extra Duty
Texaco Ursa Extra Duty oils deliver value through:Excellent high temperature deposit control. Protects against high temperature oxidation and oil thickening.Special extreme pressure antiwear propert..
|
|||