| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage, Transverse | 0.0040 - 0.0060 cm/cm | 0.0040 - 0.0060 in/in | ASTM D955 |
|
PolyOne Trilliant™ HC HC7300-0013 ESD Black Acrylonitrile Butadiene Styrene (ABS)
Information provided by PolyOne
|
|||
| Linear Mold Shrinkage, Transverse |
0.0040
-
0.0070
cm/cm <br>@Thickness 3.20 mm
|
0.0040
-
0.0070
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Geloy XTWM200 ASA (Europe-Africa-Middle East)
ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Linear Mold Shrinkage, Transverse |
0.0040
-
0.0080
cm/cm <br>@Thickness 3.20 mm
|
0.0040
-
0.0080
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Lexan® EXL1132 PC Copolymer
Lexan* EXL1132 polycarbonate (PC) siloxane copolymer resin is a high flow, UV stabilized injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high fl..
|
|||
| Linear Mold Shrinkage, Transverse |
0.0040
-
0.0080
cm/cm <br>@Thickness 3.20 mm
|
0.0040
-
0.0080
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Lexan® EXL1192T PC Copolymer
Lexan* EXL1192T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties for food contact applications. This resin offers good low temp..
|
|||
| Linear Mold Shrinkage, Transverse |
0.0040
-
0.0080
cm/cm <br>@Thickness 3.20 mm
|
0.0040
-
0.0080
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Lexan® EXL1810T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers cold temperature (0 °C) ductility in combination with very high flow char..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0040 - 0.0060 cm/cm | 0.0040 - 0.0060 in/in | SABIC Method |
|
SABIC Innovative Plastics LNP COLORCOMP NX05467 PC+ABS
LNP* COLORCOMP* NX05467 is an unfilled Polycarbont+ABS resin. Added features of this grade are: Non-Chlorinated, Non-Brominated Flame Retardant.
|
|||
| Linear Mold Shrinkage, Transverse |
0.0040
-
0.0050
cm/cm <br>@Thickness 3.20 mm
|
0.0040
-
0.0050
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Lexan® HFD4472 PC
Lexan* HFD4472 is a 20% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4472 has enhanced mold release, impact ductili..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0040 cm/cm | 0.0040 in/in | ASTM D955 |
|
LNP Stat-Kon® PDX-E-99689 CCS Polyetherimide, Carbon Fiber Reinforcement
(discontinued **)
Features: Low to None Ion Content, Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0040 cm/cm | 0.0040 in/in | Measured on 102 mm X 102 mm X 3.2 mm Plaques, Edge Gated |
|
Chevron Phillips Ryton® R-7 Polyphenylene Sulfide Compound
(discontinued **)
Natural Color Polyphenylene Sulfide CompoundRyton® R-7 is polyphenylene sulfide compounded with glass fibers and mineral fibers to produce an injection moldable high temperature engineering compoun..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0040 - 0.0060 cm/cm | 0.0040 - 0.0060 in/in | ISO 294-4 |
|
Ineos ABS Lustran® ABS 970
Lustran® ABS 970 has high impact strength and good paintability.
|
|||
| Linear Mold Shrinkage, Transverse |
0.0040
-
0.0060
cm/cm <br>@Thickness 3.20 mm
|
0.0040
-
0.0060
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics NORYL ZX09022 PPE+PP (Europe-Africa-Middle East)
Thermocomp ZX09022 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile mod..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0040 - 0.0060 cm/cm | 0.0040 - 0.0060 in/in | ASTM D955 |
|
Solvay Specialty Polymers AvaSpire® AV-848 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber
AvaSpire® AV-848 CF30 is a 30% carbon fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparabl..
|
|||
| Linear Mold Shrinkage, Transverse |
0.0040
cm/cm <br>@Thickness 3.20 mm
|
0.0040
in/in <br>@Thickness 0.126 in
|
ASTM D955 |
|
Solvay Specialty Polymers Ryton® R-7-120BL Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® R-7-120NA and R-7-120BL glass fiber and mineral filled polyphenylene sulfide compounds provide good strength and low maintenance molding using conventional molding equipment.Features: Good..
|
|||
| Linear Mold Shrinkage, Transverse |
0.0040
-
0.0060
cm/cm <br>@Thickness 3.20 mm
|
0.0040
-
0.0060
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC202M PPE+HIPS (Europe-Africa-Middle East)
DATA ON BK1005 ONLY.
|
|||
| Linear Mold Shrinkage, Transverse |
0.0040
-
0.0060
cm/cm <br>@Thickness 3.20 mm
|
0.0040
-
0.0060
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Xenoy® 1760E PBT+PC
11% Glass Reinforced alloy. Impact/chemical resistant. Excellent physical property retention in automotive exteriors. High flow version of Xenoy 1760 resin.
|
|||
| Linear Mold Shrinkage, Transverse |
0.0040
-
0.0060
cm/cm <br>@Thickness 3.20 mm
|
0.0040
-
0.0060
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics XYLEX HX8300HP PC+POLYESTER
Medium flow, Transparent PC/Polyester alloy. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant...
|
|||
| Linear Mold Shrinkage, Transverse |
0.0040
cm/cm <br>@Time 86400 sec
|
0.0040
in/in <br>@Time 24.0 hour
|
ASTM D955 |
|
SABIC Innovative Plastics LNP THERMOCOMP AF006XXZ ABS
LNP* THERMOCOMP* AF006XXZ is a compound based on ABS resin containing 30% Glass Fiber.
|
|||
| Linear Mold Shrinkage, Transverse |
0.0040
-
0.0060
cm/cm <br>@Thickness 4.00 mm
|
0.0040
-
0.0060
in/in <br>@Thickness 0.157 in
|
|
|
Teijin Panlite® LN-1010RM High Light Reflection, Flame Resistant Polycarbonate Resin
Polycarbonate-resin-base flame retardant and good light-reflection grade. It exhibits high light-reflection (over 96 %) at whole visible light range and also good light shut-out even at a thinner th..
|
|||
| Linear Mold Shrinkage, Transverse |
0.0040
-
0.0060
cm/cm <br>@Thickness 4.00 mm
|
0.0040
-
0.0060
in/in <br>@Thickness 0.157 in
|
|
|
Teijin Panlite® LN-3000RM High Light Reflection, Halogen-Free Flame Resistant Polycarbonate Resin
Polycarbonate-resin-based halogen-free flame retardant and good light-reflection grade. It exhibits high light-reflection (over 96 %) at whole visible light range and also good light shut-out even a..
|
|||
| Linear Mold Shrinkage, Transverse |
0.0040
-
0.0060
cm/cm <br>@Thickness 3.20 mm
|
0.0040
-
0.0060
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Ultem ATX102R PEI+PCE
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Linear Mold Shrinkage, Transverse |
0.0040
-
0.0060
cm/cm <br>@Thickness 3.20 mm
|
0.0040
-
0.0060
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Ultem ATX152R PEI+PCE
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Linear Mold Shrinkage, Transverse |
0.0040
-
0.0060
cm/cm <br>@Time 86400 sec
|
0.0040
-
0.0060
in/in <br>@Time 24.0 hour
|
ASTM D955 |
|
SABIC Innovative Plastics LNP VERTON RV00AE PA 66
LNP* VERTON* RV00AE is a compound based on Nylon 66 containing 50% Long Glass Fiber. Added features of this grade include: Easy Molding, Structural.
|
|||
| Linear Mold Shrinkage, Transverse |
0.0040
-
0.0060
cm/cm <br>@Thickness 3.20 mm
|
0.0040
-
0.0060
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics NORYL PPX PPX830 PPE+PP (Europe-Africa-Middle East)
Noryl* PPX830 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus ..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0040 cm/cm | 0.0040 in/in | ASTM D955 |
|
Unitika RUN35-TA Light resistant PA6, Dry
Light resistant and internalInformation provided by Unitika Ltd.
|
|||
| Linear Mold Shrinkage, Transverse | 0.0040 cm/cm | 0.0040 in/in | ISO 294-4, 2577 |
|
EMS-Grivory Grivory® LV-65H FWA nat PA12-GF65
Product description: Grilamid LV-65H FWA natural is a 65 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combined w..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0040 cm/cm | 0.0040 in/in | ISO 294-4, 2577 |
|
EMS-Grivory Grivory® LVX-50H nat PA12-GF50
Product description: Grilamid LVX-50H natural is a 50% glass fiber reinforced, heat stabilized polyamide 12. Special characteristics of this injection molding product are: Very high stiffness and st..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0040 cm/cm | 0.0040 in/in | measured on flat plaques, 320 x 320 mm; ISO 2577 |
|
Azdel Plus U400-B01N 41.5% Directionalized Continuous Fiber Mat / PP Resin Matrix
AZDEL® U400-B01N is a uni-directional fiber and random glass mat reinforced polypropylene composite material featuring excellent fiber distribution over long flow paths and complex part forms. Thi..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0040 - 0.0060 cm/cm | 0.0040 - 0.0060 in/in | 24 hrs; ASTM D955 |
|
LNP Verton™ UF-700-12 Polyphthalamide, Long Glass Fiber Filled
(discontinued **)
LNP™ Verton™ UF-700-12 HS EXP is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized.Information provided by LNPThis dat..
|
|||
| Linear Mold Shrinkage, Transverse |
0.0040
cm/cm <br>@Time 86400 sec
|
0.0040
in/in <br>@Time 24.0 hour
|
ISO 294 |
|
SABIC Innovative Plastics LNP Verton OV00A PPS
LNP* Verton* OV00A is a compound based on Polyphenylene Sulfide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
|
|||